Application of zirconia surface coating to improve fracture resistance and stress distribution of zirconia ceramic restorations
...Show More Authors

Zirconia ceramic restoration (ZCR) has a higher fracture incidence rate than metal ceramic restoration. Different surface treatments were used to improve fracture performance of ZCR such as grit blasting (GB) by aluminium oxide powder. This type of surface treatment generate residual stresses on veneering ceramic causing crack initiation and ending with a fracture. In order to overcome the stress generated by GB, zirconia surface coating is used as a surface treatment to improve fracture resistance and to accommodate stresses along the ZCR layers. Fifty zirconia ceramic crowns were fabricated and divided according to the type of surface treatment into three groups; the first group is (ZG), involving 20 cores were coated with a mixture of partially-sintered zirconia powder (PZP) and glaze ceramic powder; the second group is (ZL), including of 20 cores were coated with PZP and liner ceramic paste. The third group is grit blasting (GB), preparing of 10 fully sintered cores at 1350 °C which then abraded by 50 µm aluminium oxide powder. The groups ZG and ZL were further subdivided into ZG26, ZG47, ZL26 and ZL47 based on two PZP sizes (47 and 26 µm). Each treated core was veneered with the veneering ceramic layer. Fracture resistance (FR) was measured by the universal testing machine. Finite element analysis (FEA) was used to simulate the stress distributions on the coated and non-coated zirconia crown models. The ZG47 group had higher FR (647.92 ± 97.33 N) and a significant difference (P < 0.00) compared to GB and other coated groups. The FEA exhibited lower and evenly distributed stresses of the zirconia glaze model than the zirconia liner and the non-coated models. The ZG47 coating considered as an alternative method to GB treatment which increases the FR which significantly improved the clinical performance of the ZCR.

Scopus
Publication Date
Sat Oct 27 2018
Journal Name
Surface And Coatings Technology
Effect of surface treatment of zirconia-ceramic dental restorations
...Show More Authors

The zirconia ceramic restoration (ZCR) is used as substitutes for the metal-ceramic restoration. Clinical studies demonstrating of ZCRs showed a high fracture incidence of veneering layer than metal-ceramic restorations. This attributed to the low bond strength of zirconia to veneering ceramic as a result of lacking of glass content in its matrix. Surface treatment was proposed to improve the bonding strength between zirconia and veneering ceramic. Several studies revealed that some treatment such as airborne particle abrasion (APA) is responsible for generating chipping of veneering ceramic. The study aimed to develop a new zirconia coatings to increase bonding strength between zirconia substrate and veneering porcelain. Three groups of 15

... Show More
Preview PDF
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of zirconia surface treatments on the shear bond strength of veneering ceramic
...Show More Authors

Background: The aim of the study was to investigate the effect of surface treatments of zirconia (grinding and sandblast with 50μm, 100 μm) on shear bond strength between zirconia core and veneering ceramic. Material and methods: Twenty-eight presintered Y-TZP ceramic specimens (IPS e.max ZirCAD, Ivoclar vivadent) were fabricated and sintered according to manufacturer’s instructions. The core specimens were divided randomly in to 4 groups, group 1: no surface treatment, group2: zirconia specimens were ground with silicon carbide paper up to1200 grit under water cooling, group3: zirconia specimens were ground and sandblast with 100 μm alumina, group 4: zirconia specimens were ground and sandblast with 50 μm alumina. Surfa

... Show More
View Publication Preview PDF
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Evaluation of shear bond strength of zirconia to tooth structure after different zirconia surface treatment techniques
...Show More Authors

Background: This study aimed to evaluate the effect of zirconia different surface treatments (primer, sandblast with 50μmAl2O3, Er,Cr:YSGG laser) on shear bond strength between zirconia surface and resin cement. Material and methods: Sixty presintered Y-TZP zirconia cylinder specimens (IPS e.max ZirCAD, Ivoclar vivadent) will be fabricated and sintered in high temperature furnace of (1500 C for 8 hours) according to manufacturer’s instructions to the selected size and shape of (5mm. in diameter and 6mm in height). All specimens were ground flat using 600.800.1000.1200, aluminum oxide abrasive paper to obtain a standardized surface roughness. Surface roughness values were then recorded in µm using surface roughness tester (profi

... Show More
View Publication Preview PDF
Publication Date
Mon Jan 01 2018
Journal Name
Surface And Coatings Technology
Effect of new zirconia surface coatings on the surface properties and bonding strength of veneering zirconia substrate
...Show More Authors

View Publication
Scopus (10)
Crossref (10)
Scopus Clarivate Crossref
Publication Date
Thu Jun 15 2017
Journal Name
Journal Of Baghdad College Of Dentistry
A Comparison of Vertical Marginal Fit of different Brands of Translucent Zirconia Crown Restorations
...Show More Authors

Background: As the development of zirconia crown using CAD/CAM technology, the usage of full zirconia crown is gradually increased. The aim of this in-vitro study was to evaluate and contrast the vertical marginal fit of single all-ceramic translucent zirconia crowns constructed from different brands translucent zirconia blanks. Materials and Methods: An acrylic resin model of a left maxillary premolar was prepared all around the tooth with (1 mm) depth and 3D scanning to get fifteen STL files, then distributed into three groups (Imes-icor, Whitepeaks and Dental direct), 3D scanning and milling machine by Imes-icor CAD/CAM devise. Marginal gaps along vertical planes were measured at four indentations at the (mid mesial, mid distal, mid bucc

... Show More
View Publication Preview PDF
Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
An evaluation of the influence of different finishing lines on the fracture strength of full contour zirconia CAD/CAM and heat press all-ceramic crowns
...Show More Authors

ABSTRACT Background: One of the major problems of all ceramic restorations is their probable fracture against the occlusal forces. The objective of this in vitro study was to evaluate the effect of two gingival finishing lines (90°shoulder and deep chamfer) on the fracture resistance of full contour CAD/CAM and heat press all-ceramic crowns. Materials and Methods: Thirty two maxillary first premolars were prepared to receive full contour CAD/CAM (zolid) and heat press (Cergo Kiss) ceramic crowns using a special paralleling device (Parallel-A-Prep). The teeth were divided into four groups according to the type of finishing line prepared. Each crown was cemented to its corresponding tooth using self-etch, self-adhesive dual cure resin ceme

... Show More
View Publication Preview PDF
Publication Date
Fri Jan 07 2022
Journal Name
Iraqi Journal Of Laser
Influence of Fractional CO2 Laser Irradiation on Temperature Elevation and Bonding Strength of Resin Cement to the Zirconia Ceramic
...Show More Authors

Abstract: Objectives: To investigate the effect of temperature elevation on the bonding strength of resin cement to the zirconia ceramic using fractional CO2 laser. Background: Fractional CO2 laser is an effective surface treatment of zirconia ceramic, as it increases the bonding strength of zirconia to resin cement. Methods: Thirty sintered zirconia discs (10 mm diameter, 2 mm thickness) were prepared and divided to three groups (N=10) and five diffident pulse durations were used in each group (0.1, 0.5, 1, 5 and 10 ms). Group A was treated with 10 W power setting, group B with 20 W and group C with 30 W. During laser irradiation, temperature elevation measurement was recorded for each specimen. Luting cement was bonded to the treated z

... Show More
View Publication Preview PDF
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of different polishing systems on the surface roughness of full-contour zirconia
...Show More Authors

Background: Adjustment of any premature occlusal contact of any zirconia restoration requires its polishing or glazing in order to restore the smoothness of the restoration. The objective of this in vitro study was to evaluate the effects of different polishing systems and glazing on the surface roughness of full-contour zirconia. Material and methods: Forty disks (diameter: 8 mm, thickness: 6.4 mm) were prepared from pre-sintered full-contoured zirconia block; they were colored and sintered in a high-temperature furnace at 1500ËšC for 8 hours. The specimens were then leveled and finished using grinding and polishing machine and adjusted using diamond disk. The specimens were then randomly divided into four groups (n=10), group I involves

... Show More
View Publication Preview PDF
Publication Date
Fri Apr 01 2022
Journal Name
Baghdad Science Journal
Fractographic Analysis of Tensile Failures of Zirconia Epoxy Nanocomposites
...Show More Authors

This work characterizes the fractographic features of the neat epoxy and ZrO2 epoxy nanocomposites. All samples were subjected to a tensile test to determine the tensile strength and tensile modulus. SEM images were used to study the morphology of the fractured surface. The fractographic of the fracture surfaces were studied by microstructure analysis program (j-images) to specify the effect of ZrO2 nanoparticles on tensile performance and failure mechanism for ZrO2 epoxy nanocomposites. The tensile test results show that the addition of ZrO2 nanoparticles (2, 4, 6, 8, and 10 vol.%) to the epoxy matrix leads to increase the tensile strength about 40% for optimal content of ZrO2 nanop

... Show More
View Publication Preview PDF
Scopus Clarivate Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Fracture resistance of endodontically treated premolars with extensive MOD cavities restored with different composite restorations (An In vitro study)
...Show More Authors

Background: This in vitro study evaluated the fracture resistance of weakened endodontically treated premolars with class II MOD cavities restored with different composite restorations (Low-shrinkage Filtek P90, nanohybrid Filtek Z250 XT and SDR bulk fill). The type and mode of fracture were also assessed for all the experimental groups. Materials and Method: Fifty human adult maxillary premolar teeth were selected for this study. Standardized extensive class II MOD cavities with endodontic treatment were prepared for all teeth, except those that were saved as intact control. The teeth were divided into five groups of ten teeth each (n=10): (Group 1) intact control group, (Group 2) unrestored teeth with endodontic treatment, (Group 3) resto