Preferred Language
Articles
/
yoa_t4YBIXToZYAL_7Md
Numerical Analysis of Segmental Post Tensioned Concrete Beams Exposed to High Fire Temperature
...Show More Authors

The main objective of this study is to characterize the main factors which may affect the behavior of segmental prestressed concrete beams comprised of multi segments. The 3-D finite element program ABAQUS was utilized. The experimental work was conducted on twelve simply supported segmental prestressed concrete beams divided into three groups depending on the precast segments number. They all had an identical total length of 3150mm, but each had different segment numbers (9, 7, and 5 segments), in other words, different segment lengths. To simulate the genuine fire disasters, nine beams were exposed to high-temperature flame for one hour, the selected temperatures were 300°C (572°F), 500°C (932°F) and 700°C (1292°F) as recommended by ASTM–E119. Four numerical models have been utilized to represent the unburned and the burned specimens at the three elevated temperatures. Calibration and simulation of the experimental work were conducted, while comparisons were made with the experimental results. These included the prestress effect, load-deflection relation under applied load, and load at failure of the reference beam and the beams after the exposure to fire.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Sat Aug 10 2019
Journal Name
Engineering, Technology & Applied Science Research
Performance of Segmental Post-Ī¤ensioned Concrete Beams Exposed to High Fire Temperature
...Show More Authors

The present study illustrates observations, record accurate description and discussion about the behavior of twelve tested, simply supported, precast, prestressed, segmental, concrete beams with different segment numbers exposed to high fire temperatures of 300°C, 500°C, and 700°C. The test program included thermal tests by using a furnace manufactured for this purpose to expose to high burning temperature (fire flame) nine beams which were loaded with sustaining dead load throughout the burning process. The beams were divided into three groups depending on the precast segments number. All had an identical total length of 3150mm but each had different segment number (9, 7, and 5 segments), in other words, different segment length

... Show More
View Publication Preview PDF
Crossref (6)
Crossref
Publication Date
Fri May 01 2020
Journal Name
Civil Engineering Journal
Post-Fire Behavior of Post-Tensioned Segmental Concrete Beams under Monotonic Static Loading
...Show More Authors

This paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,

... Show More
Crossref (1)
Crossref
Publication Date
Fri May 01 2020
Journal Name
Civil Engineering Journal
Post-Fire Behavior of Post-Tensioned Segmental Concrete Beams under Monotonic Static Loading
...Show More Authors

This paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,

... Show More
View Publication Preview PDF
Scopus (1)
Crossref (1)
Scopus Clarivate Crossref
Publication Date
Thu Feb 01 2018
Journal Name
Association Of Arab Universities Journal Of Engineering Sciences
Effect of High Temperature (Fire Flame) on the Behavior of Post-tensioned Concrete Beams
...Show More Authors

View Publication Preview PDF
Publication Date
Tue Jan 19 2021
Journal Name
Sn Applied Sciences
Post-fire serviceability and residual strength of composite post-tensioned concrete T-beams
...Show More Authors
Abstract<p>In this study, the response of ten composite post-tensioned concrete beams topped by a reinforced concrete deck with adequate reinforcing shear connectors is investigated. Depending on the concrete compressive strength of the deck slab (20, 30, and 40 MPa), beams are grouped into three categories. Seven of these beams are exposed to a fire attack of 700 and 800 °C temperature simultaneously with or without the presence of a uniformly distributed sustained static loading. After cooling back to ambient temperature, these composite beams are loaded up to failure, using a force control module, by monotonic static loading in a four-point-bending setup with two symmetrical concentrated loads applied in </p> ... Show More
View Publication Preview PDF
Scopus (3)
Crossref (3)
Scopus Clarivate Crossref
Publication Date
Tue Jan 19 2021
Journal Name
Sn Applied Sciences
Post-fire serviceability and residual strength of composite post-tensioned concrete T-beams
...Show More Authors
Abstract<p>In this study, the response of ten composite post-tensioned concrete beams topped by a reinforced concrete deck with adequate reinforcing shear connectors is investigated. Depending on the concrete compressive strength of the deck slab (20, 30, and 40 MPa), beams are grouped into three categories. Seven of these beams are exposed to a fire attack of 700 and 800 °C temperature simultaneously with or without the presence of a uniformly distributed sustained static loading. After cooling back to ambient temperature, these composite beams are loaded up to failure, using a force control module, by monotonic static loading in a four-point-bending setup with two symmetrical concentrated loads applied in </p> ... Show More
Crossref (4)
Crossref
Publication Date
Fri Aug 10 2018
Journal Name
In Book: Challenges In Mechanics Of Time-dependent Materials, Volume 2edition: 1stchapter: 12
Experimental Investigation of Segmental Post-tensioned Girders
...Show More Authors

Scopus (2)
Scopus Clarivate Crossref
Publication Date
Thu May 18 2023
Journal Name
Journal Of Engineering
Behaviour of Fire Exposed Reinforced Concrete Rigid Beams with Restrained Ends
...Show More Authors

This paper is devoted to investigate the effect of burning by fire flame on the behavior and load carrying capacity of rectangular reinforced concrete rigid beams. Reduced scale beam models (which are believed to resemble as much as possible field conditions) were suggested. Five end restrained beam specimens were cast and tested. The specimens were subjected to fire flame temperatures ranging from (25-750) ºC at age of 60 days, two temperature levels of 400ºC and 750ºC were chosen with exposure duration of 1.5 hour. The cast rectangular reinforced concretebeam (2250×375×375 mm) (length× width× height respectively) were subjected to fire. Results indicate remarkable reduction in the ultrasonic pulse velocity and rebound number of

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Wed Jan 31 2018
Journal Name
Engineering Journal
Residual Strength of Composite Unprotected Steel-Deck Floor Exposed to High Temperature (Fire Flame)
...Show More Authors

View Publication Preview PDF
Scopus (1)
Scopus Clarivate Crossref
Publication Date
Thu Feb 01 2018
Journal Name
Association Of Arab Universities Journal Of Engineering Sciences
Performance of composite unprotected steel Beam-deck floor exposed to high temperature (fire flame)
...Show More Authors

An experimental program was conducted to determine the residual of composite Steel Beams-Reinforced Concrete (SB-RC) deck floors fabricated from a rolled steel beam topped with a reinforced concrete slab, exposed to high temperatures (fire flame) of 300, 500, and 700ºC for 1 hour, and then allowed to cool down by leaving them in the lab condition to return to the ambient temperature. The burning results showed that, by exposing them to a fire flame of up to 300ºC, no serious permanent deflection occurred. It was also noticed that the specimen recovered 93% of 19.2 mm of the deflection caused by burning. The recovered deflection of burned composite SB-RC deck floor at 500ºC was 40% of 77.9 mm of the deflection caused by burning with a res