The effect of D phase polyamide (PA6)on the rheological properties, Young Modulus and the thermal expansion coefficient of two blends groups (bitumen-polyamide) were tested. The first group was for bitumen-PA6 blends and the second group for bitumen blended with polymer resulted from the crystallization of PA6-formic acid solution in water(PAFW).The obtained results proved that adding both types of polyamide has led to a rise in toughness and softening point temperature while the penetration Index approached -3 after adding the polyamide. So, all these changes make bitumen-polyamide blends more suitable for use in hot climate regions. The blends properties were explained according to the reaction that takes place between the polyamide and the epoxy present in the bitumen at temperatures exceeding 200 ° C. However, these changes were more pronounced for mixtures that contained PAFW due to their porous morphological structure, which increased the reaction and made the blends more miscibility even when the addition ratio reached to4%. In the case of PA6, when its ratio in bitumen increased by more than 1%, the unreacted portion of this polymer with epoxy would be mere filler in the mixtures and it did not appear to have a pronounced effect on the properties of bitumen.
Background: Orthodontic tooth movement is characterized by tissue reactions, which consist of an inflammatory response in periodontal ligament and followed by bone remodeling in the periodontium depending on the forces applied. These processes trigger the secretion of various proteins and enzymes into the saliva.The purpose of this study was to evaluate the activity of alkaline phosphatase (ALP) in saliva during orthodontic tooth movement using different magnitude of continuous orthodontic forces. Materials and Methods: Thirty orthodontic patients (12 males and 18 females) aged 17-23 years with class II division I malocclusion all requiring bilateral maxillary first premolar extractions were randomly divided into three groups according to t
... Show MoreThis study was carried out to determine the effects of some environmental variables on biodiversity index value of benthic invertebrates' community in samples that collected monthly from two adjacent sites nearby the confluence of Tigris and Diyala rivers within Baghdad city that’s from November 2007 - October 2008. Results showed differences in chemical and physical characteristics for each river. Where the annual averages of these characteristics in Rivers Tigris and Diyala respectively for: water temperature (20, 19) Cº, pH (8, 8), Dissolved oxygen DO(8,4 ) mg/l , EC(1152,2979)µc/cm , Turbidity (28,74) NTU, Total Hardness of CaCO3 (485,823)mg/l, and finally NO3 (4,6)mg/l. Concerning the biological groups, included types of Insect
... Show MoreBackground: In dentistry, dentist takes the advantages of soft lining materials due to the viscoelastic properties. The major problem is the adhesion of the soft liner with the denture base material. Materials and Methods: Heat cured of high impact acrylic resin specimens prepared with dimensions 75x13x13mm for shear bond strength test, soft lining material (Refit and Mollosil) with a 3-mm thickness and used to join each two acrylic blocks. Also four specimens with the same previous dimensions utilized for chemical and physical surface analysis. The specimens grouped as control (without plasma) and experiment (with oxygen plasma) treated high impact acrylic specimens. Results: Plasma treatment increased the shear bond strength for both Refi
... Show MoreIn this work, varying compositions of SiO2 micro filler were added
with the Polyvinyl Chloride (PVC) and samples have been prepared
using film casting technique. The results have been analyzed and
compared for PVC samples with (1 wt%, 3 wt%, 5 wt% and 10 wt%)
SiO2 micro filler. Mechanical characteristics such as tensile strength,
elongation at break and Young`s modulus were measured for all the
samples, where the tensile strength was increased from 8.39 Mpa for
purified PVC to 16 Mpa for 3% SiO2/PVC composite. Also, thermal
conductivity measurement values illustrated that composite materials
have a good thermal insulation at 10 wt. %, thermal conductivity was
decreased from 0.1684 W/m.
Results of a study of alloys and films with various Pb content have been reported and discussed. Films of of thickness 1.5
The Asphalt cement is produced as a by-product from the oil industry; the asphalt must practice further processing to control the percentage of its different ingredients so that it will be suitable for paving process. The objective of this work is to prepare different types of modified Asphalt cement using locally available additives, and subjecting the prepared modified Asphalt cement to testing procedures usually adopted for Asphalt cement, and compare the test results with the specification requirements for the modified Asphalt cement to fulfill the paving process requirements. An attempt was made to prepare the modified Asphalt cement for pavement construction in the laboratory by digesting each of the two penetration grade Asphalt c
... Show MoreMany cases of gravitational bullets are reported in developed and non-developed countries. However, few papers highlighted these cases in the literature. In our study, we present two cases of gravitational bullets that have an unusual coincidence in the injury characteristics through their ages, and gender, the site of the inlet.