Optical losses represent one of the primary obstacles to increasing the efficiency of silicon solar cells. The recommended solution to minimize optical losses is the use of plasmonic metal nanoparticles; however, they act as recombination centers within the solar cell construction, leading to a decrease in performance. The goal of this article is to introduce cobalt/graphene nanoparticles into the solar cell to minimize the optical losses. An ultra-thin film silicon PIN solar cell of dimensions (400 ×400 ×900) nm3 with ring metal contact shape was designed and numerically investigated using COMSOL Multiphysics software version 6.2 by the finite element method (FEM). Core/shell cobalt-graphene (Co/Gr) nanoparticles are periodically introduced into the cell between two layers (electron transport and active) in a ratio of 50:50 with an inter-spacing of a similar diameter. The Co/Gr parameters, number of nanoparticles (2, 4, 6), radius (10, 20, 30) nm, and shell thickness (1, 2, 4) nm were extensively studied. In addition, the arrangement of the core/shell nanoparticle material was considered. The results manifest the best performance of the proposed cell at 4 nanoparticles of 30 nm radius with 2 nm shell thickness for Co/Gr nanoparticles to get a maximum photocurrent of 26.28 mA/cm2. It is concluded that the optical losses of the Co/Gr core/shell nanoparticles embedded in an ultra-thin film silicon solar cell are significantly reduced owing to the increment in the absorption and hence the photocurrent. This enhancement opens a new avenue for further improvements.
The synthesis oxadiazole derivative 2,5-disubstituted-1,3,4oxadiazole (3a,3b,3c) was prepared from reaction of N-(4-amino benzene sulphonyl)Morpholipebut-2-enehydrazide with (4-hydroxybenzaldehyde,4-methoxy benzaldehyde,4-ethoxybenzaldehyde) in the presence of lone as catalyst. The structure of (3a,3b,3c) was characterized by using FT-IR, H-NMR and spectroscopy. Nanoparticles of the prepared compounds have been fabricated in aqueous media using re-precipitation method.Characterization of the nano particles (ONPs) have been performed by using UV-VIS spectrophotometer and scanning electron micro scope ( SEM). The size of the nanoparticales were around 150-200 nm as indicated by (SEM). T
Polyacrylamide Solutions of different concentrations (0.2, 0.4, 0.6, 0.8, 1.0 %) of Ag nanoparticles and ZnO nanoparticles were prepared, the viscosities and surface tension were measured for all solutions, where measurements indicated an increase in these properties with increased concentration, where the relative viscosity of polyacrylamide/zinc nanoparticles increased from 1.275 to 2.243, and the relative viscosity of polyacrylamide/silver nanoparticles increased from 1.178 to 1.934. Viscosity is significant parameters during electrospinning process. While the surface tension of the polyacrylamide/zinc nanoparticles has changed from 0.0343 Nm-1 to .0.0.0 Nm-1 and changed from .0.000Nm-1 to.0.0.0 Nm-1. Also the constants KH and KK were
... Show MoreTheoretical calculation of the electronic current at N 3 contact with TiO 2 solar cell devices ARTICLES YOU MAY BE INTERESTED IN Theoretical studies of electronic transition characteristics of senstizer molecule dye N3-SnO 2 semiconductor interface AIP Conference. Available from: https://www.researchgate.net/publication/362813854_Theoretical_calculation_of_the_electronic_current_at_N_3_contact_with_TiO_2_solar_cell_devices_ARTICLES_YOU_MAY_BE_INTERESTED_IN_Theoretical_studies_of_electronic_transition_characteristics_of_senstiz [accessed May 01 2023].
ABSTRACT: Thin film of CdS has been deposited onto clean glass substrate by using Spray pyrolysis technique. Results of Morphological (AFM) studied; electrical properties and optical conductivity studied are analysis. AFM results show a crystalline nature of the films. From the conductivity measurement at different temperatures, the activation energy of the films was calculated and found to be between 0.188 - 0.124 eV for low temperature regions, and between 1.67-1.19eV for high temperature regions. Hall measurements of electrical properties at room temperature show that the resistivity and mobility of CdS polycrystalline films deposited at 400 C0, were 3.878x103 . cm and 1.302x104cm2/ (V.s), respectively. The electrical conductivity of th
... Show MoreVacuum evaporation technique was used to prepare pure and doped ZnS:Pb thin films at10% atomic weight of Pb element onto glass substrates at room temperature for 200 nm thickness. Effect of doping on a.c electrical properties such as, a.c conductivity, real, and imaginary parts of dielectric constant within frequency range (10 KHz - 10 MHz) are measured. The frequency dependence of a.c conductivity is matched with correlated barrier hoping especially at higher frequency. Effect of doping on behavior of a.c mechanism within temperature range 298-473 K was studied.
BixSb2-xTe3 alloys with different ratios of Bi (x=0, 0.1, 0.3, 0.5, and 2) have been prepared, Thin films of these alloys were prepared using thermal evaporation method under vacuum of 10-5 Torr on glass substrates at room temperature with different deposition rate (0.16, 0.5, 0.83) nm/sec for thickness (100, 300, 500) respectively. The X–ray diffraction measurements for BixSb2-xTe3 bulk and thin films indicate the polycrystalline structure with a strong intensity of peak of plane (015) preferred orientation with additional peaks, (0015) and (1010 ) reflections planes, which is meaning that all films present a very good texture along the (015) plane axis at different intensities for each thin film for different thickness. AFM measureme
... Show MoreA thin film of (SnSe) and SnSe:Cu with various Cu ratio (0,3,5 and 7)% have been prepared by thermal evaporation technique with thickness 400±20 nm on glass substrate at (R.T). The effect of Cu dopants concentration on the structural, morphological, optical and electrical properties of (SnSe) Nano crystalline thin films was explored by using X-ray diffraction (XRD), scanning electron microscopy (SEM), atomic force microscopy (AFM), energy dispersive spectroscopy (EDS), UV–Vis absorption spectroscopy and Hall Effect measurement respectively. X-ray diffraction analysis reveal the polycrystalline nature of the all films deposited with orthorhombic structure which possess a preferred orientation along the (111) plane. The crystalline sizes o
... Show More