Q-switch Nd: YAG laser of wavelengths 235nm and 1,460nm with energy in the range 0.2 J to 1J and 1Hz repetition rate was employed to synthesis Ag/Au (core/shell) nanoparticles (NPs) using pulse laser ablation in water. In this synthesis, initially the silver nano-colloid prepared via ablation target, this ablation related to Au target at various energies to creat Ag/Au NPs. Surface Plasmon Resonance (SPR), surface morphology and average particle size identified employing: UV-visible spectrophotometer, scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The absorbance spectra of Ag NPs and Ag/Au NPs showed sharp and single peaks around 400nm and 410nm, respectively. The average diameter achieved for Ag/Au NPs were as 30nm and 25nm corresponding to 532nm and 1064nm, respectively. The TEM images showed that Ag/Au NPs possess a spherical shape, while the samples average size were in range from 20 to 30nm. There was an obvious increase in size during the use of 532nm laser. As for the effects of toxicity, results on human blood components showed that these nanoparticles have no effect on RBCs, WBCs and HB Therefore; these particles considered promising in the biological and medical applications.
Colloidal dispersions of mono Au, Ag , Cu and bimetallic Ag/Au and Cu/Au
core/shell nanoparticles are synthesized by pulsed laser ablation of metals targets
immersed in 5 ml distilled water (DW). Surface Plasmon resonance (SPR) and
particle sizes are characterized by UV-VIS and HRTEM, the X-ray diffraction
shows the structure of core/shell. The Surface Plasmon resonance of the produced
nanoparticles solutions for silver nanoparticles about 402 nm and copper
nanoparticles about 636 nm. While for the core-shell observed two peaks of SPR,
Ag/Au core/shell at (406-516) nm, and Cu/Au core/shell observed one peak at
565nm, because the region of gold and copper close together. The shape and
particle size have been con
Ag nanoparticles were prepared using Nd:YAG laser from Ag matel in distilled water using different energies laser (100 and 600) mJ using 200 pulses, and study the effect of the preparation conditions on the structural characteristics of and then study the effect of nanoparticles on the rate of killing the two types of bacteria particles (Staph and E.coli). The goal is to prepare the nanoparticle effectively used to kill bacteria.
Metal nanoparticles (NPs) of silver (Ag), copper (Cu), zinc oxide (ZnO), cadmium oxide (CdO) and tin (Sn) were synthesized by laser ablation of a solid target in de-ionized water (DI). X-ray diffraction patterns showed the formation of AgO, Ag, Cu, ZnO, CdO, and Sn NPs. Absorbance spectrum of the produced nanoparticles was measured by UV-Vis spectrophotometer which showed that Ag and CdO NPs shifted to the short wavelength (blue shift), indicating the formation of NPs with smaller sizes, whereas CuO showed the formation two peaks. ZnO and Sn NPs shifted to the long wavelength (red shift) which indicates the formation NPs with larger size. Zeta potential results proved that ZnO nanoparticles were more stable (-26.53mV) than the othe
... Show MoreMetal nanoparticles can serve as an efficient nano-heat source with confinement photothermal effects. Thermo-plasmonic technology allows researchers to control the temperature at a nanoscale due to the possibility of precise light propagation. The response of opto-thermal generation of single gold-silica core-shell nanoparticle immersed in water and Poly-vinylpyrrolidone surrounding media is theoretically investigated. Two lasers (CW and fs pulses) at the plasmonic resonance (532 nm) are utilized. For this purpose, finite element method is used via COMSOL multiphysics to find a numerical computation of absorption cross section for the proposed core –shell NP in different media. Thermo-plasmonic response for both lasers is studied. The
... Show MoreNanoparticle has pulled in expanding consideration with the developing enthusiasm for nanotechnology which hold potential as essential segments for development applications. In the present work, a copper nanoparticle is manufactured as a suspension in distilled water by beating a bulk copper target with laser source (532 nm wavelength, 10 ns pulse duration and 10 Hz repletion rate) via method. UV- visible absorption spectra and AFM analysis has been done to observe the effect of repetition rate for the pulsation of laser. Copper nanoparticles (Cu-NPs) were successfully synthesized with green color. The Cu- NPs have very high purity because the preparation was managed in aqueous media to eliminate ambient contaminations. Absorption
... Show MoreZinc Oxide nanoparticles were prepared using pulsed laser ablation process from a pure zinc metal placed inside a liquid environment. The latter is composed of acetyltrimethylammonium bromide (CTAB) of 10−3 molarity and distilled water. A Ti:Sapphire laser of 800 nm wavelength, 1 kHz pulse repetition rate, 130 fs pulse duration is used at three values of pulse energies of 0.05 mJ, 1.11 mJ and 1.15 mJ. The evaluation of the optical properties for the obtained suspension was applied through ultraviolet–visible absorption spectroscopy test (UV/VIS). The result showed peak wavelengths at 210 nm, 211 nm and 213 nm for the three used pulse energies 0.05 mJ, 1.11 mJ and 1.15 mJ respectively. This indicates a blue shift,
... Show MoreThe natural polyphenolic compound that cinnamon contains is well known for its various biological activities, a broad variety of pharmacological and therapeutic properties. Diversified biomedical and pharmacological applications benefit from organic nanoparticles with controlled properties. Bioactive and non-toxic, cinnamon nanoparticles (CNPs) can be effective antibacterial agents. Driven by this idea, we prepared spherical CNPs using liquid (PLAL) pulse laser ablation technique and defined those NPs. Using Q-switched Nd : YAG With a wavelength of 1064 nm pulse laser of constant energy 500 mj , And different laser pulses ( 250 , 500 , 750 , 1000 ) pulse /sec a pure cinnamon target submerged in
... Show MoreIn this study, graphene oxide (GO) and reduced graphene oxide were synthesized by pulsed Nd:YAG laser with a fundamental wavelength (1064 nm) focused on the pure graphite target which was immersed in distilled water. Different pulse energies were applied in two cases; with and without magnetic field. The synthesized GO and rGO nanoparticles were characterized by UV-visible spectroscopy, X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy and atomic force microscopy (AFM) with and without magnetic field. The data show the presence of a magnetic field which illustrated increasing oxygen functional groups of GO. This caused a change in the morphology of the surface of GO, increasing crystallite size from 12.19 nm to 71.2
... Show More