The influence and hazard of fire flame are one of the most important parameters that affecting the durability and strength of structural members. This research studied the influence of fire flame on the behavior of reinforced concrete beams affected by repeated load. Nine self- compacted reinforced concrete beams were castellated, all have the same geometric layout (0.15x0.15x1.00) m, reinforcement details and compressive strength (50 Mpa). To estimate the effect of fire flame disaster, four temperatures were adopted (200, 300, 400 and 500) oC and two method of cooling were used (graduated and sudden). In the first cooling method, graduated, the tested beams were leaved to cool in air while in the second method, sudden, water splash was used to reduce the temperature. Eight of the tested beams were divided in to four groups, each were burned to one of the adopted temperature for about half an hour and cooled by the adopted cooling methods (one by sudden cooling and the other by graduated cooling). After burning and cooling the beams were tested under the effect of repeated load (loading – unloading) for five cycle and then up to failure. As a compared with the non- burned beam, the results indicated that the ultimate load capacity of the tested beams were reduced by (16, 23, 54 and 71)% after being burned to (200, 300, 400 and 500) oC , respectively, for a case of sudden cooling and by (8, 14, 36 and 64)% , respectively, for a case of graduated cooling. It was also found that the effect of sudden cooling was greater than that in a case of graduated cooling. Regarding the failure mode, there was a different between the non-burred beam and the other ones even that all of them had the same geometric layout, compressive strength and reinforcement details. The failure mode for all burned beams was combined shear- flexure failure which was belong to the reduction in the compressive strength of the concrete due to the effect of the temperature rising , while the failure mode of the non-burned beam was flexure failure which was compatible with the preliminary design. It was also detected that the residual deflection proportion directly with the temperature, as the temperature increase to (200, 300, 400 and 500) oC the residual deflection compared with the non-burned beam increased by (32, 48, 326 and 358)% for a case of sudden cooling and by (13, 29, 303 and 332)% for a case of graduated cooling. Another effect was appear represented by the method of cooling, the results showed that the sudden cooling had more effect on the residual deflection than the graduated cooling by (15-6)% approximately. To vanish the residual deflection, numbers of cycle (loading-unloading) were required. It was found that this number increase as the temperature of burning increased and it’s also larger in a case of sudden cooling.
To enhance the structural performance of concrete-filled steel tube (CFST) columns, various strengthening techniques have been proposed, including the use of internal steel stiffeners, external wrapping with carbon fiber-reinforced polymer (CFRP) sheets, and embedded steel elements. However, the behavior of concrete-filled stainless-steel tube (CFSST) columns remains insufficiently explored. This study numerically investigates the axial performance of square CFSST columns internally strengthened with embedded I-section steel profiles under biaxial eccentric loading. Finite element (FE) simulations were conducted using ABAQUS v. 6.2, and the developed models were validated against experimental results from the literature. A comprehen
... Show MoreThis research aimed to explore the use of foamed concrete (FC), a lightweight concrete, by replacing sand with crushed plastic from washing machines to improve environmental and thermal properties. The primary components included traditional materials like cement, water, and a foaming agent, along with the innovative use of waste plastic (WP). Utilizing Minitab software, the study applied the Response Surface Method to optimize mix designs, reducing the experimental mixtures to 31, which were then tested for dry density, porosity, water absorption, shrinkage, compressive strength, splitting tensile strength, and thermal conductivity. Results indicated a significant 24% reduction in dry density when using plastic as fine and coarse aggregate
... Show MoreA novel demountable shear connector for precast steel-concrete composite bridges is presented. The connector uses high-strength steel bolts, which are fastened to the top flange of the steel beam with the aid of a special locking nut configuration that prevents bolts from slipping within their holes. Moreover, the connector promotes accelerated construction and overcomes the typical construction tolerance issues of precast structures. Most importantly, the connector allows bridge disassembly. Therefore, it can address different bridge deterioration scenarios with minimum disturbance to traffic flow including the following: (1) precast deck panels can be rapidly uplifted and replaced; (2) connectors can be rapidly removed and replaced; and (
... Show MoreBackground: In Iraqi communities, the workers considered the largest population groups, so increasing their dental education by increasing the care for their dental health knowledge and behavior is very important, the present study was aimed to evaluate the gingival health and oral hygiene in relation to knowledge and behavior among a group of a workers selected randomly from Al Fedaa company in Baghdad city. Materials and methods: A sample of 110 workers (65 men and 45 women) included in this study, a questionnaire used to evaluate their oral health knowledge and behavior. The gingival health condition of the workers was examined by using Loe and Silness index (1963), Silness and Loe index (1964) was used to asses plaque quantity, and Ramf
... Show MoreThe present study was conducted to determine histopathological changes caused by chronic effect of Nitrofurantoin(NFT) in The albino mice Testes. The Study included 40 mice were divided on the five groups: the first group taken distilled water and become control group . the remaining group which are exposure with NFT drug in concentration (100-150-200-250) mg / kg, respectively, Doses were given orally for a period (month and two months). The results of histopathological changes included occurrence of congestion in the blood vessel and degeneration of spermatogonia and aggregation of spermatids in the lumen of semineferous tubules and inhibition of spermatogensis process and decrease of sperm inside the lumen
... Show More