The Ge0.4Te0.6 alloy has been prepared. Thin films of Ge0.4Te0.6 has been prepared via a thermal evaporation method with 4000A thickness, and rate of deposition (4.2) A/sec at pressure 2x10-6 Torr. The A.C electrical conductivity of a-Ge0.4Te0.6 thin films has been studied as a function of frequency for annealing temperature within the range (423-623) K, the deduced exponent s values, was found to decrease with increasing of annealing temperature through the frequency of the range (102-106) Hz. It was found that, the correlated barrier hopping (CBH) is the dominant conduction mechanism. Values of dielectric constant ε1 and dielectric loss ε2 were found to decrease with frequency and increase with temperature. The activation energies have been calculated for the annealed thin films.
The work was carried out in two stages. The first stage concerned
with study of silicon carbide (SiC) ratio (1.5, 2.5, 3.5, and 4.5 wt%)
effect on the Thermal conductivity of polyvinyl chloride (PVC); and
the second stage concerned with the UV – weatherizing (25, 50, and
75 hr), thermal aging (40, 50, and 60 °C), and rain- weatherizing (1,
2.5, and 4 hr) effect on the samples involved. Thermal conductivity
results proved that there was slight increase in thermal conductivity
by (SiC) loading; it increased from 0.17 W/m.K for PVC to 0.19
W/m.K for 4.5% SiC/PVC; where as it was systematically decreased
by UV- weatherizing, thermal aging, and rain- weatherizing. This
property is in a good agreement with gene
The study aims to build a model that enhances trust-building for public and private banks to compare and determine the significant differences between public and private banks, by testing the impact of governance mechanisms (transparency, accountability, justice, independence, and social responsibility) (Agere, 2000) on trust-building strategies (trust and trust building, people management, work relations, training and development, leadership practices, and communications) (Ngalo, 2011; Stone et al., 2005), to indicate the level of employees’ awareness of the theoretical contents of the two variables and their importance to banking work, with the aim of improving performance. The main question is the role of governance mechanisms
... Show MoreGaN thin films were deposited by thermal evaporation onto
glass substrates at substrate temperature of 403 K and a thickness of
385 nm . GaN films have amorphous structure as shown in X-ray
diffraction pattern . From absorbance data within the range ( 200-
900 ) nm direct optical energy gap was calculated . Also the others
optical parameters like transmittance T, reflectance R , refractive
index n , extinction coefficient k , real dielectric constant 1 Î , and
imaginary dielectric constant 2 Î were determined . GaN films
have good absorbance and minimum transmittance in the region of
the visible light .
The paper reports the influence of annealing temperature under vacuum for one hour on the some structural and electrical properties of p-type CdTe thin films were grown at room temperature under high vacuum by using thermal evaporation technique with a mean thickness about 600nm. X-ray diffraction analysis confirms the formation of CdTe cubic phase at all annealing temperature. From investigated the electrical properties of CdTe thin films, the electrical conductivity, the majority carrier concentration, and the Hall mobility were found increase with increasing annealing temperatures.
Newly acid hydrazide was synthesized from ethyl 2-(2,3-dimethoxyphenoxy) acetate (2), which is cyclized to the corresponding 4-amino-1,2,4-triazole (3). Five newly azo derivatives (4a-e) were synthesized from this 1,2,4-triazole by converting the amine group to diazonium salt then reacted with various substituent phenol,as well three newly imine derivatives (5a-c) were synthesized from reacting the amine group of compound (3) with three aryl aldehyde. The thermal electro conductivity of these compounds was tested at 30, 50, 75 and 100 áµ’C. compound 4a showed interesting electro conductivity at 75áµ’C as well 5a
... Show MoreIn this work, silicon nitride (Si3N4) thin films were deposited on metallic substrates (aluminium and titanium sheets) by the DC reactive sputtering technique using two different silicon targets (n-type and p-type Si wafers) as well as two Ar:N2 gas mixing ratios (50:50 and 70:30). The electrical conductivity of the metallic (aluminium and titanium) substrates was measured before and after the deposition of silicon nitride thin films on both surfaces of the substrates. The results obtained from this work showed that the deposited films, in general, reduced the electrical conductivity of the substrates, and the thin films prepared from n-type silicon targets using a 50:50 mixing ratio and deposited on both
... Show MoreWe have theoretically investigated the in-plane lattice thermal conductivity of Zn4Sb3single quantum well structure taking into account spatial confinement of phonons. The calculations were carried out for free-surface quantum wells with thickness 8.5nm in the room temperature. We show that the lattice thermal conductivity is a significant reduce. The reduction is mostly due to the drop in the average group velocity caused by the spatial confinement of acoustic phonons and the corresponding increase in phonon relaxation rates. The predicted decrease is important for the anticipated applications of Zn4Sb3 nanostructure materials for room-temperature thermoelectric devices. Our theoretical results are in a good agreement with available exp
... Show MoreA.C electrical conductivity and dielectric properties for poly
(vinyl alcohol) (PVA) /poly (ethylene oxide) (PEO) blends undoped
and doped with multi-walled carbon nanotube (MWCNTs) with
different concentrations (1, and 3 wt %) in the frequency range
(25x103 - 5x106 Hz) were investigated. Samples of (PVA/PEO)
blends undoped and doped with MWCNTs were prepared using
casting technique. The electrical conductivity measurements showed
that σA.C is frequency dependent and obey the relation σA.C =Aωs for
undoped and doped blends with 1% MWCNTs, while it is frequency
independent with increases of MWCNTs content to 3%. The
exponent s showed proceeding increase with the increase of PEO
ratio (≥50%) for undope