Results of a study of alloys and films with various Pb content have been reported and discussed. Films of of thickness 1.5
In this research ,Undoped Nio and 1%Li doped Nio thin films were deposited utilizing chemical spray pyrolysis on the glass substrates heated (450C). The effects of non-thermal plasma on the structural and optical properties were studied. XRD measurement shows that Nio and Nio:1%Li films were found to be polycrystalline and have cubic structure with a preferred orientation (111). Decreased crystal size after exposure especially at (7) sec. AFM data indicate that the surface roughness average and (RMS) values of the prepared doped films are increasing after exposure to plasma, the transmittance increases after doped samples exposure to plasma, it was found that the energy gap value decreased when doped samples exposure to plasma, also, thickn
... Show MoreAg-doped NiO thin films were fabricated by dip coating and subsequently annealed at 373, 473, 573, and 673 K to elucidate the influence of annealing temperature on their structural, morphological, optical, and NO2-sensing characteristics. X-ray diffraction confirmed the formation of polycrystalline Ag/NiO films, with progressively improved crystallinity and larger crystallite size at elevated annealing temperatures. Atomic force microscopy revealed a homogeneous surface morphology with grain growth, with the average grain diameter increasing from 26.40 to 34.2 nm. Optical analysis showed high visible-region transmittance (65–70%) and a gradual reduction in the optical band gap from 2.75 to 2.07 eV with increasing annealing temperature. Ga
... Show MorePure and Fe-doped zinc oxide nanocrystalline films were prepared
via a sol–gel method using -
C for 2 h.
The thin films were prepared and characterized by X-ray diffraction
(XRD), atomic force microscopy (AFM), field emission scanning
electron microscopy (FE-SEM) and UV- visible spectroscopy. The
XRD results showed that ZnO has hexagonal wurtzite structure and
the Fe ions were well incorporated into the ZnO structure. As the Fe
level increased from 2 wt% to 8 wt%, the crystallite size reduced in
comparison with the pure ZnO. The transmittance spectra were then
recorded at wavelengths ranging from 300 nm to 1000 nm. The
optical band gap energy of spin-coated films also decreased as Fe
doping concentra
This work investigates the properties of polyvinyl alcohol (PVA) nanocomposite films with varying multi-walled carbon nanotube (MWCNT) content, ranging from 2 to 8 wt.%. The films were prepared using a solution casting method and characterized using UV-visible spectroscopy, optical microscopy, X-ray diffraction, and tensile tests. The prepared PVA/MWCNT nanocomposite films exhibited optical band gap values ranging from 3.5 eV to 5.3 eV. XRD analysis confirmed the semi-crystalline nature of these nanocomposites. Mechanical properties, including hardness, yield strength, ultimate tensile strength, and Young's modulus, were enhanced by increasing MWCNT content by up to 8%. Contact angle measurements showed an increase in hydrophobicity with in
... Show MoreDiamond-like carbon (DLC) homogeneous thin films were deposited from cyclohexane (Ccyclohexane (Ccyclohexane (Ccyclohexane (C cyclohexane (Ccyclohexane (Ccyclohexane (C cyclohexane (Ccyclohexane (C 6H12 ) liquid by using a plasma jet system which operates with alternating high voltage 7.5 which operates with alternating high voltage 7.5which operates with alternating high voltage 7.5which operates with alternating high voltage 7.5 which operates with alternating high voltage 7.5which operates with alternating high voltage 7.5which operates with alternating high voltage 7.5 which operates with alternating high voltage 7.5which operates with alternating high voltage 7.5 which operates with alternating high voltage 7.5which operates with al
... Show MoreThe influence of silver doped n-type polycrystalline CdTe film with thickness of 200 nm and rate deposition of 0.3 nm.s -1 prepared under high vacuum using thermal co-evaporation technique on its some structural and electrical properties was reported. The X- ray analysis showed that all samples are polycrystalline and have the cubic zinc blend structure with preferential orientation in the [111] direction. Films doping with impurity percentages (2, 3, and 4) %Ag lead to a significant increase in the carrier concentration, so it is found to change from 23.493 108 cm -3 to 59.297 108 cm -3 for pure and doped CdTe thin films with 4%Ag respectively. But films doping with impurity percentages above lead to a significant decrease in the electrica
... Show MoreIn this work, InSe thin films were deposited on glass substrates by thermal evaporation technique with a deposit rate of (2.5∓0.2) nm/sec. The thickness of the films was around (300∓10) nm, and the thin films were annealed at (100, 200 and 300)°C. The structural, morphology, and optical properties of Indium selenide thin films were studied using X-ray diffraction, Scanning Electron Microscope and UV–Visible spectrometry respectively. X-ray diffraction analyses showed that the as deposited thin films have amorphous structures. At annealing temperature of 100°C and 200°C, the films show enhanced crystalline nature, but at 300°C the film shows a polycrystalline structure with Rhombohedral phas