In this research, Argon gas was used to generate atmospheric plasma in the manufacture of platinum nanomaterials, to study the resultant plasma spectrum and to calculate the cellular toxicity of those manufactured nanomaterials. This research is keen on the generation of nonthermal atmospheric pressure plasma using aqueous platinum salts (H2PtCl6 6H2O) with different concentrations and exposure of cold plasma with a different time period used to produce platinum nanoparticles, to ensure typical preparation of nanoparticles. Visible UV and X-rays were performed for this purpose, and the diameter of the system probe was (1[Formula: see text]mm) with the Argon gas flow of 2.5[Formula: see text]min/L to prepare the platinum nanoparticles, and spectroscopic study of plasma parameter including, electron temperature, electron density, Debye length and plasma frequency, were computed using spectral analysis techniques. The effect of nanoparticles on natural lymphocytes was studied to calculate cytotoxicity and the greatest proportion was at the concentration of 100% nanoparticle platinum is 37.4%. The study results revealed that cold in the atmosphere is a promising technology when used in the production of nanoparticle materials which can be used for many industrial and medical applications.
In the current work, Punica granatum L. peel, Artemisia herba-alba Asso., Matricaria chamomilla L., and Camellia sinensis extracts were used to prepare manganese dioxide (MnO2) nanoparticles utilizing a green method. Energy-dispersive X-ray (EDX) analysis, Fourier Transform Infrared Spectroscopy (FTIR) analysis, and Filed emission-scanning electron microscopy (FE-SEM) analysis were used to evaluate the produced MnO2 NPs. FE-SEM pictures demonstrated how agglomerated nanoparticles formed. According to FE-SEM calculations, the particle size ranged from 18.7-91.5 nm. FTIR spectra show that pure Mn-O is formed, while EDX results show that Mn and O are present. The ability to suppress biofilm growth in the produced MnO
The design, synthesis, and characterization of a star shaped 2,4,6-tris-(4`-carboxyphenoxy)-1,3,5-triazine liquid crystalline with columnar discotic mesophase properties establish H-bond interactions with 3,5-dialkoxypyidine were reported. The structures of the synthesized compounds were actually determined by elementary analysis, and FT-IR, ¹HNMR, ¹³CNMR, and mass spectroscopy. The mesomorphic properties of these mesogens were examined using differential scanning calorimetry (DSC) and optical polarizing microscopy (OPM). The synthesized molecules exhibited enantiotropic hexagonal columnar liquid crystal, which depends for the H- bond complex in a 1:3 ratio.
The size and the concentration of the gold nanoparticles (GNPs)
synthesized in double distilled deionized water (DDDW) have been
found to be affected by the laser energy and the number of pulses.
The absorption spectra of the nanoparticles DDDW, and the
surface plasmon resonance (SPR) peaks were measured, and found to
be located between (509 and 524)nm using the UV- Vis
spectrophotometer. SPR calculations, images of transmission
electron microscope, and dynamic light scattering (DLS) method
were used to determine the size of GNPs, which found to be ranged
between (3.5 and 27) nm. The concentrations of GNPs in colloidal
solutions found to be ranged between (37 and 142) ppm, and
measured by atomic absorptio
A new ligand N-(methylcarbamothioyl) acetamide (AMP) was synthesized by reaction of acetyl chloride with adenine. The ligand was characterized by FT-IR, NMR spectra and the elemental analysis. The transition metal complexes of this ligand where synthesize and characterized by UV-Visible spectra, FT-IR, magnetic suscepility, conductively measurement. The general formula [M(AMP)2Cl2], where M+2 = (Mn, Co, Ni, Cu, Zn, Cd, Hg).
In this study, Zinc oxide nanostructures were synthesized via a hydrothermal method by using zinc nitrate hexahydrate and sodium hydroxide as a precursor. Three different annealing temperatures were used to study their effect on ZnO NSs properties. The synthesized nanostructure was characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), Atomic force microscope (AFM), and Fourier Transform Infrared Spectroscopy (FTIR). Their optical properties were studied by using UV -visible spectroscopy. The XRD analysis confirms that all ZnO nanostructures have the hexagonal wurtzite structure with average crystallite size within the range of (30.59 - 34
... Show MoreGreen synthesis methods have emerged as favorable techniques for the synthesis of nano-oxides due to their simplicity, cost-effectiveness, eco-friendliness, and non-toxicity. In this study, Nickel oxide nanoparticles (NiO-NPs) were synthesized using the aqueous extract of Laurus nobilis leaves as a natural capping agent. The synthesized NiO-NPs were employed as an adsorbent for the removal of Biebrich Scarlet (BS) dye from aqueous solution using adsorption technique. Comprehensive characterization of NiO-NPs was performed using various techniques such as atomic force microscopy (AFM), Fourier transform infrared (FTIR), X-ray diffraction (XRD), Brunauer-Emmett and Teller (BET) analysis, and scanning electron microscopy (SEM). Additionally, o
... Show MoreBackground In recent years, there has been a notable increase in the level of attention devoted to exploring capabilities of nanoparticles, specifically gold nanoparticles AuNPs, within context of modern times. AuNPs possess distinct biophysical properties, as a novel avenue as an antibacterial agent targeting Streptococcus Mutans and Candida Albicans. The aim of this study to create a nano-platform that has the potential to be environmentally sustainable, in addition to exhibiting exceptional antimicrobial properties against Streptococcus Mutans as well as Candida Albicans. Methods this study involved utilization of
A sensitive and selective method have been developed for the determination of palladium (II)and platinum (II) . A new reagent and two complexes have been prepared in ethanolic solutions .The method is based on the chelation of metal ions with 4-(4?- pyrazolon azo) resorcinol (APAR) to form intense color soluble products, that are stable and have a maximum absorption at 595 nm and at 463 nm and ?max of 1.11×10 4 and.1.35 ×104 Lmole-1cm-1 for Pd(II) Pt(II) respectively. A linear correlation of (1.4 – 0.2) and (3.2 -0.4 ) ppm for pd(II) pt(II) respectively .The stability constants , relative errors , a relative standard deviations for Pd(II) and Pt(II) were 0.40×105 , 0.4×104 L mol-1 ,0.34 - 0.21% and 2.4 – 0.91% respectively.
... Show More