Biogenic gold nanoparticles (AuNPs) were synthesized using broccoli extract to assess their antioxidant activity, wound-healing potential, and selective anticancer effects. Green synthesis with broccoli offers an environmentally friendly way to produce stable and biocompatible nanomaterials. In this study, Brassica oleracea aqueous extract served as both the reducing and capping agent, producing AuNPs with a characteristic surface plasmon resonance peak at 560 nm and a well-defined cubic crystalline structure confirmed by XRD. TEM analysis showed uniformly dispersed, semi-spherical nanoparticles with an average size of 7.5 ± 3.6 nm. The biosynthesized AuNPs exhibited potent antioxidant activity, achieving 91.2 % DPPH scavenging at 100 µg/mL. In vivo tests demonstrated significantly faster wound healing, with approximately 90 % contraction by day 7 compared to 60 % in the control group, supported by histological evidence of increased collagen deposition and complete epithelialization. Moreover, AuNPs showed selective cytotoxicity towards HepG2 cancer cells (IC50 = 53.45 µg/mL) while maintaining over 70 % viability in normal HDF cells. This selectivity likely stems from differences in redox balance and mitochondrial vulnerability between cancer and healthy cells. Overall, the study presents broccoli-mediated AuNPs as multifunctional nanomaterials with potent antioxidant, regenerative, and targeted anticancer properties, highlighting their promising potential in biomedical applications.
Abstract In the current contribution, a novel binuclear nickel(II) and zinc(II) complexes were prepared from a hexadentate ligand prepared via condensation of 3,3'-Bipyridine-6,6'-dicarbaldehyde , 2-amino-5-chlorobenzaldehyde and 2-Aminophenol .The symmetric ligand (H2DTPE) and its metal complexes were illustrated utilizing various techniques of physicochemical containing magnetic moment, analytical analysis and spectroscopy of mass, IR, 13C and 1H NMR, TGA and UV-Vis. The particles of MO Nanoscale were created from the labeled complex applying the ways of pyrolysis and utilizing methods of XRD, FT-IR, and FE-SEM, that specified close compatibility with the typical pattern for nanoparticles of NiO, ZnO and appeared the reasonable size in
... Show MoreAbstract
Nano-crystalline ZSM-5 zeolite was synthesized by hydrothermal method using chelating agent and two gel compositions:Compositionɪ:Al2O3:86SiO2:5.5TPA:12.7Na2O:3.4Trien:3320H2O.Compositionɪɪ:Al2O3:68SiO2:5.4TPA:10Na2O:2.6Trien:2626H2O.Study of hydrothermal reaction factors on characteristics of nano- sized zsm-5 has been carried on ,among them are crystallization temperature, crystallization time and concentration of template ( TPAOH ) solution. Synthesis was accomplished in PTFE lined autoclave ( reactor ) . The product were characterized by X-ray diffraction ( XRD ),Atomic force microsc
... Show MoreBackground: Low-level laser therapy (LLLT) has been extensively applied to improve wound healing due to some biostimulatory properties presented by laser arrays apparently able to accelerate the repair of soft tissue injuries. However, the role of proinflammatory interlukines not been studied yet. IL_1 ? represent one of the most important poroinflammatory interlukines that involved in wound healing. The goal of this study was to investigate the effect of 790-805nm diode laser on the expression of IL_1 ? during wound healing in mice. Materials and Methods: Standard-sized wounds (1.5cm) were carried out in the face of 96 white albino mice. Half of them underwent LLLT treatment (360 J/cm 2) at 790-805 nm delivered immediately after wound pro
... Show MoreIn this article the nanoparticles synthesis of ZnO (Nps) by using the precipitation method at concentrations range (0.5, 0.25, 0.125, 0.0625, 0.03125) mg/mL and then activity was examined against Streptococcus spp that causing dental caries in vitro by well diffusion method, find these concentrations effected in these bacteria and better concentration is 0.03125. ZnO Nps were characterization by EDS to prove this particles are ZnO, and also characterized by atomic force microscope (AFM), X-ray Diffraction (XRD) and TEM, from these technic found that the average size about 30.52 nm and hexagonal shape. The UV-visible result reveals that the large band is observed at 340.8 nm, Zeta potential show that the surface charge is 30.19 mv an
... Show MoreBackground: A great dental and biomedical interest had been paid to silver nanoparticles because of their antimicrobial activity. Objective: To evaluate the antimicrobial and cytotoxic activity of a newly developed Nano-silver fluoride that was synthesized from moringa oleifera leaf extract against S. mutants. Material and method: The green synthesis method was used to prepare Nano-silver fluoride from moringa oleifera leaf extract. The minimum inhibitory concentration and the minimum bactericidal concentration were evaluated using brain heart infusion plates, while the cytotoxicity was evaluated by the hemolytic activity. Results: Nano-silver fluoride had a bactericidal and bacteriostatic effect (MIC was 60 ppm a
... Show MoreIn this work, the antibacterial effectiveness of face masks made from polypropylene, against Candida albicans and Pseudomonas aeruginosa pathogenic was improved by soaking in gold nanoparticles suspension prepared by a one-step precipitation method. The fabricated nanoparticles at different concentrations were characterized by UV-visible absorption and showed a broad surface Plasmon band at around 520 nm. The FE-SEM images showed the polypropylene fibres highly attached with the spherical AuNPs of diameters around 25 nm over the surfaces of the soaked fibres. The Fourier Transform Infrared Spectroscopy (FTIR) of pure and treated face masks in AuNPs conform to the characteristics bands for the polypropylene bands. There are some differences
... Show MoreIn the present study, gold nanoparticles (AuNPs) were prepared using a simple low cost method synthesized cold plasma at different exposure time . The nanoparticles were characterized using UV-Visible spectra, X-ray diffraction (XRD). The prepared AuNPs showed surface Plasmon resonance centered at 530, 540,and 533 nm. The XRD pattern showed that the strong intense peaks indicate crystalline nature and face centered cubic structure of gold nanoparticles for all samples were prepared .The average crystallite size of the AuNPs was 20-40 nm. Morphology of the AuNPs were carried out using FESEM. Observations show that the AuNPs synthesized we well dispersed with and particle sizes ranging from 9 to 31 nm with spherical shapes which are cle
... Show More