Background: Dental implants act as infrastructure for fixed restoration to look like as a natural tooth. Osseointegration is a biological events and considered as a base for success of dental implant. The aim of this study is to evaluate the bond strength between bone and Ti implant coated with mixture of nano hydroxyapatite-chitosan-collagen compared with Ti implants coated with nano hydroxyapatite implanted in rabbit tibia, after different period of implantation time (two and six weeks) by torque removal test. Material and methods: 36 screws of commercially pure titanium; 8mm in length and 3mm diameter , 18 screws coated with mixture of nano hydroxyapatite-chitosan-collagen and18 screws coated with nano hydroxyapatite by dip coating. Structural characteristics was assessed by scanning electron microscope, and FTIR analysis. The screws were implanted in 18 healthy adult male New Zeeland rabbits each tibia received one screw, right tibia received screw coated with nano hydroxyapatite while left tibia received screw coated nano hydroxyapatite-chitosan-collagen composite. Removal torque test was done by torque meter to determine the highest torque value necessary to remove the implants from tibia bone after different period of time of implantation(2 and 6 weeks). Result: Nano hydroxyapatite-chitosan-collagen composite coating was resulting in higher torque removal value than nano hydroxyapatite coating for two periods of time. Conclusion: Concluded that addition of collagen and chitosan to nano hydroxyapatite was more efficient in rapid bone formation than nano hydroxyapatite only.
Hydrothermal process method using different dimensions reactors with volume 100 ml (homemade) was employed to prepare titanium sub-oxide Ti6O11, where one gram of TiO2 nanoparticles 30-50 nm and 3M (20 ml) of NaOH as suspension was used . The samples are characterized using X-ray diffraction, Raman spectroscopy, and Field Emission Scanning Electron Microscopy (FE-SEM). X-ray diffraction revealed the formation of sub- oxide titanium Ti6O11 of triclinic structure with Magneli phase, when the temperature applied was 363K for 9h.While FE-SEM showed uniform hierarchical structures with planar grass-like shapes. A novel phase has been found from rutile titanium.
Choosing an appropriate impression material is a challenge for many dentists, yet an essential component to provide an excellent clinical outcome and improve productivity and profit. The purpose of present study was to compare wettability, tear strength and dimensional accuracy of three elastomeric impression materials, with the same consistencies (light-body). Three commercially available light body consistency and regular set 3M ESPE Express polyvinylsiloxane (PVS), 3M ESPE Permadyne polyether (PE), and Identium (ID), impression materials were comparedTear strength test, contact angle test and linear dimensional accuracy were evaluated for three elastic impression material. Among the three experimental groups PE impression materia
... Show MoreIn this work, polypyrrole (PPy) composites were chemically prepared by a chemical oxidation method. Also, Tungsten Trioxide (WO3) nanoparticles were prepared and added in certain proportions to PPy. The structure properties were studied for the polypyrole and tungesten trioxide separately before mixing them together. The X-ray diffraction (XRD) analysis revealed a hexagonal WO3 and a triclinic PPy. It was observed that the nano-composite prepared by the addition of WO3 with 10 and 20% volume ratios to PPy shows a triclinic phase with the presence of hexagons. The molecular structures of PPy, WO3, and PPy–WO3 nano composites were depicted by Fourier-transform infrare
... Show MoreIN this work, a titanium dental implant was modified by electro-polymerized of 4-allyl-2-methoxyphenol (Eugenol) using direct current lower than 3.5 volt. The modification of titanium dental implant was achieved to improve its corrosion resistant. Fourier transform infrared spectroscopy (FTIR) was employed to confirm the electro-polymerization of Eugenol to Poly Eugenol (PE) on pure titanium. Deposition of PE on titanium was confirmed by X-ray diffraction and was characterized by thermogravimetric analysis (TGA). The surface morphology of polymeric film were examined through scanning electron microscopy (SEM). Coated titanium by (PE) revealed a good corrosion protection efficiency even at temperature ranged (293-323)K in artificial saliva.
... Show MoreIn this work, some mechanical properties of the polymer coating were improved by preparing a hybrid system containing Graphene (GR) of different weight percentages (0.25, 0.5, 1, and 2wt%) with 5wt% carbon fibres (CF) and added to a polymer coating by using casting method. The properties were improved as GR was added with further improvement on adding 5wt% of CF. The impact strength of acrylic polymer with GR increases with increasing weight ratio of GR; maximum value was obtained when the polymer coating was incorporated with 1wt% GR and 5wt% CF. The impact strength of acrylic polymer with GR and GR/CF composites incorporated with GR at 1wt% and CF at 5wt%. Hardness increase with increasing weight ratio of Gr and a significant imp
... Show MoreThis study was aimed to evaluate the effect of spraying nano chitosan loaded with NPK fertilizer and nettle leaf and green tea extracts on the growth and productivity of potato for the spring and fall seasons of 2021.It was conducted at private farm in Wasit Governorate, Iraq, as a factorial experiment (5 × 5) within randomized complete block design using three replicates. The first factor included spraying with four concentrations of chitosan nanoparticles loaded with NPK fertilizer 0, 10. 15 and 20% in addition to chemical fertilization treatment, the second factor was spraying nettle leaf extract 25 and 35 gL-1 and green tea extract with 2 and 4 g.L-1, in addition to the control treatment, spraying with distilled water only. The
... Show MoreIn this research the effect of laser energy by using argon gas on the some physical properties of semiconductor film of TiO2, was studied used Q-Switch Nd:YAG laser in different energies (600-1000) mJ with temperature 100 0C for glass substrate under vacuum nearly 10-3 - - , and by AFM test the roughness of films increased when the energy of laser increased too. The values of roughness between (6.77-13) nm, therefore the thicknesses increased to change from (34.88 - 165.48) nm, so the absorption of film increased because of the thickness of the film increased and we can get the optical energy gap between (3.6-3.9) eV.
The aim of this work is to evaluate some mechanical and physical
properties (i.e. the impact strength, hardness, flexural strength,
thermal conductivity and diffusion coefficient) of
(epoxy/polyurethane) blend reinforced with nano silica powder (2%
wt.). Hand lay-up technique was used to manufacture the composite
and a magnetic stirrer for blending the components. Results showed
that water had affected the bending flexural strength and hardness,
while impact strength increased and thermal conductivity decreased.
In addition to the above mentioned tests, the diffusion coefficient
was calculated using Fick’s 2nd law.
The interest in calcium phosphates arises from the fact that bones contain a high percentage of mineralized calcium phosphate . In this study, pure and biocompatible hydroxyapatite (HAP) powder was successfully synthesized using hen’s egg shell as calcium source and phosphoric acid by precipitation method.The precipitate obtained was subjected to ripenning process for 24 hours, filtered, air dried, and calcined at temperatures of 400,800,900,and 1000 ºC.
X-Ray diffraction(XRD) technique was used to investigate the formation of HAP powder, XRD results revealed the HAP formation and also indicate no occurrence of secondary phases. Fourier Transform Infrared(FT-IR) spectrum shows the characterstic peaks for phosphate and hydroxyl grou
The sol-gel route using an agar gel with calcium nitrate and phosphate solution as starting materials for producing hydroxyapatite (HAP). The product formed were needle like, zigzag and straight fibres. The fibrous products on sintering transformed into stoichiometric HAP with a biological Ca/P ratio of 1.67. The influences of pH, temperature, nature of base and phosphate solution on the growth of fibrous HAP were studied. The pH of the solution was found to greatly influence the growth rate and morphology of the resultant product. The optimum gel temperature was found to be 60oC and sintering temperature of 900oC for 1 hour. The crystalline, thermal, functional and morphological characteristics of the fibrous HAP were investigated.