In this research, Mn-doped TiO2 thin films were grown on glass, Si and OIT/glass substrates by R.F magnetron sputtering technique with thicknesses (250 nm) using TiO2:Mn target under Ar gas pressure and power of 100 Watt. Through the results of X-ray diffraction, the prepared thin films are of the polycrystallization type after the process of annealing at 600°C for two hour The average crystalline size were 145.32, 280.97 and 261.23 nm for (TiO2:Mn) thin film on glass, Si and OIT/glass substrates respectively, while the measured surface roughness is between 0.981nm and 1.14 nm. The fabricated (TiO2:Mn) thin film on glass sensors have high sensitivity for hydrogen( H2 reducing gas) compared to the sensitivity for hydrogen gas on Si and OIT/glass substrates at room temperature as well faster in response and recovery times. It was found that the sensing properties strongly depended on the structure characteristics, especially the surface area and morphology.
Recently, numerous the generalizations of Hurwitz-Lerch zeta functions are investigated and introduced. In this paper, by using the extended generalized Hurwitz-Lerch zeta function, a new Salagean’s differential operator is studied. Based on this new operator, a new geometric class and yielded coefficient bounds, growth and distortion result, radii of convexity, star-likeness, close-to-convexity, as well as extreme points are discussed.
Background: With the increasing demand on esthetic orthodontic appliances, discoloration of clear elastomeric chains and modules remains an issue which concerns both orthodontics and patients. This in vitro study was conducted to evaluate the effect of exposing stretched clear elastomeric chains from six different companies (Ortho Technology, Ormco, Ortho Organizer, American Orthodontics, Opal and G&H companies) to three types of dietary media (tea, coffee and turmeric). Materials and methods: A total of 960 lengths of six modules were cut from short type elastomeric chain; 160 pieces from each brand. The specimens were stretched 50%, placed on plastic boards, and incubated in water at 37°C for 1 day, 7 days, 14 days and 28 days. Once a
... Show MoreLight isotopes, especially closed shell nuclei, have significance in thermonuclear reactions of the Carbon-Nitrogen-Oxygen (CNO) cycle in stars. In this research, 12C(p, γ) 13N and 14N(p, γ) 15O reactions have been calculated by means of Matlab codes to find the reaction rate across a temperature range of 0.006 to 10 GK using non-resonant parts, as well as the astrophysical S- factor S(E) at low energies. It was concluded that the high binding energy of 12C and 14N nuclei make the reaction less probable thus enabling other competitive processes to develop, which enhances the probability of other competitive proton reactions in the CNO cycle.
Spent hydrodesulfurization (Co-Mo/γ-Al2O3) catalyst generally contains valuable metals like molybdenum (Mo), cobalt (Co), aluminium (Al) on a supporting material, such as γ-Al2O3. In the present study, a two stages alkali/acid leaching process was conducted to study leaching of cobalt, molybdenum and aluminium from Co-Mo/γ-Al2O3 catalyst. The acid leaching of spent catalyst, previously treated by alkali solution to remove molybdenum, yielded a solution rich in cobalt and aluminium.
In this study involves removing of Brilliant Dyes, were which (Brilliant Green {BG} and Brilliant Cresyl Blue {BCB}) by using Iraqi Siliceous Rocks Powder (SRP). Adsorption isotherms were studied and the factors which prefer it, like temperature and salt effect, Adsorption isotherms of dyes, Brilliant Cresyl Blue {BCB} was found to be comparable to Langmuir equation according to Giles classification, isotherms dye Brilliant Green {BG} was found to be comparable to Freundlich equation more than dye Brilliant Blue {BCB} according to Giles classification. The adsorption process on this surface (SRP) studied at different temperatures, the results showed that the adsorption of dyes (BCB, BG) on the surface increased with increased temperature (E
... Show MoreA study of irrigation water was conducted Baghdad city to find out extent of its pollution by some heavy metals (Pb, Cd, Ni, Co, CU, Cr, Zn and Fe). Water samples were collected randomly from different sources (river, well and stream). Results showed that the concentration of studied heavy metals were as follows: Lead between 0.43-11.75 mg L-1, Cadmium between 0.01-0.95 mg L-1, Nickel between 0.008-0.46 mg L-1, Cobalt between Nil - 0.185 mg L-1, Copper is between 0.326 - 1.58 mg L-1, Chromium is between Nil-0.068 mg L-1, Zinc 0.398-1.182 mg L-1, as for Iro