The galvanic corrosion of the (Cu - Fe), (Cu - Zn) and (Fe - Zn) couples have been investigated in 3.5% NaCl solution, 40ºC, different velocities (Re = 5000, 10000 and 15000) and different area ratio’s of cathode to anode (AR= 0.5,1 and 2), by using commercial metal pipe (cylindrical tube).The Zero Resistance Ammeter has been used to measure the galvanic current (Ig) and galvanic potential (Eg) with time. The galvanic current density increases with increasing velocity (Re) and the area ratio (AR). The galvanic potential (Eg) is shifted to less negative with increasing velocity (Re) and the area ratio (AR). A statistical relations for the galvanic current density and galvanic potential as a function of (Re). and the area ratio had been created depending on Quasi-Newton method. There is good agreement between experimental and predicted results.
In the present study, a total of 245 flour samples were collected from 49 mills on both sides of Baghdad city (Al- Karkh and Al- Resafa), during the period from 1/6 - 1/12/ 2015 to detect the prolportion of iron added to the flour samples. It is found that only 45% of mills produced flour contain the prescribed percentage of iron (30-60 ppm) while 51.9% of the mills produced flour at rate is less or much more than the prescribed percentage, while only 4.1% of the mills were not added iron to the flour.
Separation of Trigonelline, the major alkaloid in fenugreek seeds, is difficult because the extract of these seeds usually contains Trigonelline, choline, mucilage, and steroidal saponins, in addition to some other substances. This study amis to isolate the quaternary ammonium alkaloid (Trigonelline) and choline from fenugreek seeds (Trigonella-foenum graecum L.) which have similar physiochemical properties by modifying of the classical method. Seeds were defatted and then extracted with methanol. The presence of alkaloids was detected by using Mayer's and Dragendorff's reagents. In this work, trigonilline was isolated with traces of choline by subsequent processes of purification using analytical and preparative TLC techniques.
... Show MoreA potentiostatic study of the behaviour of Inconel (600) in molar sulphuric acid has been carried out over the temperature range 293-313 K. Values have been established for the potentials and current densities of the corrosion, active-passive transition, passivity and transpassive states. For corrosion, the current density (ic) and potential (Ec) have been determined from well-defined Tafel lines. The potential and current density prior to the commencement of passivity have been obtained corresponding respectively to the critical potential (Ecr( and to the current density (icr) for the active-passive transition state. The passive range was defined by the respective potentials and current densities for passive film formation and dissolutio
... Show MoreNiO nanoparticle synthesis by chemical method and characterized by XRD with crystal size 11.72
nm and grain size 13 nm from FESEM image also NiO micro used ,two NiO as an additive to evaluate the
possibility of producing photodegradable polymers, the practical application of solid-phase photocatalytic
degradation of polyvinyl chloride (PVC- NiO composite films) was investigated. PVC has a negative impact
on the environment since its polymer degrades slowly, yet it has a wide range of industrial applications and
the amount used shows no evidence of diminishing use. Thus, a synthesis of modified PVC- NiO micro and
nano has been studied with 0, 50, 100, 150, 200, 250, and 300 (hours) as irradiation time a
CuO nanoparticles were synthesized in two different ways, firstly by precipitation method using copper acetate monohydrate Cu(CO2CH13)2·H2O, glacial acetic acid (CH3COOH) and sodium hydroxide(NaOH), and secondly by sol-gel method using copper chloride(CuCl2), sodium hydroxide (NaOH) and ethanol (C2H6O). Results of scanning electron microscopy (SEM) showed that different CuO nanostructures (spherical and Reef) can be formed using precipitation and sol- gel process, respectively, at which the particle size was found to be less than 2 µm. X-ray diffraction (XRD)manifested that the pure synthesized powder has no inclusions that may exist during preparations. XRD result
... Show MoreThe study aimed to increase the biological value of white bean. The effect of different concentrations 0.01 ,0.02,0.03,and 0.04 M of sodium sulfite solutions for 1hr at 70 ºC on the trypsin inhibitors activity, protein isolate and protein solubility of complete and dehulling white bean flour were studied.Trypsin inhibitors activity were reduced by 42.97, 58.69, 68.59 and 69.58% in complete white bean flour at 0.01 ,0.02, 0.03, 0.04 M respectively, while the corresponding values were 50.43, 61.00, 75.61 and 85.66% respectively in dehulling white bean flour .Protein isolate value was 13.41% and protein solubility was 2.2% in control sample, Furthermore, the using of chemical treatment showed that protein isolate was reduced gradually and
... Show MoreFood fortification has an important and necessary role in compensating for the shortage of nutritional micronutrients, especially in developing and least developed countries. So, 12 samples of flour available in the local market, whether imported or locally produced flour, were obtained during 2019. The amount of base metal of the necessary iron element in the flour models studied which are available in local markets, measured by spot testing and was compared with the values that should be added according to the specification Iraqi standard. Results revealed the qualitative evaluation of iron in locally produced flour does not conform to the Iraqi standard and is almost free of any reinforcement. While the percentage of imp
... Show MoreMetal oxide nanoparticles, including iron oxide, are highly considered as one of the most important species of nanomaterials in a varied range of applications due to their optical, magnetic, and electrical properties. Iron oxides are common compounds, extensive in nature, and easily synthesized in the laboratory. In this paper, iron oxide nanoparticles were prepared by co-precipitation of (Fe+2) and (Fe+3) ions, using iron (II and III) sulfate as precursor material and NH4OH solution as solvent at 90°C. After the synthesis of iron oxide particles, it was characterized using X-ray diffraction (XRD), infrared spectroscopy (FTIR), and scanning electron microscopy (SEM). These tests confirmed the obtaining o
... Show More