This in vitro study evaluated the influence of chemomechanical caries removal solution on the surface topography of metal-ceramic feldspar porcelain (MAJOR ceramic) and All-ceramic feldspar porcelain (Vita Alpha) using light polarizing microscope. Forty specimens of MAJOR ceramic and forty specimens of Vita Alpha ceramic of (12mm diameter & 3mm height) were prepared .All specimens were polished with silicon polishing burs, cleaned, autoglazed and stored in 37°C before exposure to Carisolv. Thirty specimens of each material randomly exposed to Carisolv gel for 5, 10 and 20 minutes respectively, other ten specimens were not, to act as control group. All specimens were subjected to surface roughness test by profilometer and evaluated using light polarizing microscope. ANOVA and student t-test were used to analyze the surface roughness values.Different exposure times of modified Carisolv gel showed highly significant difference compared to control (P<0.001).Surface treatment with modified Carisolv gel for 20 minutes resulted in the highest surface roughness. Metal-ceramic feldspar porcelain (MAJOR ceramic) showed high surface roughness than all ceramic feldspar porcelain (Vita Alpha), however, the difference is statistically not significant (P>0.05).Different exposure times of modified Carisolv gel affect the surface roughness of dental ceramic materials differently. This study showed major influence on surface topography after exposure to modified Carisolv gel for 20 minutes on dental ceramics MAJOR and Vita Alpha.
Objective: The aim of this study was to evaluate the effect of pumice, burning investment material
and black sand on the surface roughness of heat cure acrylic resin.
Methodology: Sixty specimens were prepared from pink heat cure acrylic resin, the specimens
where grouped into; 20 specimens which polished with pumice and water (control group); 20
specimens which polished with investment material (after burning it) and water; and 20 specimens
which polished with black sand and water. The average surface roughness of specimens after
polishing procedure had been determined by profilometer (surface roughness tester).
Results: Through the application of ANOVA and LSD tests, the result of this study showed that there
wa
Background: To investigate the effect of different types of storage media on enamel surface microstructure of avulsed teeth by using atomic force microscope.Materials and methods : Twelve teeth blocks from freshly extracted premolars for orthodontic treatment were selected . The study samples were divided into three groups according to type of storage media :A-egg white , B- probiotic yogurt , and C-bovine milk . All the samples were examined for changes in surface roughness and surface granularity distribution using atomic force microscope, at two periods: baseline, and after 8 hours of immersing in the three types of storage media. Results: Milk group had showed a significant increase in the mean of the roughness values at
... Show MoreBackground:The demand for esthetic orthodontic appliances is increasing so that the esthetic orthodontic archwires were introduced. This in vitro study was designed to evaluate the surface roughness offiber-reinforced polymer composite (FRPC) archwires compared to coated nickel-titanium (NiTi) archwires immersed in artificial saliva. Materials and Methods:Three types of esthetic orthodontic archwires were used: FRPC (Dentaurum), Teflon coated NiTi (Dentaurum) and epoxy coated NiTi (Orthotechnology). They were round (0.018 inch) in cross section and cut into pieces of 15 mm in length.Forty pieces from each type were divided into four groups; one group was left at a dry condition and the other three groups were immersed in artificial saliva (
... Show MoreBackground:Â Various fluids in the oral environment can affect the surface roughness of resin composites. This in vitro study was conducted to determine the influence of the mouth rinses on surface roughness of two methacrylate-based resin (nanofilled and packable composite) and siloraine-based resin composites.
Materials and methods: Disc-shaped specimens (12 mm in diameter and 2mm in height) were prepared from three types of composi
... Show MoreObjective(s): In the present study, glycerin is used as a substitute for tin-foil and cold mold seal (Alginate mould seal)
in the process of curing heat and cold-cure acrylic resin denture base against stone and plaster.
Methodology: 60 specimens were prepared from heat-cure acrylic resin and cold-cure acrylic resin denture base. The
study includes 12 groups of specimens depending on the type of processing, investment material and type of
separating medium that are used in curing process. Each group of them contains 5 specimens for each test.
Some of physical properties of the processed acrylic denture base that (water sorption and solubility) have been
compared with those processed using tin-foil and tin-foil substitut
Background: Alterations in the microhardness and roughness are commonly used to analyze the possible negative effects of bleaching products on restorative materials. This in vitro study evaluated the effect of in-office bleaching (SDI pola office +) on the surface roughness and micro-hardness of four newly developed composite materials (Z350XT –nano-filled, Z250XT-nano-hybrid, Z250-mico-hybrid and Silorane-silorane based). Materials and methods: Eighty circular samples with A3 shading were prepared by using Teflon mold 2mm thickness and 10mm in diameter. 20 samples for each material, 10 samples for base line measurement (surface roughness by using portable profillometer, and micro-hardness by usingDigital Micro Vickers Hardness Test
... Show MoreIn this work, results from an optical technique (laser speckle technique) for measuring surface roughness was done by using statistical properties of speckle pattern from the point of view of computer image texture analysis. Four calibration relationships were used to cover wide range of measurement with the same laser speckle technique. The first one is based on intensity contrast of the speckle, the second is based on analysis of speckle binary image, the third is on size of speckle pattern spot, and the latest one is based on characterization of the energy feature of the gray level co-occurrence matrices for the speckle pattern. By these calibration relationships surface roughness of an object surface can be evaluated within the
... Show MoreDue to the rapid advancement of technology and the technology of things, modern industries start to need a highprecision equipment and surface finishing, so many finishing processes began to develop. One of the modern processes is Magnetic Abrasive Finishing (MAF), which is a high-precision process for internal and external finishing under the influence of a magnetic field of abrasive particles. Boron Carbide (B4C) ceramics was tested by mixing it with iron (Fe) and produced abrasive particles to reduce the intensity of scraping on the surface, reduce the economic cost and achieve a high finishing addition to remove the edges at the same time. The material selected for the samples was mild steel (ASTM E415) under (Quantity of Abrasives, Mac
... Show MoreBackground: In this study we evaluate the effect of plasma treatment (oxygen and argon) gas in two different exposure times on the surface of heat cure and light cure acrylic resin. Materials and method: 100 specimens of heat cure and light cure acrylic resin were fabricated. The measurements of the samples were (75mm, 25mm and 4.5mm) length, width and depth respectively with stopper of 3mm depth. Two types of gas used oxygen and argon in (5,10) min by using (DC-glow discharge plasma device) then we apply cold cure soft lining material, with the help of Instron machine we test the shear stress value. Results: A highly significant effect after argon and oxygen gases treatment in both 5 and 10 min exposure times on shear bond strength to soft
... Show MoreObjective: In order to evaluate the effect of different typed of Separating Medium on the roughness of the fitted
tissue surface of acrylic denture base.
Methodology: Chosen three types of separating medium (Group A Tin foil), (Group B Detery Isolant),(Group C
Cold Mould Seal),used 30 samples of hot cure acrylic resin ,10 samples for each group, after complete curing of
these samples , Profilometer device was used to measure the surface roughness of each sample in all groups.
Results: Using One Way ANOVA Test and LSD test, the results were highly significant in differences among all
groups. Although (Group A) showing lest roughness, (Group B) showing a satisfactory result of roughness, While
(Group C) Showing the hig