Preferred Language
Articles
/
zea_Mp4BmraWrQ4dTl8i
Effect of Fire Exposure on the Properties of Self-Compacting Concrete reinforced by Glass Fibers
...Show More Authors

The optimal design of any structural elements requires examining all environmental risks, emergency accidents, and standard load cases. Exposure to fire is one of the most common safety threats. Nowadays wide developments are achieved in the field of concrete technology, therefore, experimental and theoretical investigations should be performed on the characteristics of such developed materials under different loading conditions. This study investigates the impact of fire exposure on the mechanical characteristics of self-compacting concrete, specifically compressive and tensile strength, modulus of elasticity, and stress-strain relation. The adopted fire exposure consisted of six steady-state temperatures (300, 400, 500, 600, 700, and 800°C) for one hour and a sudden cooling method. Four glass fiber volume fractions were adopted: 0, 0.5, 1, and 1.5%. The glass fiber volume fractions considered (0.5-1.5%) improved the mechanical properties investigated. Two states were detected for the effect of fire exposure. The effect of fire exposure was inversely proportional to fiber content in burning temperatures of 300-700°C, while the reduction in mechanical properties of 1.5% fiber content was greater than those of 0.5 and 1% when the temperature increased to 800°C. Furthermore, the addition of glass fiber changed the brittle mode stress-strain relation to semi-ductile for the non-burned and burned up to 600°C specimens, whereas a brittle behavior was detected when the temperature increased above 600°C. In general, a similar effect was noticed for all the glass fiber ratios considered regarding the slope of the stress-strain linear stage compared to the non-burned specimens, which was more salient when the burning temperature increased.

Scopus Crossref
View Publication
Publication Date
Sun Aug 01 2021
Journal Name
Journal Of Composites For Construction
Prediction of Concrete Cover Separation in Reinforced Concrete Beams Strengthened with FRP
...Show More Authors

View Publication
Publication Date
Sun Aug 01 2021
Journal Name
Journal Of Composites For Construction
Prediction of Concrete Cover Separation in Reinforced Concrete Beams Strengthened with FRP
...Show More Authors

Scopus (21)
Crossref (20)
Scopus Clarivate Crossref
Publication Date
Mon Aug 01 2016
Journal Name
Journal Of Engineering
Behavior of Reinforced Concrete Deep Beams Strengthened with Carbon Fiber Reinforced Polymer Strips
...Show More Authors

This research is concerned to investigate the behavior of reinforced concrete (RC) deep beams strengthened with carbon fiber reinforced polymer (CFRP) strips. The experimental part of this research is carried out by testing seven RC deep beams having the same dimensions and steel reinforcement which have been divided into two groups according to the strengthening schemes. Group one was consisted of three deep beams strengthened with vertical U-wrapped CFRP strips. While, Group two was consisted of three deep beams strengthened with inclined CFRP strips oriented by 45o with the longitudinal axis of the beam. The remaining beam is kept unstrengthening as a reference beam. For each group, the variable considered

... Show More
View Publication Preview PDF
Publication Date
Tue Jan 19 2021
Journal Name
Sn Applied Sciences
Post-fire serviceability and residual strength of composite post-tensioned concrete T-beams
...Show More Authors
Abstract<p>In this study, the response of ten composite post-tensioned concrete beams topped by a reinforced concrete deck with adequate reinforcing shear connectors is investigated. Depending on the concrete compressive strength of the deck slab (20, 30, and 40 MPa), beams are grouped into three categories. Seven of these beams are exposed to a fire attack of 700 and 800 °C temperature simultaneously with or without the presence of a uniformly distributed sustained static loading. After cooling back to ambient temperature, these composite beams are loaded up to failure, using a force control module, by monotonic static loading in a four-point-bending setup with two symmetrical concentrated loads applied in </p> ... Show More
View Publication Preview PDF
Scopus (8)
Crossref (7)
Scopus Clarivate Crossref
Publication Date
Tue Jan 19 2021
Journal Name
Sn Applied Sciences
Post-fire serviceability and residual strength of composite post-tensioned concrete T-beams
...Show More Authors
Abstract<p>In this study, the response of ten composite post-tensioned concrete beams topped by a reinforced concrete deck with adequate reinforcing shear connectors is investigated. Depending on the concrete compressive strength of the deck slab (20, 30, and 40 MPa), beams are grouped into three categories. Seven of these beams are exposed to a fire attack of 700 and 800 °C temperature simultaneously with or without the presence of a uniformly distributed sustained static loading. After cooling back to ambient temperature, these composite beams are loaded up to failure, using a force control module, by monotonic static loading in a four-point-bending setup with two symmetrical concentrated loads applied in </p> ... Show More
Crossref (7)
Crossref
Publication Date
Fri May 01 2020
Journal Name
Civil Engineering Journal
Post-Fire Behavior of Post-Tensioned Segmental Concrete Beams under Monotonic Static Loading
...Show More Authors

This paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,

... Show More
Crossref (1)
Crossref
Publication Date
Fri May 01 2020
Journal Name
Civil Engineering Journal
Post-Fire Behavior of Post-Tensioned Segmental Concrete Beams under Monotonic Static Loading
...Show More Authors

This paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,

... Show More
View Publication Preview PDF
Scopus (1)
Crossref (1)
Scopus Clarivate Crossref
Publication Date
Wed Oct 09 2019
Journal Name
Engineering, Technology &amp; Applied Science Research
Numerical Analysis of Segmental Post Tensioned Concrete Beams Exposed to High Fire Temperature
...Show More Authors

The main objective of this study is to characterize the main factors which may affect the behavior of segmental prestressed concrete beams comprised of multi segments. The 3-D finite element program ABAQUS was utilized. The experimental work was conducted on twelve simply supported segmental prestressed concrete beams divided into three groups depending on the precast segments number. They all had an identical total length of 3150mm, but each had different segment numbers (9, 7, and 5 segments), in other words, different segment lengths. To simulate the genuine fire disasters, nine beams were exposed to high-temperature flame for one hour, the selected temperatures were 300°C (572°F), 500°C (932°F) and 700°C (1292°F) as recomm

... Show More
View Publication Preview PDF
Crossref (6)
Crossref
Publication Date
Sun Sep 04 2016
Journal Name
Baghdad Science Journal
Study the Shielding Properties against Gamma-rays for Epoxy Resin Reinforced by Different materials
...Show More Authors

In the present work the Buildup factor for gamma rays were studied in shields from epoxy reinforced by lead powder and by aluminum powder, for NaI(Tl) scintillation detector size ( ×? ), using two radioactive sources (Co-60 and Cs-137). The shields which are used (epoxy reinforced by lead powder with concentration (10-60)% and epoxy reinforced by aluminum powder with concentration (10-50)% by thick (6mm) and epoxy reinforced by lead powder with concentration (50%) with thick (2,4,6,8,10)mm. The experimental results show that: The linear absorption factor and Buildup factor increase with increase the concentration for the powders which used in reinforcement and high for aluminum powder than the lead powder and decrease with inc

... Show More
View Publication Preview PDF
Crossref
Publication Date
Fri Oct 01 2010
Journal Name
Iraqi Journal Of Physics
Effect ofweight percentage chopped carbon fibers on the mechanism of cracks propagation for Epoxy composites
...Show More Authors

In this research, the mechanism of cracks propagation for epoxy/ chopped carbon fibers composites have been investigated .Carbon fibers (5%, 10%, 15%, and 20%) by weight were used to reinforce epoxy resin. Bending test was carried out to evaluate the flexural strength in order to explain the mechanism of cracks propagation. It was found that, the flexural strength will increase with increasing the percentage weight for carbon fibers. At low stresses, the cracks will state at the lower surface for the specimen. Increasing the stresses will accelerate the speed of cracks until fracture accorded .The path of cracks is changed according to the distributions of carbon fibers

View Publication Preview PDF