This work focuses on the preparation of pure nanocrystalline SnO2 and SnO2:Cu thin films on cleaned glass substrates utilizing a sol-gel spin coating and chemical bath deposition (CBD) procedures. The primary aim of this study is to investigate the possible use of these thin films in the context of gas sensor applications. The films underwent annealing in an air environment at a temperature of 500 ◦C for duration of 60 minutes. The thickness of the film that was deposited may be estimated to be around 300 nm. The investigation included an examination of the structural, optical, electrical, and sensing characteristics, which were explored across various preparation circumstances, specifically focusing on varied concentrations of Cu-doping (2, 4, and 6 wt.%). The deposited films were analyzed by several techniques, including X-ray diffraction (XRD), scanning electron microscopy (SEM), atomic force microscopy (AFM), and optical absorption spectroscopy. The films generated by the spin coating method had a tetragonal rutile structure, while the films created via the chemical bath deposition (CBD) technique displayed both tetragonal rutile and orthorhombic structures. The spin coating technique was used to make films of several weight percentages (0, 2, 4, and 6 wt.%). The resulting crystallite sizes were examined and found to be 23 nm, 18 nm, 14 nm, and 10.5 nm, respectively. Similarly, films made using the chemical bath deposition (CBD) method exhibited crystallite sizes of 22, 13.9, 9.3, and 8.15 nm, respectively. The obtained findings from atomic force microscopy (AFM) and scanning electron microscopy (SEM) analyses indicate a consistent trend whereby, as the concentration of Cu-doped material rises, there is a decrease in the average grain size. The transmittance and absorbance spectra were examined within the wavelength range of 300 to 1000 nm. The films generated by both approaches exhibit a significant level of light transmission throughout the visible spectrum. The bandgap energy of spin coating and CBD films decreases with increasing Cu-doped concentrations; the values were (3.88, 3.8, 3.68, and 3.63) eV and (3.8, 3.78, 3.66, and 3.55) eV, respectively. The electrical characteristics of the films include direct current (DC) electrical conductivity, which indicates the presence of two activation energies, Ea1 and Ea2. These activation energies exhibit an upward trend when the concentration of Cu doping is increased. The films were examined for their ability to detect carbon monoxide (CO) gas at a concentration of about 50 ppm at normal room temperature conditions. The sensitivity of the films to carbon monoxide (CO) gas was assessed at various time intervals and temperatures. The results indicated that the film generated using spin coating exhibited a notably high sensitivity at a temperature of 200 °C, while the film prepared using the chemical bath deposition (CBD) approach had heightened sensitivity at a temperature of 150 °C. Keywords: Spin coating, SnO2 thin films, CBD, AFM, XRD, gas sensor.
KE Sharquie, AA Al-Nuaimy, WJ Kadhum, Saudi medical journal, 2006 - Cited by 3
Nanocrystalline micro-mesoporous ZSM/MCM-41 composite was synthesized using alkaline treatment method and two step of crystallization in poly tetraflouroethylene (PTFE) lined autoclave. The synthesized zeolites was characterized by X-Ray diffraction (XRD), Scanning electron microscopy (SEM), Transmission electron microscopy (TEM), Atomic force microscopy (AFM), Fourier transport infrared (FTIR), and N2 adsorption-desorption (BET). It was approved that the best results for alkaline leaching can be got with 1.5M NaOH solution. High surface (BET) area of 630 m2/g with pore volume of 0.55 cm3/g has been got. AFM reports showed a nano-level size for average particle size of 50nm.
In this research the effect of grain size and effect of La2O3 doping on densification rate for the initial and intermediate stages of sintering were studied .The experimental results for α – cristobilite powder are modeled using ( L2-Regression ) technique in studying the effect of grain size and La2O3 doping using three particles size (6.12, 8.92, 13.6 ) µm, with undoped initial powder and with La2O3 doping . The mathematical simulation showes that the densification rates increase as the initial particles sizes decrease and vice versa. This shows that the densification depends directly on the initial compact density which reflects the contacts area between the particles . How
... Show MoreThin films of pure polycarbonate (PC) with anthracene doping PC films for different doping ratios (10, 20, 30, 40, 50 and 60 ml) were prepared by using a casting method. The influence of anthracene doping ratio on photo-fries rearrangement of polycarbonate was systematic investigated. Furthermore, pure PC and anthracene doping PC films were irradiated via UV light at a wavelength (254 nm) for different periods (5, 240, 288, and 360 hrs). The photo-fries rearrangement occurring in pure PC and anthracene doping PC films were monitored using UV and FTIR spectroscopies. The photo-fries rearrangement leads to scission the carbonate linkage and formation phenylsalicylate and dihydroxybenzophenes. The result of the UV spectrum confirms disappea
... Show MoreZinc oxide films (ZnO) are prepared by an electrolysis technique and without vacuum and then annealed atvarious temperatures (300,400,500)OC for an hour. The structural analysis performed by X-Ray diffraction (XRD) shows,dominant orientation of this films is plane (101), has a hexagonal structure and polycrystalline pattern and it was is found that the crystal size increases(24,29) nm at annealing temperatures (300, 400)° C, but the crystal size decreases to (20 nm) at annealing temperature (500 ° C). As the results of a surface nature study of these films showed by examining the atomic force microscope (AFM), the grain size increases from (60.79 to 88.11) nm, and the surface roughnes
... Show More