The Moisture damage is considered as one of the main challenge for the experts in the field of asphalt pavement design. The aims of the present study is to modify moisture resistance of the asphalt concrete by utilizing ceramic fibers as a type of reinforcement incorporated with hydrated lime. For this purpose, a penetration grade of the asphalt cement (40-50) was utilized as a binder with an aggregate of the maximum nominal size of 12.5mm and mineral filler limestone dust. A series of specimens has been fabricated by utilizing 0.50, 1.0, 1.5, and 2.0 percentages of ceramic fibers. For each of these contents, another subsequent group of specimens with hydrated lime with 0.0, 1.0, 1.5, and 2.0 percentages were moulded. For the addition of ceramic fiber and hydrated lime to the mixtures the dry method for ceramic fiber was adopted while for the hydrated lime, the saturated surface dry method was adopted. The results of this study have shown that the addition of 1% ceramic fiber with 1.5% hydrated lime recorded the highest levels of growth. Furthermore, the outputs of the tests used in this study have shown that the use of ceramic fibers resulted in a growth in the value of tensile strength ratio (TSR) and in the index of retained strength (IRS) compared with the control mixture. Maximum values for TSR were achieved at 1% ceramic fibers with 1.5 % hydrated lime.
Chemical resistance ceramic tiles and mortar to alkali solution are prepared and characterized in this study due to the lack of this kind of publications in ceramic literature. Most of the utilized materials are readily available raw materials and the other materials are available commercially. Physical and mechanical properties are measured and indicate that the prepared ceramic tile and mortars are competitive to traditional building materials. Chemical resistance test against alkali solution is also performed by subjecting test specimens to 10%NaOH liquid for two weeks. The results give no indication of chemical attack to specimens of ceramic tile and mortar. The results are discussed and important conclusions are drawn to encourage c
... Show MorePrevious experimental studies have suggested that hot mixed asphalt (HMA) concrete using hydrated lime (HL) to partially replace the conventional limestone dust filler at 2.5% by the total weight of all aggregates showed an optimum improvement on several key mechanical properties, fatigue life span and moisture susceptibility. However, so far, the knowledge of the thermal response of the modified asphalt concrete and thermal influence on the durability of the pavement constructed are still relatively limited but important to inform pavement design. This paper, at first, reports an experimental study of the tensile fatigue life of HMA concrete mixes designed for wearing layer application. Tests were conducted under three different temperatur
... Show MoreBackground: This in vitro study was carried out to evaluate the effects of various veneering dentin ceramic thicknesses and repeated firings on the color of lithium disilicate glass-ceramic (IPS e.max Press) and zirconium-oxide (IPS ZirCAD) all-ceramic systems, measured by clinical spectrophotometers (Easyshade Advance 4.0) . Materials and methods: The 72specimens cube-shaped have the dimension of about 11 mm in width, 14 mm in length, 1mm in thickness, these cores divided into 3 groups according to the type of material each group have (24)core specimens. Each group had been divided into three sub-groups (each having 8 specimens) according to veneering with dentin ceramic thicknesses: as 0.5, 1, or 2 mm (n=8). IPS e.max press and ZirCAD c
... Show MoreZirconia ceramic restoration (ZCR) has a higher fracture incidence rate than metal ceramic restoration. Different surface treatments were used to improve fracture performance of ZCR such as grit blasting (GB) by aluminium oxide powder. This type of surface treatment generate residual stresses on veneering ceramic causing crack initiation and ending with a fracture. In order to overcome the stress generated by GB, zirconia surface coating is used as a surface treatment to improve fracture resistance and to accommodate stresses along the ZCR layers. Fifty zirconia ceramic crowns were fabricated and divided according to the type of surface treatment into three groups; the first group is (ZG), involving 20 cores were coated with a mixture of pa
... Show MoreGypseous soils are common in several regions in the world including Iraq, where more than 28.6% of its surface is covered with this type of soil. This soil, with high gypsum content, causes different problems for construction and strategic projects. As a result of water flow through the soil mass, the permeability and chemical arrangement of these soils varies with time due to the solubility and leaching of gypsum. In this study, the soil of 36% gypsum content, was taken from one location about 100 km southwest of Baghdad, where the samples were taken from depths (0.5 - 1) m below the natural ground and mixed with (3%, 6%, 9%) of Copolymer and Novolac polymer to improve the engineering properties that include: collapsibility, perm
... Show MoreRandom throwing of industrial waste has a significant impact on the environment unless it takes into account the conditions of engineered destroying and/or re-used. Taking the advantage of re-using waste materials in engineering projects represents a well-planned project in order to resolve a lot of engineering problems for some difficult soils. The objective of this study was to evaluate the capability and effects of Rubber Shreds (RS) from scrap torn belts towards improving the shear strength of soft clay. A direct shear tests were conducted on soft clay-RS mixture. The following parameters were investigated to study the influence of RS content, water content, normal stress, and dilation ratio. From experimental test results it was fou
... Show More