Biogenic gold nanoparticles (AuNPs) were synthesized using broccoli extract to assess their antioxidant activity, wound-healing potential, and selective anticancer effects. Green synthesis with broccoli offers an environmentally friendly way to produce stable and biocompatible nanomaterials. In this study, Brassica oleracea aqueous extract served as both the reducing and capping agent, producing AuNPs with a characteristic surface plasmon resonance peak at 560 nm and a well-defined cubic crystalline structure confirmed by XRD. TEM analysis showed uniformly dispersed, semi-spherical nanoparticles with an average size of 7.5 ± 3.6 nm. The biosynthesized AuNPs exhibited potent antioxidant activity, achieving 91.2 % DPPH scavenging at 100 µg/mL. In vivo tests demonstrated significantly faster wound healing, with approximately 90 % contraction by day 7 compared to 60 % in the control group, supported by histological evidence of increased collagen deposition and complete epithelialization. Moreover, AuNPs showed selective cytotoxicity towards HepG2 cancer cells (IC50 = 53.45 µg/mL) while maintaining over 70 % viability in normal HDF cells. This selectivity likely stems from differences in redox balance and mitochondrial vulnerability between cancer and healthy cells. Overall, the study presents broccoli-mediated AuNPs as multifunctional nanomaterials with potent antioxidant, regenerative, and targeted anticancer properties, highlighting their promising potential in biomedical applications.
A Schiff base ligand (L) was synthesized via condensation of N-( 1-naphthyl) ethylenediamine dihydrochloride with phthalaldehyde. The ligand was characterized by FT-IR, UV–Vis, 1H NMR, mass spectrometry, and elemental analysis (C, H, N). Five metal complexes (Co(II), Ni(II), Cu(II), Zn(II), and Cd(II)) were prepared with the ligand in a 1:1 (M:L) ratio using an aqueous ethanol solution. The complexes were characterized by FT-IR, UV–Vis, mass spectrometry, and elemental analysis (C, H, N). Additionally, 1H NMR spectroscopy was employed for Cd(II) complex. Antimicrobial activity of the ligand and its metal complexes against pathogenic bacteria (K. pneumoniae, E. coli, S. aureus, and S. epidermidis) and fungus (C. albicans) were evaluated
... Show MoreA Schiff base ligand (L) was synthesized via condensation of
A Schiff base ligand (L) was synthesized via condensation of
Abstract In the current contribution, a novel binuclear nickel(II) and zinc(II) complexes were prepared from a hexadentate ligand prepared via condensation of 3,3'-Bipyridine-6,6'-dicarbaldehyde , 2-amino-5-chlorobenzaldehyde and 2-Aminophenol .The symmetric ligand (H2DTPE) and its metal complexes were illustrated utilizing various techniques of physicochemical containing magnetic moment, analytical analysis and spectroscopy of mass, IR, 13C and 1H NMR, TGA and UV-Vis. The particles of MO Nanoscale were created from the labeled complex applying the ways of pyrolysis and utilizing methods of XRD, FT-IR, and FE-SEM, that specified close compatibility with the typical pattern for nanoparticles of NiO, ZnO and appeared the reasonable size in
... Show MoreMany attempts have been made to modify the surface of orthodontic micro-implants and prevent the development of microbes by coating them with antimicrobial nanoparticles (NPs). The purpose of the present study was to evaluate the cytotoxicity of different NPs, namely, TiO2 and zinc oxide (ZnO) NPs, that are used to coat titanium orthodontic micro-implants.
Thirty orthodontic micro-implants were included in this study. Those were divided into three groups: control group without coating, TiO2-coated orthodontic micro-implants, and TiO2- and ZnO-coated orthodontic micro-implants. Scann
In this article the nanoparticles synthesis of ZnO (Nps) by using the precipitation method at concentrations range (0.5, 0.25, 0.125, 0.0625, 0.03125) mg/mL and then activity was examined against Streptococcus spp that causing dental caries in vitro by well diffusion method, find these concentrations effected in these bacteria and better concentration is 0.03125. ZnO Nps were characterization by EDS to prove this particles are ZnO, and also characterized by atomic force microscope (AFM), X-ray Diffraction (XRD) and TEM, from these technic found that the average size about 30.52 nm and hexagonal shape. The UV-visible result reveals that the large band is observed at 340.8 nm, Zeta potential show that the surface charge is 30.19 mv an
... Show MoreThe size and the concentration of the gold nanoparticles (GNPs)
synthesized in double distilled deionized water (DDDW) have been
found to be affected by the laser energy and the number of pulses.
The absorption spectra of the nanoparticles DDDW, and the
surface plasmon resonance (SPR) peaks were measured, and found to
be located between (509 and 524)nm using the UV- Vis
spectrophotometer. SPR calculations, images of transmission
electron microscope, and dynamic light scattering (DLS) method
were used to determine the size of GNPs, which found to be ranged
between (3.5 and 27) nm. The concentrations of GNPs in colloidal
solutions found to be ranged between (37 and 142) ppm, and
measured by atomic absorptio
Alot of medical and industrial applications used the metal nanoparticles (NPs) with increase interest to be used as cancer therapy. The current work aimed to prepare AuNPs and AgNPs through the use of plasma jet and test their antitumor mechanism of apoptosis induction. The results indicating the face-centered cubic structures and crystalline nature of AuNPs and AgNPs. Also, the image of FESEM showed that the well dispersions regarding AuNPs and AgNPs, while the NP’s spherical shape with the particle size distributions which are considered to be close that estimated from the XRD. cytotoxicity have been assessed against the Normal embryonic cell line REF and the digestive system (HC , SK-GT-4) cell lines under a variety of the seri
... Show MoreIn this study, gold nanoparticles (AuNPs) were synthesized using a plasma jet system at different exposure times. Using ultraviolet, visible spectra, X-ray diffraction, the nanoparticles were characterized (XRD). A Plasmon surface resonance concentrated at 530, 540, and 533 nm for the prepared AuNPs. The pattern of XRD showed that the extreme peaks of the film reflect crystalline existence. The face-centered cubic structure of the gold nanoparticles was prepared for all samples, with an average crystallite size of 25-40 nm. The effect of AuNPs in vivo on liver function levels was measured. For all doses, we notice an increase in the ranks of liver function in the blood during the period of dosing, and it begins to decrease when the dosi