This research has presented a solution to the problem faced by alloys: the corrosion problem, by reducing corrosion and enhancing protection by using an inhibitor (Schiff base). The inhibitor (Schiff base) was synthesized by reacting of the substrates materials (4-dimethylaminobenzaldehyde and 4-aminoantipyrine). It was diagnosed by infrared technology IR, where the IR spectrum and through the visible beams proved that the Schiff base was well formed and with high purity. The corrosion behavior of carbon steel and stainless steel in a saline medium (artificial seawater 3.5%NaCl) before and after using the inhibitor at four temperatures: 20, 30, 40, and 50 C° was studied by using three electrodes potentiostat. The corrosion behavior was studied by cathode and anode polarization through which all corrosion parameters were investigated which include: corrosion current icorr (1341× 10-7- 5393 × 10-9A/cm2), corrosion potential Ecorr (-1.031- -0.227 mV vs SCE) , corrosion rates CR (0.658-0.007 mm.y-1), inhibition efficiency %IE (92-98%), and energy activation barriers Ea (4.709-26.733 kJ/mole). The thermodynamic and kinetic properties of the corrosion behavior of these two metals under study, which include: enthalpy ∆H*(2.153-24.176 kJ/mole), entropy ∆S*(-197 -156 J/mole), and free Gibbs energy ∆G*(59.87-74.56 kJ/mole) before and after using the inhibitor, were also studied.
This study is concerned with the effect of Deep Cryogenic Treatment (DCT) at liquid nitrogen temperature (-196 o C) on the mechanical properties and performance of low carbon steel (A858). The tests specimens were divided in to two groups, the first group was subjected to the conventional heat treatment of normalizing, and the second group was also normalized then subjected to (DCT). The results have shown that after (DCT), the Hardness, Tensile properties and the impact energy absorbed were all slightly increased. However the fatigue test showed some positive improvement in fatigue limit by 20(N/mm2 ), and the volume wear rates at different loads were significantly decreased after (DCT). The changes in microstructure due to (DCT) were c
... Show MoreLow- and medium-carbon structural steel components face random vibration and dynamic loads (like earthquakes) in many applications. Thus a modification to improve their mechanical properties, essentially damping properties, is required. The present study focuses on improving and developing these properties, significantly dampening properties, without losing the other mechanical properties. The specimens used in the present study are structural steel ribbed bar ISO 6935 subjected to heating temperatures of (850, 950, and 1050) ˚C, and cooling schemes of annealing, normalizing, sand, and quenching was selected. The damping properties of the specimens were measured experimentally with the area under the curve for the loadi
... Show MoreRemoval of heavy metal ions such as, cadmium ion (Cd 2+) and lead ion (Pb 2+) from aqueous solution onto Eichhornia (water hyacinth) activated carbon (EAC) by physiochemical activation with potassium hydroxide (KOH) and carbon dioxide (CO2) as the activating agents were investigated. The Eichhornia activated carbon was characterized by Brunauer Emmett Teller (BET), Fourier Transform Infrared spectroscopy (FTIR), and Scanning Electron Microscopy (SEM) techniques. Whereas, the effect of adsorbent dosage, contact time of pH, and metal ion concentration on the adsorption process have been investigated using the batch process t
The importance of the present work falls on the pitting corrosion behavior investigation of 304 SS and 316 SS alloys in 3.5 wt% of aqueous solution bearing with chloride and bromide anion at different solutions temperature range starting from (20-50)oC due to the pitting corrosion tremendous effect on the economic, safety and materials loss due to leakage. The impact of solution temperatures on the pitting corrosion resistance at 3.5wt% (NaCl and NaBr) solutions for the 304 SS and 316 SS has been investigated utilizing the cyclic polarization techniques at the potential range -400 to1000 mV vs. SCE at 40 mV/sec scan rate followed by the surface characterization employing Scanning Electron&nbs
... Show MoreA new furfural Schiff base derivative ligand (L-FSB) named N-(4- Bromo-2-methylphenyl)-1-(furan-2-yl)methanimine, was synthesized from the condensation reaction of furfural (fur) with 4-Bromo-2- methylaniline (bma) in 1:1molar ratio. A new series of VO(II), Cr(III), Mn(II), Co(II), Ni(II), Cu(II), Zn(II), and Cd(II) metal complexes are synthesized according to the metal content analysis in an 2:1 ligand:metal ratio. The stereochemistry of the ligand complexes have been deduced by Fourier Transform-Infra Red (FT-IR), Atomic Adsorption (A.A), Ultra violate-Visible Spectra (UV-Vis Spectra), (Mass Spectra, Proton,13Carbon-Nuclear Magnetic Resonance) (1H-NMR,13CNMR) for ligand), magnetic susceptibility at 25oC and conductivity measurements. Fr
... Show MoreBackground: Due to the variations in tooth anatomy and size among different populations, this study aimed to compare the mesiodistal width of primary second molars in Iraqi children with the mesiodistal width of stainless-steel crowns from different companies. Materials and Methods: This cross-sectional study was conducted on 220 intact maxillary and mandibular primary second molars selected from boys and girls’ Iraqi children aged 8-9 years collected from different primary schools in Baghdad city. The mesiodistal dimensions of the selected teeth and the available maxillary and mandibular stainless-steel crowns from three different companies were measured by using a 3-D scanner, and then the whole measurements were calculated usin
... Show MoreThe aim of this study was to evaluate tensile properties of low and medium carbon ferrite -martensite dual phase steel, and the effect cryogenic treatment at liquid nitrogen temperature (-196 ºC) on its properties. Low carbon steel (C12D) and medium carbon steels (C32D & C42D) were used in this work. For each steel grade, five groups of specimens were prepared according to the type of heat treatment. The first group was normalized, the second group was normalized and subsequently subjected to cryogenic treatment then tempered at (200 ºC) for one hour, the third group was quenched from intercritical annealing temperature of (760 ºC) to obtain dual phase (DP) steel, the fourth and fifth groups were both quenched from (760 ºC), but
... Show More