The Moisture damage is considered as one of the main challenge for the experts in the field of asphalt pavement design. The aims of the present study is to modify moisture resistance of the asphalt concrete by utilizing ceramic fibers as a type of reinforcement incorporated with hydrated lime. For this purpose, a penetration grade of the asphalt cement (40-50) was utilized as a binder with an aggregate of the maximum nominal size of 12.5mm and mineral filler limestone dust. A series of specimens has been fabricated by utilizing 0.50, 1.0, 1.5, and 2.0 percentages of ceramic fibers. For each of these contents, another subsequent group of specimens with hydrated lime with 0.0, 1.0, 1.5, and 2.0 percentages were moulded. For the addition of ceramic fiber and hydrated lime to the mixtures the dry method for ceramic fiber was adopted while for the hydrated lime, the saturated surface dry method was adopted. The results of this study have shown that the addition of 1% ceramic fiber with 1.5% hydrated lime recorded the highest levels of growth. Furthermore, the outputs of the tests used in this study have shown that the use of ceramic fibers resulted in a growth in the value of tensile strength ratio (TSR) and in the index of retained strength (IRS) compared with the control mixture. Maximum values for TSR were achieved at 1% ceramic fibers with 1.5 % hydrated lime.
Cohesive soils present difficulties in construction projects because it usually contains expansive clay minerals. However, the engineering properties of cohesive soils can be stabilized by using various techniques. The research aims to elaborate on the influences of using hydrated lime on the consistency, compaction, and shear strength properties of clayey soil samples from Sulaimnai city, northern Iraq. The proportions of added hydrated lime are 0%, 2.5%, 5%, 7.5% and 10% to the natural soil sample. The results yielded considerable effects of hydrated lime on the engineering properties of the treated soil sample and enhancement its strength. The soil's liquid limit, plasticity index, and optimum moisture content were de
... Show MoreRecently, increasing material prices coupled with more acute environmental awareness and the implementation of regulation has driven a strong movement toward the adoption of sustainable construction technology. In the pavement industry, using low temperature asphalt mixes and recycled concrete aggregate are viewed as effective engineering solutions to address the challenges posed by climate change and sustainable development. However, to date, no research has investigated these two factors simultaneously for pavement material. This paper reports on initial work which attempts to address this shortcoming. At first, a novel treatment method is used to improve the quality of recycled concrete coarse aggregates. Thereafter, the treated recycled
... Show MoreMany researchers tried to prevent or reduce moisture damage and its sensitivity to temperature to improving the performance of hot mix asphalt because it is decreasing the functional and structural life of fixable pavement due to the moisture damage had exposed to it.
The main objective of this study is to inspect the effect of (fly ash “3%, 6%, 12%”, hydrated lime”5%, 10%, 20%” and silica fumes”1%, 2%, 4%) referring to previous research by the net weight asphalt cement as a modified material on the moisture and temperature sensitivity of hot mix asphalt. This was done using asphalt from AL-Nasiria refinery with penetration grade 40-50, nominal maximum size (12.5) mm (surface course) of aggregate and on
... Show MoreThis investigation was undertaken to evaluate the effectiveness of using Hydrated lime as a (partial substitute) by weight of filler (lime stone powder) with five consecutive percentage namely (1.0, 1.5, 2.0, 2.5, 3.0) % by means of aggregate treatment, by introducing dry lime on dry and 2–3% Saturated surface aggregate on both wearing and binder coarse. Marshall design method, indirect tensile test and permanent deformation under repeated loading of Pneumatic repeated load system at full range of temperature (20, 40, 60) C0 were examined The study revealed that the use of 2.0% and 1.5 % of dry and wet replacement extend the pavement characteristics by improving the Marshall properties and increasing the TSR%. Finally, increase permanent
... Show MoreDespite widespread agreement on the beneficial nature of hydrated lime (HL) addition to asphalt concrete mixes, understanding of the effect of HL particle size is still limited. Previous investigations have focused mainly on two different size comparisons, and so certain guidance for a practical application cannot yet be produced. This study investigates three distinct sizes of HL, in the range of regular, nano, and sub-nano scales, for their effects on the properties of modified asphalt concretes. Five different percentages of HL as a partial replacement of ordinary limestone filler in asphalt concrete mixes were studied for wearing course application purposes. Experimental tests were conducted to evaluate the mechanical properties
... Show MoreImplementation of Warm Mix Asphalt concrete (WMA) is getting global acceptance due to the restrictions for protecting the environment and the requirements to reduce fuel consumption. In this investigation, two WMA mixtures have been prepared in the laboratory using medium curing cutback (MC-30) and Cationic emulsion asphalt. Hot Mix Asphalt (HMA) was also prepared for comparison. The cylinder specimens (63.5mm) in height and (101.6mm) in diameter were constructed from the mixtures and subjected to indirect tensile strength test to determine the Tensile Strength Ratio (TSR). The cylinder specimens of (101.6mm) in height and (101.6mm) in diameter were also constructed from those mixtures and subjected to static compressive
... Show MoreRecently, some of Iraq's newly constructed asphalt concrete pavements showed premature failures with significant negative impacts on roadway safety and the economy. Using Nano hydrated lime (NHL) in pavement construction could be one of the possible steps to improve pavement durability. This article discusses how NHL affects the durability of hot mix asphalt. NHL was added in two methods to the asphalt concrete mixture for the wearing course. The first is the dry method, i.e., on the aggregate, whereas the second is the wet addition method, i.e., to the bitumen. The percentages were tried for each additional method; 1, 2, and 3% by weight of aggregate for the dry method and 0.5, 1, and 1.5% by weight of asphalt concrete for the wet
... Show MorePremature failure in asphalt concrete pavement has been the main concern for pavement construction companies and engineers in recent years because of the large rise in traffic volume and loads and the temperature extremes in the summer and winter. The use of modifiers in asphalt concrete mixtures has attracted much attention to increase the performance and lifespan of pavements. As nanotechnology developed, several researchers concentrated on how these materials can help increase pavement serviceability by minimizing rutting and moisture damage. This study evaluates the Hydrated Lime (HL) effect by two methods (wet and dry hydrated lime) on the durability of the warm mix asphalt. The first method, HL, has been supplemented to the as
... Show MoreThe purpose of this study is to evaluate the effect of hydrated lime addition methods as filler replacement on fatigue performance of Hot Mix Asphalt (HMA). Three types of addition methods of hydrated lime were introduced namely dry HL on dry aggregate and saturated surface aggregate above 3% and slurry HL on dry aggregate, ordinary Lime stone powder was reduced by three HL percentage (1.0, 2.0 and 3.0 %). The effect of different methods were investigated on the fatigue properties of HMA using, third-point flexural fatigue bending Test. Pneumatic Repeated Load System (PRLS) was carried out to establish the effect of hydrated lime on the fatigue failure criteria and to select the proper hydrated lime application methods on fatigue behavior o
... Show MoreThis paper reports on the experimental study, which conducted a series of triaxial tests for the asphalt concrete using hydrated lime as a mineral additive. Three HMA mixes, prepared by the specification for wearing, levelling and base layers, were studied under three different temperatures. The test results have demonstrated that, compared with the control mixes excluding HL, the permanent deformation resistance of the HL modified mixes has significant improvement. The deformation has been reduced at the same load repetition number, meanwhile the flow number has been considerably increased. The degree of improvement in permanent deformation resistance using HL is more pronounced at high stress deviation states and high temperature.
... Show More