ABSTRACT Background: Color changes that are detectable to human eye can affect the esthetic appearance of ceramic veneers. The purpose of this study was to evaluate and compare the effect of artificial accelerated aging on the color of ceramic veneers cemented with different resin cements. Materials and Methods: Sixty discs were prepared with 0.5 mm thickness, 30 discs made from IPS e.max press (Ivoclar Vivadent) and 30 discs were made from VITA Enamic (VITA Zahnfabrik). The discs were cemented with three resin cements: Variolink Veneer MV 0 shade (Ivoclar Vivadent), Rely X veneer Translucent shade (3M ESPE) and NX3 Nexus Clear shade (Kerr Corporation) with 0.1 mm thickness. The spectrophotometer Easyshade Advance was used to measure the color parameters (Lightness, axis a* of chroma and axis b*of chroma) immediately after cementation, after 150 and 300 hours of aging. The specimens were subjected to artificial accelerated aging in Accelerated Weathering Tester. Color change greater than 3.3 was considered unacceptable. One-way ANOVA, paired t-tests and Bonferroni adjusted t-test were used for statistical analysis (p <0.05). Results: Artificial aging caused high significant color change in both ceramic types, but there were non-significant difference in color change among the three resin cements used. The color change was between1.997-14.8 after 150 hours and it was between 2.179-15.68 after 300 hours. The color change of e.max discs after aging were within acceptable limit<3.3 whereas Vita Enamic specimens had shown unacceptable color change >3.3 after aging. Conclusions: The majority of color change after aging related to veneering materials while resin cement have only slight effect on color change after aging. IPS e.max had shown an acceptable color change after aging, so it is suitable for fabrication of restorations in esthetic zone while Vita Enamic should not be used in esthetic zone since it has poor color stability according to the results of this study.
In this paper the effect of mixing TiO2 nanoparticles with epoxy resin is studied. The TiO2 nanoparticles would be synthesis and characterized by scanning electron microscopy (SEM), XRD FTIR, for two particle sizes of 50 and 25 nm. The thermal conductivity is measured with and without composite epoxy resin; the results showed that the thermal conductivity was increased as nanoparticle concentration increased too. The thermal conductivity was increased as particle size decreased.
Objective Advantageous properties of silicone elastomer made it one of the favorable materials in maxillofacial prosthesis construction, but these properties may change after months of usage or after pigments addition. This study aimed to define the optimum concentration for a mixture of two types of intrinsic pigments that added to VST-50 maxillofacial silicone material and study their effects on mechanical properties before and after artificial aging. Methods After the pilot study was conducted, 0.1% by weight of rayon flocking and 0. 2% by weight of burnt sienna intrinsic pigment concentration was selected because of improvement in tested mechanical properties of VST-50 maxillofacial silicone. A total of one hundred and eighty samples we
... Show MorePurpose: To evaluate the effect of different surface treatments on shear bond strength between dentin and IPS e.max lithium disilicate glass-ceramic. Materials and Methods: Eighteen extracted third molars were embeded in epoxy resin. The tooth was sectioned vertically in mesiodistal direction using a low speed hard tissue microtome. The buccal and lingual surfaces of each section were ground flat using 600 grit Silicone carbide paper. Eighteen ceramic discs consisted of lithium disilicate glass-ceramic were prepared with a diameter of 4.7mm and height of 2.2mm. The discs were divided in two groups (n=10): (1) IPS e.max treated with hydrofluoric acid and Monobond Plus (MBP) and (2) IPS e.max treated with Monobond Etch &Prime (MBEP). The toot
... Show MoreThis research aims to find how three different types of mouthwashes affect the depth of artificial white spot lesions. Teeth with various depths of white spot lesions were immersed in either splat mouthwash, Biorepair mouthwash, Sensodyne mouthwash, or artificial saliva (control)twice daily for one minute for 4 weeks and 8 weeks at 37°C. After this immersion procedure, lesion depth was measured using a diagnosed pen score. A one-way analysis of variance, Dunnett T3 and Tukey's post hoc α = .05 were used to analyze the testing data. Splat mouthwash enhanced the WSL remineralization and made the lowest ΔF compared with other mouthwashes in shallow and deep enamel after 4 and 8 weeks of treatment. In the repair groups, after 4 weeks
... Show MoreBackground: Maxillary first premolar with wide MOD cavity more susceptible to fracture. The aim of this study was to assess the influence of cavity design for cusp coverage on the fracture resistance of weakened maxillary first premolar restored with CAD/CAM hybrid ceramic versus nanohybide composite. Materials and Methods: Fifty six intact maxillary first premolars of approximately comparable sizes were divided into seven groups eight for each: Group A: Intact teeth (control group); Group B: teeth prepared for MOD inlay; Group C: teeth prepared for MOD onlay covering the lingual cusp; Group D: teeth prepared for MOD covering buccal and lingual cusps ,the previous three groups indirectly restored with nanohybrid composite (3M ESPE Z 250 X
... Show MoreABSTRACT Background: Improving the properties of heat- cured and self-cured acrylic resin have been studied by many researchers. However, little studies concerned with visible light cured resin (VLCR) improved through addition of nanofiller are available. The purpose of this study was to evaluate some properties of (VLCR) after addition of SiO2 nanofiller. Materials and Methods: SiO2 nanofiller were added to (VLCR) tray material after being dissolved in tetrahydrofuran (THF) solvent. According to the pilot study 2% SiO2 nanofiller addition exhibited better properties than the other percentages (1%, 3%). The main study conducted involved (100) specimens divided into 5 groups according to the test included. (20) Specimens were selecte
... Show MoreBackground: The desire for an attractive appearing fixed orthodontic appliance fueled the use of ceramic brackets and clear accessories. Elastics are one of the most versatile materials available to orthodontists so studying their effect on the esthetic appearance is important. This an in vivo study, conducted to evaluate the effect of exposing stretched clear elastomeric ligatures to the oral environment from four different companies (OrthoTechnology, Morelli, Ortho Organizer, and Ormco). Materials and Methods: A total of 240 elastomeric modules were examined, 60 modules from each brand. Each of the 60 patients enrolled in the study, received 4 elastomeric modules on the 4 lower incisors, one from each brand. The specimens were placed on t
... Show MoreIn vitro tests have been carried out to find out the efficacy of watery extracts of garlic Allium sativum and hot pepper Capsicum spp. against the trophozoites of Entamoeba histolytica cultivated in liver infusion agar media at 37 c . The doses of ( 0.01, 0.05 ,0.1, 0.5, 1 ml )of garlic and hot pepper watery extracts were added to certain number of E. histolotica trophozoits for exposure time of 24 hrs., the mortality percentage of trophozoites treated with garlic extract were ( 14.82 %, 31.05% ,46.16% , 64.29% , 92.7%) respectively , these percentages were very close to that obtained from the treatment with the hot peper extract which were (17.86%, 32% , 44% ,66.67% ,100%) respectively . Generally these results showed that the ga
... Show MoreIn this work, the effect of ceramic coating on performance, exhaust gas temperature and gases emissions of diesel engine operated on diesel fuel and biodiesel blends was investigated. A conventional four stroke, direct injected, single cylinder, diesel engine was tested at constant speed and at different load conditions using diesel fuel and biodiesel blends. The inlet and exhaust valves, the head of piston and cylinder head of the engine were coated by ceramic materials. Ceramic layers were made of (210-240) μm of Al2O3 and (30-60) μm of 4NiCr5Al as a bond coat for inlet and exhaust valves and (350-400) μm of YSZ and (50-100) μm of 4NiCr5Al as a bond coat for head of piston and (280-320) μm of Sic and (40-80) μm of 4NiCr5Al as a b
... Show More