In this work, silver (Ag) self-metallization on a polyimide (PI) film was prepared through autocatalytic plating. PI films were prepared through the solution casting method, followed by etching with potassium hydroxide (KOH) solution, sensitization with tin chloride (SnCl2), and the use of palladium chloride (PdCl2) to activate the surface of PI. Energy-dispersive X-ray analysis (EDX) showed the highest peak in the (Ag) region and confirmed the presence of AgNPs. The diffraction peaks at 2θ = 38.2°, 44.5°, 64.6°, and 78.2° represented the 111, 200, 220, and 311 planes of Ag, respectively. The FT–IR analysis for Ag-metalized PI showed that the =C-O-C= stretching absorption bands at 1735 cm−1 had no changes in position, only a significant difference in peak size at the deposition time increase. The formation of new bands (N–H stretching absorption band and N–C stretching band) assigned at 2325 and 955 cm−1 indicated strong coordination between N atoms and silver nanoparticles. The C–C stretching and = C–H plane vibration band at 1488 and 1117 cm−1 are shifted to 1413 and 1112 cm−1, indicating the silver nanoparticles' interaction with the polymer backbone. The thermal stability of PI- and Ag-metalized PI films at various deposition times (5, 10, and 15 min) was examined using thermogravimetric analysis (TGA). For PI, T0, T5, T10, and Tmax were observed to be 388°C, 402°C, 414°C, and 515°C, respectively. When the deposition time increased, the thermal stability increased. As a function of the deposition, the thickness and surface morphology of the copper layer on the PI films were characterized using scanning electron microscopy (SEM).
The work include synthesis of nanocomposites (X / S / Ag) based on blend from Xanthan gum / sodium alginate polymers (X / S) with different loading of synthesized silver nanoparticales (0.01, 0.03 and 0.05 wt%) were added to the blend. The silver nanoparticles were prepared by reduction method and were characterized and analyzed using X-ray diffraction (XRD) and Atomic force microscope (AFM). XRD study showed the presence nanoparticle of silver with crystalline nature and face-centered cubic (FCC) structure and an average size of nanoparticles ranging from 32 to 37 nm. The surface study was performed using AFM which showed a fairly uniform shape to the nanocomposites and a spherical nature for the silver nanoparticles. The nanocomposite exh
... Show MorePowder of silver nanoparticles was prepared by Sol - Gel method successfully using silver nitrate , (AgNO3) gesture is added to sodium citrate (C6H5O7Na3) as a reducing agent and by using Magnetic Stirrer to mix the solutions and heated then using centrifuge machine to separate the silver nanoparticles from solution .It is then dried in an oven at a temperature 40oC for 24 hours. Structure characteristics was studied , the synthetic silver powder was prepared through the use of an (XRD). Results showed the composition of silver nanoparticles is a (fcc) and a constant lattice (4.086 ± 0.006 Å) by comparing it with standard tables (JCPDS) which is found perfectly matched to file with a number 04-0783, which
... Show MoreA cermet (ceramic-metal) composite have been prepared from alumina (γ-Al2O3) reinforced with aluminum (Al) for the concentrations of (0, 10, 20, 30, 40, & 50) wt. %Al. The cermet was formed by single axial pressing, sintered in vacuum atmosphere. Compaction behaviors were studied in solid state sintering at sintering temperatures (400, 450, & 550) °C, sintering times (2, 4, & 6) hrs., and forming pressures (5, 10, 15) MPa, also in liquid phase sintering at (800 °C). The cermet was characterized by x-ray diffraction (XRD) and by scanning electron microscope (SEM), also physical and mechanical properties have been studied. SEM results showed the Al flowing inside the ceramic body due to uniform distribution of Al particles a
... Show MoreIn this research, we prepared a polymer blend of polyvinylalcohol (PVA)/carrageenan/kaolinite by means of the solution cast approach. The composition of the blend was PVA in 1 gm by weight with 0.2 gm carrageenan as a plasticizer. The ratio of nanoclay varied between 1 and 5 wt%. Different properties were investigated in this study such as water vapor permeability, hardness, tear strength, color stability, thermal stability, and antibacterial activity. Water vapor permeability was decreased with increasing the ratio of nanoclay, while the values of hardness, tear strength, color stability, and thermal stability were increased. Also, the antibacterial activity examination with two types of bacteria, e.g.
... Show MoreDue to the specific characteristic of porcelain, the insertion of Beryllium oxide has been studied. The basic materials and quantities were selected carefully. In this work, porcelain containing 32 wt% feldspar, 24 wt% quartz and 44 wt% clay was synthesized and beryllium oxide (BeO) (1 wt.%, 3 wt.%, 5 wt% and 7wt%) were add. The basic and new composition porcelain powders were uniaxially compacted into standard samples dimensions and fired at various sintering temperatures, 1100°C, 1300°C, and 1450°C then held for 2 hour in a furnace.
The effects of sintering temperatures and beryllium oxide content on mechanical, electrical and structural properties were studied. The increasing of sintering temperature on the basi
... Show MoreThe aim of present study was to develop solid and liquid self-microemulsifying drug delivery system of poorly water soluble drug mebendazole using Aerosil 200 as solid carrier. Microemulsions are clear, stable, isotropic liquid mixtures of oil, water and surfactant, frequently in combination with a co-surfactant having droplet size range usually in the range of 20-250 nm. Oleic acid, tween 80 and polypropylene glycol were selected as oil, surfactant and co-surfactant respectively and for preparation of stable SMEDDS, micro emulsion region was identified by constructing pseudo ternary phase diagram containing different proportion of surfactant: co-surfactant (1:1, 2:1 and 3:1), oil and water. In brief S/ CoS mix means su
... Show MoreIn recent years, observed focus greatly on gold nanoparticles synthesis due to its unique properties and tremendous applicability. In most of these researches, the citrate reduction method has been adopted. The aim of this study was to prepare and optimize monodisperse ultrafine particles by addition of reducing agent to gold salt, as a result of seed mediated growth mechanism. In this research, gold nanoparticles suspension (G) was prepared by traditional standard Turkevich method and optimized by studying different variables such as reactants concentrations, preparation temperature and stirring rate on controlling size and uniformity of nanoparticles through preparing twenty formulas (G1-G20). Subsequently, the selected formula that pr
... Show MoreFour batches of sertraline HCl microspheres were prepared using a poly (D-L-lactide-co-glycolide) (PLGA) polymer ( Mw. 9, 27, 30 and 83 KDa) as a delivery system. The microspheres were prepared by a dispersion/solvent extraction-evaporation method and characterized for drug loading by UV, particle size by laser diffractometry and surface morphology by scanning electron microscopy (SEM). The in vitro sertraline HCl release was studied. Spherical microspheres with a mean diameter of 21 to 26 µm loaded with 24.6 – 38.2% were produced. The in vitro drug release was shown to be depend on polymer molecular weight and also on the drug loading. Differential scanning calorimetry (DSC) was employed to investigate the physical state
... Show MoreIraqi kaolin was used for the preparation and characterization of NaY zeolite for biodiesel production via esterification reaction. Oleic acid was used usually as a typical simulated feedstock of high acid number for the esterification reaction.
The chemical composition for the prepared Nay zeolite is as following: (Ca2.6Na1.K0.1)(Al6.3Si17.7)O48.16H2O, the silica to alumina ratio in the prepared catalyst was found equal to 2.6 and Na2O content was 12.26 wt. %, with relative crystallinity equal to 147.4 % obtained by the X-ray diffraction. The surface area result shows that the prepared catalyst has 330 m2