Background: The bonded orthodontic retainer constructed from multistrand wire and composite is an efficient esthetic retainer, which can be maintained long-term. Clinical failures of bonded orthodontic retainers, most commonly at the wire/composite interface, have been reported. This in vitro investigation aimed to evaluate the tensile forces of selected multistrand wires and composite materials that are available for use in the construction of bonded fixed retainers. Materials and Methods: The study sample includes 120 wires with three types of retainer wires (3 braided strands\ Orthotechnology, 8 braided strands\ G&H Orthodontics, 6 coaxial strands\ Orthoclassic wires), two types of adhesive (flowable\ Orthotechnology, non flowable\ G&H Orthodontics composites) and two thickness of the adhesive (1mm, 2mm). The samples were prepared for each composite in which a wire was embedded; then the composite was light cured for 40 seconds and the specimens were stored in artificial saliva at 37°C in the incubator for 24 hours. The ends of the wire were drawn up and tensile force was applied through Tinius-Olsen universal testing machine until the resin failed and the results were recorded in Newton (N). Results: Statistical analysis showed that there was a highly significant difference (P ≤ 0.01) among the mean values of tensile forces of the three types of retainer wires in each thickness of composite with exception of a non significant difference (P > 0.05) between (3 braided) and (8 braided) and a non significant difference (P > 0.05) between (3 braided) and (6 coaxial) in both thickness of composite, a highly significant difference (P ≤ 0.01) between the two thickness of both composite types in each wire type and a highly significant difference (P ≤ 0.01) between the two types of composite in each wire type of both thickness of composite. Conclusion: The result of this study revealed that the 8 braided strands retainer wire shows the highest values of tensile force among the tested retainer wires, the non flowable composite demonstrates a higher tensile force than the flowable composite and increasing the thickness of composite overlying the wire increased the force required to detach the wire from the composite.
Effects of Ozonated Water on Micro Leakage between Enamel and Fissure Sealants Prepared by Different Etching Technique (An in vitro Study), Baraa M Jabar*, Muna S Khalaf
Soils that cause effective damages to engineer structures (such as pavement and foundation) are called problematic or difficult soils (include collapsible soil, expansive soil, etc.). These damages occur due to poor or unfavorited engineering properties, such as low shear strength, high compressibility, high volume changes, etc. In the case of expansive soil, the problem of the shrink-swell phenomenon, when the soil reacts with water, is more pronounced. To overcome such problems, soils can be treated or stabilized with many stabilization ways (mechanical, chemical, etc.). Such ways can amend the unfavorited soil properties. In this review, the pozzolanic materials have been selected to be presented and discussed as chem
... Show MoreBackground: Calcium hydroxide and calcium-silicate materials used as direct pulp capping materials. The aims of this in vitro study is to compare among these materials in, the calcium ion release and pH change in soaking water after immersion of materials’ specimens in deionized water. Also Solubility and water sorption of materials’ specimens measured after soaking time. Calcium-silicate materials used were Biodentine, TheraCal and MTA Plus. Materials and methods: Four materials used in this study; Urbical lining (as control group), Biodentine, TheraCal and MTA Plus. Ten discs fabricated from each tested material, by using plastic moulds of 9 mm diameter and 1 mm thickness. Each specimen was immersed in 10 ml of d
... Show MoreBackground: The aim of this study was to evaluate and compare the apical microleakage around retrograde cavities prepared with ultrasonic technique and filled with (Biodentineâ„¢) Materials and methods: 40 extracted single rooted human permanent maxillary teeth with mature apices were selected. The roots were prepared chemo-mechanically using k-files with crown-down technique and then obturated with lateral condensation gutta-percha technique. Teeth were divided into four main groups according to the cavity preparation method either manual or ultrasonic technique: Group A (n=10): A class I retrograde cavity at root end was prepared with traditional handpeice equipped and placement of Biodentine with manual condensation. Group B (n=10):
... Show MoreBackground: The aim of this study was to evaluate and compare the apical microleakage around retrograde cavities prepared with ultrasonic technique and filled with (Biodentineâ„¢) Materials and methods: 40 extracted single rooted human permanent maxillary teeth with mature apices were selected. The roots were prepared chemo-mechanically using k-files with crown-down technique and then obturated with lateral condensation gutta-percha technique. Teeth were divided into four main groups according to the cavity preparation method either manual or ultrasonic technique: Group A (n=10): A class I retrograde cavity at root end was prepared with traditional handpeice equipped and placement of Biodentine with manual condensation. Group B (n=10):
... Show MorePlant regeneration protocols were developed for medicinally important anise (Pimpinella anisum L.) that successfully achieved from seeds. Seeds were sterilized and inoculated on Murashige and Skoog (MS) medium with and without gibberellins (GA3) until full germination. The highest percentage of germination (100%) was recorded on MS medium treated with 2.0 mg/L GA3 after 7 days. For shoot proliferation, different concentrations of 6- benzyl adenine BA (1, 1.5, 2 mg/L) were used. To enhance shoot induction, 0.1 mg/L of naphthalene acetic acid (NAA) and 0.01 mg/L of thidiazuron (TDZ) were tested along with BA. Direct regenerated shoots were obtained on MS medium supplemented with BA alone (2mg/L) which gave (7shoot/explant), while the presence
... Show MorePsychological damage is one of the damages that can be compensated under the fault of negligence in the framework of English law, where the latter intends to include an enumeration of civil errors on the basis of which liability can be determined, and aims under each of these errors to protect a specific interest (for example, defamation protects Among the damage to reputation and inconvenience are the rights contained on the land), and the same is true for the rest of the other errors. Compensation for psychological damage resulting from negligence has raised problems in cases where the psychological injury is "pure", that is, those that are not accompanied by a physical injury, which required subjecting them to special requirements by the
... Show MoreBackground: The bond strength of the root canal sealers to dentin is very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate and compare the push-out bond strength of root filled with total fill Bioceramic, AH Plus and Gutta-flow®2 sealers using GuttaFusion®obturation system versus single cone obturation technique. Materials and method: sixty of mandibular premolars teeth with straight roots were used in this study, these roots were instrumented using Reciproc system, instrumentation were done with copious irrigation of 3 mL 5.25% sodium hypochlorite solution (NaOCl) during all the steps of preparation, and smear layer will be removed with 1 ml of 17% EDTA kept in
... Show MoreBackground: The bond strength of the root canal sealers to dentin is very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate and compare the push-out bond strength of root filled with total fill Bioceramic, AH Plus and Gutta-flow®2 sealers using GuttaFusion®obturation system versus single cone obturation technique. Materials and method: sixty of mandibular premolars teeth with straight roots were used in this study, these roots were instrumented using Reciproc system, instrumentation were done with copious irrigation of 3 mL 5.25% sodium hypochlorite solution (NaOCl) during all the steps of preparation, and smear layer will be removed with 1 ml of 17% EDTA kept in
... Show More