This work concerned with effect of zinc oxide concentrating on the structural and optical properties of (MgO)1-x(ZnO)x thin films. (MgO)1-x(ZnO)x compounds were produced by mixing the two oxides powders accordance to the atomic ratios and compressed as pellets, these pellets were sintered in an oven at temperature1273K for five hours. Thin films from (MgO)1-x(ZnO)x compounds were obtained using pulsed laser deposition technique using Nd:YAG laser . The results of x-ray diffraction as well as UV-Visible- spectrophotometer measurements transmittance of (MgO)1-x(ZnO)x thin films were presented From the x-ray pattern it was observed reflection peaks (200) and (111) for cubic structure MgO and (100),(002) and (101) for ZnO wurtzite-phase reflections planes corresponding to the MgO cubic structure and ZnO wurtzite-phase while the prepared thin films with x content from 0 to 0.75 seemed to gather and rearranges their atoms until reveals some little peaks reveals at x=1.0 which give an indication to attend polycrystalline structure. The optical results declare a reducing of band gap i.e. red shift by the growth of ZnO incorporation in the prepared thin films.The data reveals that energy gap reduces from 4.0 eV to 3.20 eV . This affirms that the ablation of ZMO targets results in a tuneable band gap ZMO thin films. The calculated optical constants are greatly effected by ZnO incorporation in the prepared thin films.
(NiO) 1-x (ZnO) x compounds were prepared with different composition ratios. The compounds were obtained by mixing Nickle oxide and zinc oxide in the appropriate ratio and sintered at 1000°C for six hours. Pulsed laser deposition (PLD) method which is simple and inexpensive method was used to deposit (NiO) 1-x (ZnO) x thin films on glass substrate at ambient temperature. Structural, optical and properties were investigated. The structures investigation obtained from x-ray diffraction showed that the prepared of compound as well as thin films have polycrystalline structure where the diffraction peaks w
The compound Fe0.5CoxMg0.95-xO where (x= 0.025, 0.05, 0.075, 0.1) was prepared via the sol-gel technique. The crystalline nature of magnesium oxide was studied by X-ray powder diffraction (XRD) analysis, and the size of the sample crystals, ranging between (16.91-19.62nm), increased, while the lattice constant within the band (0.5337-0.4738 nm) decreased with increasing the cobalt concentration. The morphology of the specimens was studied by scanning electron microscopy (SEM) which shows images forming spherical granules in addition to the presence of interconnected chips. The presence of the elements involved in the super
Superconducting compound Bi2Sr2-xYxCa2Cu3O10+δ were Synthesized by method of solid state reaction, at 1033 K for 160 hours temperature of the sintering at normal atmospheric pressure where substitutions Yttrium oxide with Strontium. When Y2O3 concentration (0.0, 0.1, 0.2, 0.3, 0.4 and 0.5). All specimens of Bi2Sr2Ca2Cu3O10+δ superconducting compounds were examined. The resistivity of electrical was checked by the four point probe technique, It was found th
In this study, the melting-cooling method was used to prepare the chalcogenide compound S60-Se40-X-PbX. Four samples were obtained by partial replacement of Selenium with Lead in the weight ratios x = 0, 10, 20, and 30, respectively. The materials were mixed separately, ground, placed in quartz ampoules, and heated to 500 degrees Celsius. After conducting several operations on the samples, their insulating properties were studied, represented by the real dielectric constant and the imaginary dielectric constant, and the electrical conductivity was measured as a function of the frequency. It was found that partial replacement plays an impo
This study includes the manufacture of four ternary alloys represented S60Se40-XPbX with weight ratios x = 0, 10, 20, and 30 by the melting point method. The components of each alloy were mixed separately, then placed in quartz ampoules and vacuumed out with a vacuum of roger that 10−4 Torr. The ampule was heated in two stages to avoid sudden dissipation and precipitation of selenium on the inner mass of the quartz tube. The ampoule was gradually heated and kept at 450°C for approximately 4 hours followed by 950°C for 10 hours.at a rate of 10 degrees Celsius, the temperature of the electric furnace
In this manuscript, the effect of substituting strontium with barium on the structural properties of Tl0.8Ni0.2Sr2-xBrxCa2Cu3O9-δcompound with x= 0, 0.2, 0.4, have been studied. Samples were prepared using solid state reaction technique, suitable oxides alternatives of Pb2O3, CaO, BaO and CuO with 99.99% purity as raw materials and then mixed. They were prepared in the form of discs with a diameter of 1.5 cm and a thickness of (0.2-0.3) cm under pressures 7 tons / cm2, and the samples were sintered at a constant temperature o
... Show MoreThe non-linear components has been emphasized for its multiple applications in rewritable recording and data storage devices. Chalcogenide glasses materials are promising due to their high refractive index. In this paper, alloys for Ge30Te70-xSbxglasses semiconductor (where x =0.0, 5, 10, 15 and 20) will be fabricated by melt quenching method. The effect of partial substitution on DC electric power parameters, and its knowledge of electrical conduction mechanisms, were investigated to determine the effect of Antimony on the density of extended states, local states, and in Fermi energy states. The electrical measurements revealed the existence of three conduction mechanis
... Show MoreIn this paper deals with the effect laser irradiation on the optical properties of cobalt oxide (CoO2) thin films and that was prepared using semi computerized spray pyrolysis technique. The films deposited on glass substrate using such as an ideal value concentration of (0.02)M with a total volume of 100 ml. With substrate temperature was (350 C), spray rate (15 ml/min).The XRD diffraction given polycrystalline nature with Crystal system trigonal (hexagonal axes). The obtained films were irradiated by continuous green laser (532.8 nm) with power 140 mW for different time periods is 10 min,20min and 30min. The result was that the optical properties of cobalt oxide thin films affe