Background: This in vitro study was carried out to evaluate the effects of various veneering dentin ceramic thicknesses and repeated firings on the color of lithium disilicate glass-ceramic (IPS e.max Press) and zirconium-oxide (IPS ZirCAD) all-ceramic systems, measured by clinical spectrophotometers (Easyshade Advance 4.0) . Materials and methods: The 72specimens cube-shaped have the dimension of about 11 mm in width, 14 mm in length, 1mm in thickness, these cores divided into 3 groups according to the type of material each group have (24)core specimens. Each group had been divided into three sub-groups (each having 8 specimens) according to veneering with dentin ceramic thicknesses: as 0.5, 1, or 2 mm (n=8). IPS e.max press and ZirCAD cores group had been veneered with IPS e.max Ceram dentin ceramic shade A2 according to manufacturer’s instructions and the metal group had been veneered with IPS classic dentine ceramic with shade A2 according to manufacturer’s instructions. Repeat firings (3, 5 and 7 times) had been applied on all the specimens. Color differences among ceramic specimens had been measured using a clinical spectrophotometer (VITA Easyshade); the color data had been expressed according the Vita Classic shade guide. Results: The shade of all specimens had been compared inside the subgroups and with the main groups. The percentage of color agreement among the subgroups showed the color of all ceramic systems had been affecting by firing interval, the ceramic thickness and brand of ceramic. The number firings intervals applied on the all ceramic system has a significant effect on the final color, the increase of firing number change the color to a darker and reddish color. The 5th firing interval is the point at which the major color changes happened (darker shade), and in next interval (7th firing) less color changes happened. The thickness of veneering ceramic affected the color significantly. The 0.5 mm specimens in all groups showed the highest percentage of agreement (less color changes) after firing intervals, then the 1mm came and the least percentage of agreement ( highest color changes ) was the 2 mm specimens. The Brand of veneering ceramic and the type of core record a significance difference in color changes when exposed to firing heat. Conclusion: With limit of this study, the final color of the all ceramic system definitely affected by the number of firing cycle exposed to, and the veneering ceramic thickness have a clear effect on the final shade of the all ceramic tested.
Background: In capturing a negative image, the digital impression secures a digital record for the purposeof designing and creating restorations. The introduction of scanning system presents a paradigm shift in the way of the dental impression procedure and encourages the accuracy of obtained restoration especially in the marginal area as a result of producing accurate final impression The digital system offers many advantages over the Conventional method.. The objective of this present in vitro study was to evaluate the marginal fitness of all ceramic crowns fabricated by direct digital scanning of the prepared tooth using two types of intra-oral cameras (Bluecam camera with strip light projection technique and Omnicam camera with video sa
... Show MoreABSTRACT Background: Color changes that are detectable to human eye can affect the esthetic appearance of ceramic veneers. The purpose of this study was to evaluate and compare the effect of artificial accelerated aging on the color of ceramic veneers cemented with different resin cements. Materials and Methods: Sixty discs were prepared with 0.5 mm thickness, 30 discs made from IPS e.max press (Ivoclar Vivadent) and 30 discs were made from VITA Enamic (VITA Zahnfabrik). The discs were cemented with three resin cements: Variolink Veneer MV 0 shade (Ivoclar Vivadent), Rely X veneer Translucent shade (3M ESPE) and NX3 Nexus Clear shade (Kerr Corporation) with 0.1 mm thickness. The spectrophotometer Easyshade Advance was used to measure the co
... Show MoreIn this study, the effect of ceramic coating on the performance and gases emission on diesel engine was investigated. A four-stroke, direct injected, single cylinder, diesel engine was tested at constant speed and at different load conditions without coating. Then, the inlet and exhaust valves faces were coated by about 500µm with ceramic materials. Ceramic layers were made of YttriaStabilized Zirconia (YSZ), and NiCrAl as a bond coat. The coating technique adapted in this work is the flame spray method. The engine with valves ceramiccoated research was tested for the same operation conditions of the engine (without coating). The results indicate a reduction in both fuel consumption by about 7.6% and particulate emissions by about (13
... Show MoreABSTRACT Background: One of the major problems of all ceramic restorations is their probable fracture against the occlusal forces. The objective of this in vitro study was to evaluate the effect of two gingival finishing lines (90°shoulder and deep chamfer) on the fracture resistance of full contour CAD/CAM and heat press all-ceramic crowns. Materials and Methods: Thirty two maxillary first premolars were prepared to receive full contour CAD/CAM (zolid) and heat press (Cergo Kiss) ceramic crowns using a special paralleling device (Parallel-A-Prep). The teeth were divided into four groups according to the type of finishing line prepared. Each crown was cemented to its corresponding tooth using self-etch, self-adhesive dual cure resin ceme
... Show MoreIn this work, a ceramic model has obtained from Iraqi bentonite as a base material with limited additions of alumina and silica. The selected material can bear temperatures higher than the bearing temperature of bentonite as it achieved tolerance temperatures (1300°C) based on X-ray diffraction patterns. It was found that the addition of alumina and silica led to the occurrence of basic phases such as mullite, quartz, cordierite and feldspar in percentages that depended on the percentage of addition in the mixture and the firing temperature, which was (1000-1300)°C.
Background: The aim of the study was to investigate the effect of surface treatments of zirconia (grinding and sandblast with 50μm, 100 μm) on shear bond strength between zirconia core and veneering ceramic. Material and methods: Twenty-eight presintered Y-TZP ceramic specimens (IPS e.max ZirCAD, Ivoclar vivadent) were fabricated and sintered according to manufacturer’s instructions. The core specimens were divided randomly in to 4 groups, group 1: no surface treatment, group2: zirconia specimens were ground with silicon carbide paper up to1200 grit under water cooling, group3: zirconia specimens were ground and sandblast with 100 μm alumina, group 4: zirconia specimens were ground and sandblast with 50 μm alumina. Surfa
... Show MoreVitrifications process one of the important methods to immobilize nuclear waste. In this research nuclear waste (Strontium Oxides) with molecular weight (5%) was immobilized by vitrification methods in two types of borosilicate glass (c-type) which are glass and glass-ceramics. To investigate the physical, chemical and mechanical properties of glass and glass-ceramic after immobilize nuclear waste these samples irradiated by gamma ray radiation. Co-60 was used as gamma a irradiation with dose rate 0.38 kGy/hr for different period of time. It’s found that gamma radiation affected the glass and glass-ceramic properties. From phase analysis by the x-ray diffraction for glass-ceramic samples proved that at doses 343kGy change the cry
... Show MorePurpose: To evaluate the effect of different surface treatments on shear bond strength between dentin and IPS e.max lithium disilicate glass-ceramic. Materials and Methods: Eighteen extracted third molars were embeded in epoxy resin. The tooth was sectioned vertically in mesiodistal direction using a low speed hard tissue microtome. The buccal and lingual surfaces of each section were ground flat using 600 grit Silicone carbide paper. Eighteen ceramic discs consisted of lithium disilicate glass-ceramic were prepared with a diameter of 4.7mm and height of 2.2mm. The discs were divided in two groups (n=10): (1) IPS e.max treated with hydrofluoric acid and Monobond Plus (MBP) and (2) IPS e.max treated with Monobond Etch &Prime (MBEP). The toot
... Show MoreThe current study deals with one of the ancient and modern techniques of ceramic art, which has evolved dramatically. This technique is interested in the muddy Body and its coloring, rather than interesting in the coloring of the layer on the surface of the glass port on the ceramic object. It is classified as ceramic techniques of the single heartburn, where use many coloring oxides. As well as, the use of (Pigment), which is often made of metal compounds, or metal oxides such as iron and manganese, copper and cobalt and more others.
The first chapter includes the problem, the importance, the goal, and the boundaries of the study. In addition, focuses on determining the terms such as (Sgrafitto). The second chapter consists of two to
In this work, the effect of ceramic coating on performance, exhaust gas temperature and gases emissions of diesel engine operated on diesel fuel and biodiesel blends was investigated. A conventional four stroke, direct injected, single cylinder, diesel engine was tested at constant speed and at different load conditions using diesel fuel and biodiesel blends. The inlet and exhaust valves, the head of piston and cylinder head of the engine were coated by ceramic materials. Ceramic layers were made of (210-240) μm of Al2O3 and (30-60) μm of 4NiCr5Al as a bond coat for inlet and exhaust valves and (350-400) μm of YSZ and (50-100) μm of 4NiCr5Al as a bond coat for head of piston and (280-320) μm of Sic and (40-80) μm of 4NiCr5Al as a b
... Show More