This in vitro study evaluated the influence of chemomechanical caries removal solution on the surface topography of metal-ceramic feldspar porcelain (MAJOR ceramic) and All-ceramic feldspar porcelain (Vita Alpha) using light polarizing microscope. Forty specimens of MAJOR ceramic and forty specimens of Vita Alpha ceramic of (12mm diameter & 3mm height) were prepared .All specimens were polished with silicon polishing burs, cleaned, autoglazed and stored in 37°C before exposure to Carisolv. Thirty specimens of each material randomly exposed to Carisolv gel for 5, 10 and 20 minutes respectively, other ten specimens were not, to act as control group. All specimens were subjected to surface roughness test by profilometer and evaluated using light polarizing microscope. ANOVA and student t-test were used to analyze the surface roughness values.Different exposure times of modified Carisolv gel showed highly significant difference compared to control (P<0.001).Surface treatment with modified Carisolv gel for 20 minutes resulted in the highest surface roughness. Metal-ceramic feldspar porcelain (MAJOR ceramic) showed high surface roughness than all ceramic feldspar porcelain (Vita Alpha), however, the difference is statistically not significant (P>0.05).Different exposure times of modified Carisolv gel affect the surface roughness of dental ceramic materials differently. This study showed major influence on surface topography after exposure to modified Carisolv gel for 20 minutes on dental ceramics MAJOR and Vita Alpha.
Aim: To evaluate the effect of two bonding systems and two curing systems on sealing ability of class V composite restorative materials. Materials and methods: This study was performed in vitro on 40 caries free upper first premolar teeth. The Standardized class V cavity preparation on buccal and lin- gual surfaces of each tooth was done. Then the teeth were randomly divided into two major groups each of twenty. 40 cavities were performed on these teeth and the first group7th generation bonding agent (i Bond) were applied according to the manufacturer instructions and single increment of univer- sal composite (XRV Herculite) from kerr were applied and twenty of the cavities were cured with con- ventional light cure device (astralis-5) and t
... Show MoreIn this work an approach has been developed to investigate the influence of surface roughness on thermohydrodynamic performance in aligned and misaligned journal bearings by considering an average flow model and deriving the shear flow factor for various roughness configurations, similar to the pressure flow factor. An average Reynolds equation for rough surfaces is defined in term of pressure and shear flow factors, which can be obtained by numerical flow simulation, though the use of measured or numerically generated rough surfaces. Reynolds, heat conduction and energy equations are solved simultaneously by using a suitable numerical technique (Finite Difference Method) to obtain the pressure and temperature di
... Show MoreBackground: the aim of this study was to evaluate the effect of different surface acids treatments (37%phospjoric acid, 5%hydrofluoric acid, 1.23 acidulated phosphate fluoride) of feldspathic ceramic VITA 3D MASTER , and the effect of thermocycling on shear bond strength using a ceramic repair kit (ivoclar/vivadent). Material and Methods: sixty Nickel-Chromium metal base plates were prepared(9mm diameter,3mm depth) using lost wax technique, 2mm thick layer of ceramic(VITA 3D MASTER) fused to metal plates, all specimens were embedded in acrylic resin blocks except their examined surfaces and divided into 3 main groups 20 specimens each, Grp A: treatment with 37%phosphoric acid for 2 mins, Grp B: etching with 5% hydrofluoric acid for 2mins,
... Show MoreBackground: The aim of the study was to investigate the effect of surface treatments of zirconia (grinding and sandblast with 50μm, 100 μm) on shear bond strength between zirconia core and veneering ceramic. Material and methods: Twenty-eight presintered Y-TZP ceramic specimens (IPS e.max ZirCAD, Ivoclar vivadent) were fabricated and sintered according to manufacturer’s instructions. The core specimens were divided randomly in to 4 groups, group 1: no surface treatment, group2: zirconia specimens were ground with silicon carbide paper up to1200 grit under water cooling, group3: zirconia specimens were ground and sandblast with 100 μm alumina, group 4: zirconia specimens were ground and sandblast with 50 μm alumina. Surfa
... Show MoreThe surface finish of the machining part is the mostly important characteristics of products quality and its indispensable customers’ requirement. Taguchi robust parameters designs for optimizing for surface finish in turning of 7025 AL-Alloy using carbide cutting tool has been utilized in this paper. Three machining variables namely; the machining speeds (1600, 1900, and 2200) rpm, depth of cut (0.25, 0.50, 0.75) mm and the feed rates (0.12, 0.18, 0.24) mm/min utilized in the experiments. The other variables were considered as constants. The mean surface finish was utilized as a measuring of surface quality. The results clarified that increasing the speeds reduce the surface roughness, while it rises with increasing the depths and fee
... Show MoreBackground: This in vitro study was carried out to evaluate the effects of various veneering dentin ceramic thicknesses and repeated firings on the color of lithium disilicate glass-ceramic (IPS e.max Press) and zirconium-oxide (IPS ZirCAD) all-ceramic systems, measured by clinical spectrophotometers (Easyshade Advance 4.0) . Materials and methods: The 72specimens cube-shaped have the dimension of about 11 mm in width, 14 mm in length, 1mm in thickness, these cores divided into 3 groups according to the type of material each group have (24)core specimens. Each group had been divided into three sub-groups (each having 8 specimens) according to veneering with dentin ceramic thicknesses: as 0.5, 1, or 2 mm (n=8). IPS e.max press and ZirCAD c
... Show MoreAn atomic force microscope (AFM) technique is utilized to investigate the polystyrene (PS) impact upon the morphological properties of the outer as well as inner surface of poly vinyl chloride (PVC) porous fibers. Noticeable a new shape of the nodules at the outer and inner surfaces, namely "Crater nodules", has been observed. The fibers surface images have seen to be regular nodular texture at the skin of the inner and outer surfaces at low PS content. At PS content of 6 wt.%, the nodules structure was varied from Crater shape to stripe. While with increasing of PS content, the pore density reduces as a result of increasing the size of the pore at the fiber surface. Moreover, the test of 3D-AFM images shows that the roughness of both su
... Show MoreThe current research is concerned with methods of formation and their effect on the sintering process of ceramic materials. The research is divided into a number of chapters. The first chapter addressed the research structure (the research problem, importance, objective, limits, and it also defined the terms used in the research). The second chapter addressed the theoretical framework, where the theoretical framework has been divided into three sections. The first section dealt with methods of formation of ceramic materials including: Plasticizing method 2- semi-dry pressing method 3- dry pressing method 4- extrusion method 5- casting method.
The researcher found that there is a clear difference between the methods through her formati
The zirconia ceramic restoration (ZCR) is used as substitutes for the metal-ceramic restoration. Clinical studies demonstrating of ZCRs showed a high fracture incidence of veneering layer than metal-ceramic restorations. This attributed to the low bond strength of zirconia to veneering ceramic as a result of lacking of glass content in its matrix. Surface treatment was proposed to improve the bonding strength between zirconia and veneering ceramic. Several studies revealed that some treatment such as airborne particle abrasion (APA) is responsible for generating chipping of veneering ceramic. The study aimed to develop a new zirconia coatings to increase bonding strength between zirconia substrate and veneering porcelain. Three groups of 15
... Show More