The growing demand for optical fibers is due to their superior the ability to transmit information with high efficiency and minimal loss across extensive distances. In this study, four optical fibers with core radii ranging from (2.05-5.05) μm, and with a numerical aperture of 0.1624 were analyzed. The modal properties of these fibers were calculated at a wavelength of 1030 nm using the RP Fiber Calculator software (free version 2025). Furthermore, the impact of increasing the core radius on these properties was examined. The results showed that multimode fibers are formed when the core radius is much larger than the wavelength used. In contrast, single-mode fiber is obtained when this condition is not met. Five modes properties were calculated: cut-off wavelength, effective area, power in the core, propagation constant and effective refractive index. The geometric distribution of the amplitudes of all modes was graphically represented.
Optical properties of chromium oxide (Cr2O3) thin films which were prepared by pulse laser deposition method, onto glass substrates. Different laser energy (500-900) mJ were used to obtain Cr2O3 thin films with thickness ranging from 177.3 to 372.4 nm were measured using Tolansky method. Then films were annealed at temperature equal to 300 °C. Absorption spectra were used to determine the absorption coefficient of the films, and the effects of the annealing temperature on the absorption coefficient were investigated. The absorption edge shifted to red range of wavelength, and the optical constants of Cr2O3 films increases as the annealing temperature increased to 300 °C. X-ray diffraction (XRD) study reveals that Cr2O3 thin films are a
... Show MoreThis paper reports the effect of Mg doping on structural and optical properties of ZnO prepared by pulse laser deposition (PLD). The films deposited on glass substrate using Nd:YAG laser (1064 nm) as the light source. The structure and optical properties were characterized by X-ray diffraction (XRD) and transmittance measurements. The films grown have a polycrystalline wurtzite structure and high transmission in the UV-Vis (300-900) nm. The optical energy gap of ZnO:Mg thin films could be controlled between (3.2eV and 3.9eV). The refractive index of ZnO:Mg thin films decreases with Mg doping. The extinction coefficient and the complex dielectric constant were also investigate.
Undoped and Co-doped zinc oxide (CZO) thin films have been prepared by spray pyrolysis technique using solution of zinc acetate and cobalt chloride. The effect of Co dopants on structural and optical properties has been investigated. The films were found to exhibit maximum transmittance (~90%) and low absorbance. The structural properties of the deposited films were examined by x-ray diffraction (XRD). These films, deposited on glass substrates at (400? C), have a polycrystalline texture with a wurtzite hexagonal structure, and the grain size was decreased with increasing Co concentration, and no change was observed in lattice constants while the optical band gap decreased from (3.18-3.02) eV for direct allowed transition. Other parameters
... Show MoreSilver sulfide and the thin films Ag2Se0.8Te0.2 and Ag2Se0.8S0.2 created by the thermal evaporation process on glass with a thickness of 350 nm were examined for their structural and optical properties. These films were made at a temperature of 300 K. According to the X-ray diffraction investigation, the films are polycrystalline and have an initial orthorhombic phase. Using X-ray diffraction research, the crystallization orientations of Ag2Se and Ag2Se0.8Te0.2 & Ag2Se0.8S0.2 (23.304, 49.91) were discovered (XRD). As (Ag2Se and Ag2Se0.8Te0.2 & Ag2Se0.8S0.2) absorption coefficient fell from (470-774) nm, the optical band gap increased (2.15 & 2 & 2.25eV). For instance, the characteristics of thin films made of Ag2Se0.8Te0.2 and Ag2Se0.8S0.2
... Show MoreAlxSb1-x compounds with different aluminum content(x=0.1, 0.3 , 0.5 , 0.7 and 0.9 ) were prepared by mixing the two elements in the appropriate ratios in quartz ampulla which then sealed and put in an oven at 1273 and left 5 hours. The obtained powder were grinded and then pressed in pellets shape which will be the target to prepare thin films samples. AlxSb1-x thin films were synthesized by PLD with ~ 150nm in thickness .The structures of AlxSb1-x powders and thin films were determined using X–ray diffraction. The data revealed that all the prepare AlxSb1-x bulk and thin films have polycrystalline . The results showed that increasing of Al reduced the crystallinity of the prepared samples at the first but then the opposite take pla
... Show MoreStructural and optical properties of CdO and CdO0.99Cu0.01 thin
films were prepared in this work. Cadmium Oxide (CdO) and
CdO0.99Cu0.01semiconducting films are deposited on glass substrates
by using pulsed laser deposition method (PLD) using SHG with Qswitched
Nd:YAG pulsed laser operation at 1064nm in 6x10-2 mbar
vacuum condition and frequency 6 Hz. CdO and CdO0.99Cu0.01 thin
films annealed at 550 C̊ for 12 min. The crystalline structure was
studied by X-ray diffraction (XRD) method and atomic force
microscope (AFM). It shows that the films are polycrystalline.
Optical properties of thin films were analyzed. The direct band gap
energy of CdO and CdO0.99Cu0.01 thin films were determined from
(αhυ)1/2 v
Abstract
This study was conducted by using soil map of LD7 project to interpret the
distribution and shapes of map units by using the index of compaction as an
index of map unit shape explanation. Where there were wide and varied
ranges of compaction index of map units, where the maximum value was
0.892 for MF9 map unit and the lower value was 0.010 for same map unit.
MF9 has wide range appearance of index of compaction after those indices
were statistically analyzed by using cluster analysis to group the similar
ranges together to ease using their values, so the unit MF9 was considered as
key map unit that appears in the soils of LD7 project which may be used to
expect another map units existence in area of
Anodic electrodeposition was used to synthesize a composite electrode of nanostructured manganese dioxide/carbon fiber (CF) galvanostatically. Different characterization results of the nanostructured MnO2 were obtained by varying the H2SO4 concentration and the current density. Field emission scanning electron microscopy, X‐ray diffraction, and atomic force microscopy were utilized to characterize the prepared composite electrodes. The best conditions were: 0.3 mA cm−2 current density and 0.64 M H2SO4 concentration. The electrosorption performance of the MnO
Blood samples were collected from (31) pregnant women infected with cytomegalovirus , also (15) blood samples were collected from congenitally infected infants, and (20),(15),(15) blood samples were collected from pregnant women ,non pregnant and infants, respectively, all of them were as control groups. CMV infection identified by using ELISA assay to detect specific CMV IgM & IgG in sera. The results of lymphocyte transformation showed a significant decrease when phytoheamagglutinin (PHA) used as stimulator, lymphocytes response in infected pregnant women was lower than that of non infected pregnant women as well as non pregnant women. Result also showed a significant decrease in the ability of lymphocyte division in healthy pregnant w
... Show More