Background: In recent years, the immediate loading of dental implants has become more accepted as a standard protocol for the treatment of the edentulous area. Success in implant dentistry depends on several parameters that may improve phenomenon of osseointegration and new bone formation in close contact with the implant. The aim of study was to evaluate the effect of strontium chloride coating of screw shape commercially pure titanium dental implant osseointegration at bone - implant interface by histomorphometric analysis and compare with hydroxyapatite coating at 2 time periods (2 weeks and 6 weeks). Materials and methods: Electrophoretic Deposition Technique (EPD) was used to obtain a uniform coating layer on commercially pure titanium screws. The tibia of 4 white New Zealand rabbits was chosen as implantation sites. Each tibia of rabbit received two screws, one strontium chloride coated and one hydroxyapatite coated and a total 30 histological sections were obtained for each coating material in each period of time. Histomorphometric analysis was performed to measure new bone formed ratio between implant and original bone, after 2 and 6 weeks healing periods. Results: There was increased in new bone formation ratio for the strontium chloride coated implants than hydroxyapatite coated implants and over the two periods of time. There was an increase in the new bone formation ratio at bone-implant interface with time. Conclusion: Coating commercially pure titanium implant with strontium chloride was more efficient in increasing osseointegration at bone implant interface than hydroxyapatite , which was demonstrated by higher new bone formation and maturation at the two periods of time 2 weeks and 6 weeks after implantation. Keywords: Histomorphometric, commercially pure titanium, strontium chloride, hydroxyapatite.
A rapid and sensitive method for the determination of amoxicillin trihydrate (AMXT) based on the diazo-coupling reaction was studied. Sulphanilic acid diazotizes with nitrite ion in acidic medium to produce a water soluble, colorless diazonium ion, which subsequently coupled with AMXT to form a colored azo dye in the alkaline medium, having maximum absorption at 455 nm. The calibration graph showed that Beer's law is obeyed over the concentration range of 0.3 – 30.0 μg/mL of AMXT, with the detection limit of 0.15 μg/mL and molar absorptivity was 2.3 × 104 L/mol.cm. The accuracy and the precision were acceptable depending upon the values of error percentage and relative standard deviation. The influence of common interfer
... Show MoreBackground: The development of orthodontic biomaterials that attract less biofilm has been a goal for decades. Adhesion and colonization of cariogenic streptococci are considered to play key roles in the development of enamel demineralization related to orthodontic materials. The aim of this study was to quantitatively evaluate the Mutans streptococci adhesion to coated orthodontic archwires (Epoxy and Teflon) and uncoated archwires (stainless steel and nickel-titanium) with respect to incubation time in the presence and absence of saliva. Material and Method: Six types of archwires stainless steel and nickel titanium with two type of coating (Epoxy, Teflon) were used in this study. Twelve specimens of each archwire were incubated in steri
... Show MoreIn recent years , the interest in gold (III) species have gained more and more attention for cancer chemotherapy , this was stimulating by the possibility to develop new agents with mode of action and clinical profile different from the established platinum metalodrugs.
With this frame, recently new square planar Au(III) complexes (Au(L)(L')n); where L=SCH2COO- ; L'=HSCH2COO- had been synthesized with S/O – donor ligands.
In this article and by the aim to replace, one of (L') ligand by anion chloride ligand (which supposedly more relevant for the biodistribution of the compound than for its pharmacodynamic effects), new complex (Au(L')
The corrosion behavior of bare and chemical conversion coated (through anodizing) aluminum ASA 606 I in stagnant chromic acid solutions . Solutions of 2, 6 & J O wt. % Cr03 at 45°C, have been investigated using polarization technique. The anodizing experiments were conducted under fixed conditions of 35 minute exposure time and 30 volt supplied voltage. The most important feature achieved was the great difference in behavior between the anodic polarization curves for bare and anodized aluminum in different concentrations of chromic acid solutions.
Background: this study aimed to evaluate the effect of addition of hydroxyapatite micro filler in three concentrations (5%, 10%, 15%) on surface roughness, impact strength, flexural strength and hardness. Material and methods: One hundred sixty acrylic samples were used in this study,40 samples were used for each test(impact strength ,flexural strength ,hardness and surface roughness).The test group divided into four subgroups(n=10) for controlgroup,5%,10% ,15%H,A.concentration addition groups .Impact testing device, flexural strength testing device, shore hardness tester and profilometer device were used to measure the four tests examined in this study. Results: the results showed a significant increase in impact strength, hardness in all
... Show MoreObserved visually prominent lumps on the surface of the lung or embedded in lung tissue and microscopically Register Anfaj thrombosis with pulmonary carcinoma that took shape food or with the composition of the vesicles papillomavirus lining cells cubic vertical or connective tissue and increase
In this study, generation of elliptical gears with different teeth profiles of crowned involute, double circular arc (DCA), and combined (crowned involute with DCA) has been developed. The resulting mathematical equations have been computerized and feed to CNC end mill machine to manufacture elliptical gear models with different profiles. These models are investigated in plane polariscope to show the resulting stresses under certain load. Comparison of photo-elastic stress results shows that combined elliptical gears with DCA side as a loaded side have a minimum resulting contact stress with a reduction percentage of 40% compare with contact stresses in counterpart elliptical gear of involute profile (which is commonly u
... Show More