ABSTRACT Background: Color changes that are detectable to human eye can affect the esthetic appearance of ceramic veneers. The purpose of this study was to evaluate and compare the effect of artificial accelerated aging on the color of ceramic veneers cemented with different resin cements. Materials and Methods: Sixty discs were prepared with 0.5 mm thickness, 30 discs made from IPS e.max press (Ivoclar Vivadent) and 30 discs were made from VITA Enamic (VITA Zahnfabrik). The discs were cemented with three resin cements: Variolink Veneer MV 0 shade (Ivoclar Vivadent), Rely X veneer Translucent shade (3M ESPE) and NX3 Nexus Clear shade (Kerr Corporation) with 0.1 mm thickness. The spectrophotometer Easyshade Advance was used to measure the color parameters (Lightness, axis a* of chroma and axis b*of chroma) immediately after cementation, after 150 and 300 hours of aging. The specimens were subjected to artificial accelerated aging in Accelerated Weathering Tester. Color change greater than 3.3 was considered unacceptable. One-way ANOVA, paired t-tests and Bonferroni adjusted t-test were used for statistical analysis (p <0.05). Results: Artificial aging caused high significant color change in both ceramic types, but there were non-significant difference in color change among the three resin cements used. The color change was between1.997-14.8 after 150 hours and it was between 2.179-15.68 after 300 hours. The color change of e.max discs after aging were within acceptable limit<3.3 whereas Vita Enamic specimens had shown unacceptable color change >3.3 after aging. Conclusions: The majority of color change after aging related to veneering materials while resin cement have only slight effect on color change after aging. IPS e.max had shown an acceptable color change after aging, so it is suitable for fabrication of restorations in esthetic zone while Vita Enamic should not be used in esthetic zone since it has poor color stability according to the results of this study.
This paper presents a sight about the chemical structure deformation of poly (ethylene-co-vinyl acetate) (EVA) samples according to the change ratio of rate constant values. Spectroscopy kinetics fluorescence curves are fitted for two characteristic wavelength domains of fluorescent intensities. The short wavelengths (320-400 nm) domain show spectra overlapping, while at long wavelengths (400-800 nm) domain spectra are arranged in regular for each specific accelerated aging time. The ratio of kinetics rate constant at long wavelengths to kinetics rate constant of short wavelengths is the criterion of the degree chemical structure deformation. Molar extrin
... Show MoreBackground: The demand for better esthetic during orthodontic treatment has increased nowadays, so orthodontists starting using esthetic arch wires, brackets and ligatures.Tooth colored brackets were introduced in different types of materials. Sapphire ceramic brackets are one type of esthetic brackets and their color stability remains the main concern for the clinicians and patients at the same time. The present study design to evaluate the effect of three different staining materials (pepsi, black tea and cigarette smoke) on the stainability of sapphire ceramic brackets bonded with three types of light cure orthodontic adhesives which include: Resilience, Enlight and Transbond. Materials and Methods: The sample consisted of three hundre
... Show MoreBackground: The marginal fit is the most characteristic that closely related to the longevity or success of a restoration, which is absolutely affected by the fabrication technique. The objective of present in vitro study was to evaluate the effect of four different CAD/CAM systems on the marginal fit of lithiµm disilicate all ceramic crowns. Materials and Methods: Adentoform tooth of a right mandibular first molar was prepared to receive all ceramic crown restoration with deep chamfer finishing line (1mm) and axial reduction convergence angle of 6 degree, dentoform model duplicated to have Nickel-Chromiµm master die. Thirty two stone dies produce from master die and distributed randomly in to four groups (8 dies for each group) accor
... Show MoreBackground: Coated aesthetic archwires are currently the existing solutions for the esthetic problem, but the color of these archwires tends to change overtime. This study was aimed to evaluate the color stability of different types of esthetic archwires from four different companies at different time periods after immersion of two different staining drinks which are tea and Pepsi cola. Materials and methods: 48 specimens were prepared, each specimen contains 10 aesthetic archwires; and were divided according to type of solution into two groups: A (tea) &B (Pepsi cola); each group contained 24 specimens (12 specimens were immersed in the staining solution as 4 specimens for each time intervals and 12 specimens were immersed in distilled wa
... Show MoreBackground: The aim of this study was to evaluate the shear bond strength (SBS) and adhesive remnant index (ARI) of different orthodontic adhesive systems after exposure to aging media (water storage and acid challenge). Materials and methods: Eighty human upper premolar teeth were extracted for orthodontic purposes and randomly divided into two groups (40 teeth each): the first group in which the bonded teeth were stored in distilled water for 30 days at 37°C, and the second group in which the bonded teeth were subjected to acid challenge. Each group was further subdivided into four subgroups (10 teeth each) according to the type of adhesive system that would be bonded to metal brackets: either non-fluoride releasing adhesive (NFRA),
... Show MoreBackground: One of the drawbacks of vital teeth bleaching is color stability. The aim of the present study was to evaluate the effects of tea and tomato sauce on the color stability of bleached enamel in association with the application of MI Paste Plus (CPP-ACPF). Materials and Methods: Sixty enamel samples were bleached with 10% carbamide peroxide for two weeks then divided into three groups (A, B and C) of 20 samples each. After bleaching, the samples of each group were subdivided into two subgroups (n=10). While subgroups A1, B1 and C1 were kept in distilled water, A2, B2, and C2 were treated with MI Paste Plus. Then, the samples were immersed in different solutions as follow: A1 and A2 in distilled water (control); B1 and B2 in black
... Show MoreBackground: This in vitro study was carried out to evaluate the effects of various veneering dentin ceramic thicknesses and repeated firings on the color of lithium disilicate glass-ceramic (IPS e.max Press) and zirconium-oxide (IPS ZirCAD) all-ceramic systems, measured by clinical spectrophotometers (Easyshade Advance 4.0) . Materials and methods: The 72specimens cube-shaped have the dimension of about 11 mm in width, 14 mm in length, 1mm in thickness, these cores divided into 3 groups according to the type of material each group have (24)core specimens. Each group had been divided into three sub-groups (each having 8 specimens) according to veneering with dentin ceramic thicknesses: as 0.5, 1, or 2 mm (n=8). IPS e.max press and ZirCAD c
... Show MoreThe photooxidative degradation process of plastics caused by ultraviolet irradiation leads to bond breaking, crosslinking, the elimination of volatiles, formation of free radicals, and decreases in weight and molecular weight. Photodegradation deteriorates both the mechanical and physical properties of plastics and affects their predicted life use, in particular for applications in harsh environments. Plastics have many benefits, while on the other hand, they have numerous disadvantages, such as photodegradation and photooxidation in harsh environments and the release of toxic substances due to the leaching of some components, which have a negative effect on living organisms. Therefore, attention is paid to the design and use of saf
... Show MoreBackground: the aim of this study was to evaluate the effect of different surface acids treatments (37%phospjoric acid, 5%hydrofluoric acid, 1.23 acidulated phosphate fluoride) of feldspathic ceramic VITA 3D MASTER , and the effect of thermocycling on shear bond strength using a ceramic repair kit (ivoclar/vivadent). Material and Methods: sixty Nickel-Chromium metal base plates were prepared(9mm diameter,3mm depth) using lost wax technique, 2mm thick layer of ceramic(VITA 3D MASTER) fused to metal plates, all specimens were embedded in acrylic resin blocks except their examined surfaces and divided into 3 main groups 20 specimens each, Grp A: treatment with 37%phosphoric acid for 2 mins, Grp B: etching with 5% hydrofluoric acid for 2mins,
... Show More