In this work, silver (Ag) self-metallization on a polyimide (PI) film was prepared through autocatalytic plating. PI films were prepared through the solution casting method, followed by etching with potassium hydroxide (KOH) solution, sensitization with tin chloride (SnCl2), and the use of palladium chloride (PdCl2) to activate the surface of PI. Energy-dispersive X-ray analysis (EDX) showed the highest peak in the (Ag) region and confirmed the presence of AgNPs. The diffraction peaks at 2θ = 38.2°, 44.5°, 64.6°, and 78.2° represented the 111, 200, 220, and 311 planes of Ag, respectively. The FT–IR analysis for Ag-metalized PI showed that the =C-O-C= stretching absorption bands at 1735 cm−1 had no changes in position, only a significant difference in peak size at the deposition time increase. The formation of new bands (N–H stretching absorption band and N–C stretching band) assigned at 2325 and 955 cm−1 indicated strong coordination between N atoms and silver nanoparticles. The C–C stretching and = C–H plane vibration band at 1488 and 1117 cm−1 are shifted to 1413 and 1112 cm−1, indicating the silver nanoparticles' interaction with the polymer backbone. The thermal stability of PI- and Ag-metalized PI films at various deposition times (5, 10, and 15 min) was examined using thermogravimetric analysis (TGA). For PI, T0, T5, T10, and Tmax were observed to be 388°C, 402°C, 414°C, and 515°C, respectively. When the deposition time increased, the thermal stability increased. As a function of the deposition, the thickness and surface morphology of the copper layer on the PI films were characterized using scanning electron microscopy (SEM).
This study was conducted to prepare protein concentrates from AL-Zahdidate’s pits by using alkaline methods where the chemical composition of the pits were (7.30, 1.04, 5.80, 8.68 and 77.19) % for each of the moisture, ash, protein, fat and carbohydrates respectively and the chemical composition of the concentrate protein was (6.62, 4.10, 26.70, 0.93, and 58.65) % respectively. The content of protein concentrate from the metallic elements (144.07, 25.11, 15.02, 0.49, 0.59, 0.27, 0.22 and 234.6) mg/ 100 g each of potassium, magnesium, calcium, iron, manganese, copper, zinc and phosphorus respectively. The results of SDS-PAGE showed five bands with weights molecular ranged between 11000-70000 Dalton. Give the biscuit which contain protei
... Show MoreAlot of medical and industrial applications used the metal nanoparticles (NPs) with increase interest to be used as cancer therapy. The current work aimed to prepare AuNPs and AgNPs through the use of plasma jet and test their antitumor mechanism of apoptosis induction. The results indicating the face-centered cubic structures and crystalline nature of AuNPs and AgNPs. Also, the image of FESEM showed that the well dispersions regarding AuNPs and AgNPs, while the NP’s spherical shape with the particle size distributions which are considered to be close that estimated from the XRD. cytotoxicity have been assessed against the Normal embryonic cell line REF and the digestive system (HC , SK-GT-4) cell lines under a variety of the seri
... Show MoreIn this research, silver nanoparticles (AgNPs) were manufactured using aqueous extract of mushroom Pleurotus ostreatus. Anticancer potential of AgNPs was investigated versus human breast cancer cell line (MCF-7). Cytotoxic response was assessed by MTT assay. AgNPs showed inhibition effect at the following concentrations 12.5, 25, 50, 100 and 200 µg/ml versus MCF-7 cell line, and all treatments had a positive result. The MCF-7 cells were inhibited up to 85.14 % at the concentration 200 μg/ml of AgNPs which reduced cells viability to 14.86%, while 12.5 μg/ml of AgNPs caused 24.23% cells inhibition with reduction of cells viability to 75.77%.
The impact of applying the K-W-L self-scheduling technique on first-year intermediate students' learning of basic volleyball skills, Ayad Ali Hussein*, Israa Fouad Salih
This research investigates the impact of varying concentrations of silver oxide on the structure and morphology of phosphate bioactive glass (PBG). PBGs are gaining popularity as a potential replacement for traditional silicate glasses in biomedical applications due to their adjustable chemical resistance and exceptional bioactivity. Upon examination of the scanning electron microscope of the composites without Ag2O, it was observed that the grains tended to merge together, and the surface particles appeared to be larger than those in composites with Ag2O at concentrations of 0.25, 0.5, and 0.75 wt%. The study found that the diffraction pattern of phosphate bioactive glass composites sintered without Ag2O showed the presence of Stro
... Show MoreDiabetic foot is a catastrophic complication of diabetes. This study included isolation and identification of three types of bacteria that cause diabetic foot ulcers, fifty-five isolates of Staphylococcus aureus, thirty-five isolates of Acinetobacter baumannii, and thirty isolates of Serratia marcescens. These isolates were obtained from diabetic foot patients at different private clinics in and around Baghdad and Medical City Hospital. The proportion of male patients was greater than females, and it was noted that the age group (51-68 years) was more ages affected by diabetic foot. These isolates showed high resistance to most of the antibiotics used, Staphylococcus aureus was resistant to
... Show MoreBacterial water pollution is a genuine general wellbeing concern since it causes various maladies. Antimicrobial nanofibers can be integrated by incorporating nanobiocides, for example, silver nanoparticles into nanofibers. Nylon 6 was dissolved in formic acid at a concentration of (25 wt. %) and tough antibacterial (AgNO3/Nylon) nanofibers were produced utilizing electrospinning system. Polymer solution was tested before accomplishing electrospinning process to acquire its surface tension, electric conductivity and viscosity, where every one of those parameters increased relatively with increasing concentration of (AgNO3) additions. SEM and EDX spectra were utilized to focus on the morphology, surface elemental mem
... Show MoreIn this research we prepared nanofibers by electrospinning
from poly (Vinyl Alcohol) / TiO2. The spectrum of the solution
(Emission) was studied at 772 nm. Several process parameter were
Investigated as concentration of PVA, the effect of distance from
nozzle tip to the grounded collector (gap distance), and final the
effect of high voltage. We find the optimum condition to prepare a
narrow nanofibers is at concentration of PVA 16gm, the fiber has
20nm diameter
Abstract:In this research we prepared nanofibers by electrospinning from poly (Vinyl Alcohol) / TiO2. The spectrum of the solution (Emission) was studied at 772 nm. Several process parameter were Investigated as concentration of PVA, the effect of distance from nozzle tip to the grounded collector (gap distance), and final the effect of high voltage. We find the optimum condition to prepare a narrow nanofibers is at concentration of PVA 16gm, the fiber has 20nm diameter.
Background: A great dental and biomedical interest had been paid to silver nanoparticles because of their antimicrobial activity. Objective: To evaluate the antimicrobial and cytotoxic activity of a newly developed Nano-silver fluoride that was synthesized from moringa oleifera leaf extract against S. mutants. Material and method: The green synthesis method was used to prepare Nano-silver fluoride from moringa oleifera leaf extract. The minimum inhibitory concentration and the minimum bactericidal concentration were evaluated using brain heart infusion plates, while the cytotoxicity was evaluated by the hemolytic activity. Results: Nano-silver fluoride had a bactericidal and bacteriostatic effect (MIC was 60 ppm a
... Show More