This in vitro study evaluated the influence of chemomechanical caries removal solution on the surface topography of metal-ceramic feldspar porcelain (MAJOR ceramic) and All-ceramic feldspar porcelain (Vita Alpha) using light polarizing microscope. Forty specimens of MAJOR ceramic and forty specimens of Vita Alpha ceramic of (12mm diameter & 3mm height) were prepared .All specimens were polished with silicon polishing burs, cleaned, autoglazed and stored in 37°C before exposure to Carisolv. Thirty specimens of each material randomly exposed to Carisolv gel for 5, 10 and 20 minutes respectively, other ten specimens were not, to act as control group. All specimens were subjected to surface roughness test by profilometer and evaluated using light polarizing microscope. ANOVA and student t-test were used to analyze the surface roughness values.Different exposure times of modified Carisolv gel showed highly significant difference compared to control (P<0.001).Surface treatment with modified Carisolv gel for 20 minutes resulted in the highest surface roughness. Metal-ceramic feldspar porcelain (MAJOR ceramic) showed high surface roughness than all ceramic feldspar porcelain (Vita Alpha), however, the difference is statistically not significant (P>0.05).Different exposure times of modified Carisolv gel affect the surface roughness of dental ceramic materials differently. This study showed major influence on surface topography after exposure to modified Carisolv gel for 20 minutes on dental ceramics MAJOR and Vita Alpha.
Polyacrylamide Solutions of different concentrations (0.2, 0.4, 0.6, 0.8, 1.0 %) of Ag nanoparticles and ZnO nanoparticles were prepared, the viscosities and surface tension were measured for all solutions, where measurements indicated an increase in these properties with increased concentration, where the relative viscosity of polyacrylamide/zinc nanoparticles increased from 1.275 to 2.243, and the relative viscosity of polyacrylamide/silver nanoparticles increased from 1.178 to 1.934. Viscosity is significant parameters during electrospinning process. While the surface tension of the polyacrylamide/zinc nanoparticles has changed from 0.0343 Nm-1 to .0.0.0 Nm-1 and changed from .0.000Nm-1 to.0.0.0 Nm-1. Also the constants KH and KK were
... Show MoreBackground: This study was conducted to evaluate the surface roughness and dimensional accuracy of commercially obtainable alginate impression material in terms of imbibition after immersion in two different media. Materials and method: Two disinfecting agents, ethanol 70% and povidone-iodine 4%, were used to access the dimensional accuracy and surface roughness of alginate impression material. Weights of specimen discs of alginate impressions were measured before and immediately after immersion to gain a measure of imbibition. For surface roughness, disinfected specimens rectangle was examined before and after disinfection. Results: Minimal changes in weight were observed after disinfection, but a statistically non-significant differenc
... Show MoreHuman cerebral cortex is the outer folded neuronal layer and represents major part of the cerebrum with enormous functions. It is a laminar structure, easily visualized grossly. Previous studies showed that the Superior Temporal gyrus is one of the thickest cerebral cortex regions, reaching (about 4 mm). The Electron microscope study was made on 6 samples taken to measure the neuronal soma dimension of the large pyramidal cells present in the internal pyramidal cortical layer V in different age groups and gender. Aging process was obvious on the large pyramidal cells of the cerebral cortex, in which their neuronal soma dimensions showed shrinkage with age progression. But statistically there was no differences in the values between males an
... Show MoreBackground: This study was performed to determine the effect of aging of different types of composite material restorations on: Shear bond strength (SBS) to light cure and no mix chemical cure orthodontic adhesives with sapphire bracket and the debonding failure sites. Materials and methods: One hundred forty four composite disks were made from three different composite resin materials which are: 3M Filtek Z250, 3M filtek Z350 and 3M Valux plus, each group with (48) disks each, then according to the duration of storage each group was subdivided into two equal groups one of them stored for one day and the other was stored for one month, then each group was further subdivided into two equal subgroups with (12) disks each one bonded with ligh
... Show MoreA successful synthesis of mesoporous Santa Barbara amorphous (SBA-15) with nanoparticle size was attempted using prepared sodium silicate from Iraqi high silica sand. EO20PO70EO20 copolymer was used as a template at highly acidic conditions (pH < 2). The effect of crystallization temperature of (100, 110, 120, and 130 0C), and crystallization time of (24, 48, 72, and 120 h) on surface properties was studied. The experiments were characterized using XRD, FTIR, AFM, BET, and FESEM. The XRD and FTIR tests represent amorphous SBA-15 without any impurities. Decreasing average particle size distribution increased the surface area, and decreased the porosity (pore volume, and pore size) in all experiments. The texture properties were su
... Show MoreBackground: Denture lining materials are widely used in prosthodontic treatment and management of traumatized oral mucosa. A contaminated prosthesis can provide a source of cross-contamination between patients and dental personnel as well as a cause for denture stomatitis. Therefore, denture disinfection has been recommended as an essential procedure for maintenance of a healthy oral mucosa. This study investigated the effect of SOLO disinfectant solution on some properties of different denture lining materials. Materials and methods: Three different solutions were used in this study; SOLO disinfectant solution, sodium hypochlorite solution, and water on three types of acrylic denture lining materials; hot cure, cold cure, and soft acrylic
... Show MoreThe aim of this work is to study the influence of the type of fiber glass –mat on fatigue behavior of composite material which is manufactured from polyester and E-glass (woven roving, chopped strand mat (CSM)) as a laminate with a constant fiber volume fraction (VF) of 33%. The results showed that the laminates reinforced with E-glass (woven roving) [0/90, ±45.0/90] and [0/90, CSM, 0/90] have lower fatigue strength than the laminates reinforced with E-glass [0/90]3,[CSM]3 and [CSM, 0/90, CSM] although they had different tensile strength; the best laminate was [0/90]3 .