Background: The base of the denture is largely responsible for providing the prosthesis with retention, stability, and support by being closely adapted to the oral mucosa. However; the process of bone resorption is irreversible and may lead to an inadequate fit of the prosthesis; this can be overcome by relining. Materials and methods: Acrylic based soft denture liner is prepared by preparing polymer from purified methylmethacrylate monomer with (10-2) initiator and (30%) dibutylphthalate plasticizer concentrations. Biological properties were evaluated in comparison with the control material through subcutaneous specimens' implantation in the New Zealand rabbits. Excisional biopsies were taken after (1, 3, days 1, 2, 3, 4 weeks) period. Mic
... Show MoreLow- and medium-carbon structural steel components face random vibration and dynamic loads (like earthquakes) in many applications. Thus a modification to improve their mechanical properties, essentially damping properties, is required. The present study focuses on improving and developing these properties, significantly dampening properties, without losing the other mechanical properties. The specimens used in the present study are structural steel ribbed bar ISO 6935 subjected to heating temperatures of (850, 950, and 1050) ˚C, and cooling schemes of annealing, normalizing, sand, and quenching was selected. The damping properties of the specimens were measured experimentally with the area under the curve for the loadi
... Show MoreThis study aims to evaluate and compare the cytotoxicity and biocompatibility of a modified heat-cured acrylic denture base material containing 15% phosphoric acid 2-hydroxyethyl methacrylate ester (PA2HEME) with those of nonmodified PMMA. Discs with a diameter of 12 mm and a thickness of 2 mm were prepared using a heat-cured PMMA denture base material and divided into control and experimental groups. The experimental group was modified with 15% phosphoric acid 2-hydroxyethyl methacrylate ester (PA2HEME). The modified and nonmodified materials were tested via FTIR, and the effect of modification on surface roughness was evaluated with AFM. An in vitro test was conducted to examine the cytotoxicity and biocompatibility of heat-cured acry
... Show MoreCopper tin sulfide (Cu2SnS3) thin films have been grown on glass
substrate with different thicknesses (500, 750 and 1000) nm by flash
thermal evaporation method after prepare its alloy from their
elements with high purity. The as-deposited films were annealed at
473 K for 1h. Compositional analysis was done using Energy
dispersive spectroscopy (EDS). The microstructure of CTS powder
examined by SEM and found that the large crystal grains are shown
clearly in images. XRD investigation revealed that the alloy was
polycrystalline nature and has cubic structure with preferred
orientation along (111) plane, while as deposited films of different
thickness have amorphous structure and converted to polycrystalline
The relationships between the related parties constitute a normal feature of trading and business processes. Entities may perform parts of their activities through subsidiary entities, joint ventures and associate entities. In these cases, the entity has the ability to influence the financial and operating policies of the investee through control, joint control or significant influence, So could affect established knowledge of transactions and balances outstanding, including commitments, and relationships with related to the evaluation of its operations by users of financial statements, including the risks and opportunities facing the entity assess the parties. So research has gained importance of the importance of the availability
... Show MoreMechanical degradation hampers the practical usage of polymers for turbulent drag reduction
application. Mechanical degradation refers to the chemical process in which the activation energy of
polymer chain scission is exceeded by mechanical action on the polymer chain, and bond rupture
occurs. When a water-soluble polymer and surfactant are mixed in water solution, the specific structures
(aggregates) are formed, in which polymer film is formed around micelle. In this work, Xanthan gum (XG) –
Sodium lauryl ether sulfate (SELS) complex formation and its effect on percentage viscosity reduction
(%VR) was studied. It was found that SELS surfactant reduced the mechanical degradation of XG much
more efficiently than th