Preferred Language
Articles
/
mIairYYBIXToZYALh6Mv
Structural Behavior of Axially Loaded Composite Concrete-steel Plate Shear Walls
...Show More Authors

Scopus Clarivate Crossref
Publication Date
Thu Oct 01 2015
Journal Name
Journal Of Engineering
Strength Enhancement of Prestressed Concrete Dapped-End Girders
...Show More Authors

This paper presents the application of nonlinear finite element models in the analysis of dapped-ends pre-stressed reinforced concrete girders under static loading by using ANSYS software. The girder dimensions are (4.90 m span, 0.40 m depth, 0.20 m width, 0.20 m nib depth, and 0.10 m nib length) and the parameters considered in this research are the pre-stress effect, and strand profile (straight and draped).

    The numerical results are compared with the experimental results of the same girders. The comparisons are carried out in terms of initial prestress effect, load- deflection curve, and failure load. Good agreement was obtained between the analytical and experimental results. Even that, the

... Show More
View Publication Preview PDF
Publication Date
Sun Jan 01 2012
Journal Name
7th Rilem International Conference On Cracking In Pavements
Mechanistic Evaluation of Lime-Modified Asphalt Concrete Mixtures
...Show More Authors

Frequently, Load associated mode of failure (rutting and fatigue) as well as, occasionally, moisture damage in some sections poorly drained are the main failure types found in some of the newly constructed road within Baghdad as well as other cities in Iraq. The use of hydrated lime in pavement construction could be one of the possible steps taken in the direction of improving pavement performance and meeting the required standards. In this study, the mechanistic properties of asphalt concrete mixes modified with hydrated lime as a partial replacement of limestone dust mineral filler were evaluated. Seven replacement rates were used; 0, 0.5, 1, 1.5, 2, 2.5 and 3 percent by weight of aggregate. Asphalt concrete mixes were prepared at their

... Show More
View Publication
Crossref (9)
Crossref
Publication Date
Thu Dec 03 2020
Journal Name
Civileng
Evaluation of Concrete Material Properties at Early Age
...Show More Authors

This article investigates the development of the following material properties of concrete with time: compressive strength, tensile strength, modulus of elasticity, and fracture energy. These properties were determined at seven different hydration ages (18 h, 30 h, 48 h, 72 h, 7 days, 14 days, 28 days) for four pure cement concrete mixes totaling 336 specimens tested throughout the study. Experimental data obtained were used to assess the relationship of the above properties with the concrete compressive strength and how these relationships are affected with age. Further, this study investigates prediction models available in literature and recommendations are made for models that are found suitable for application to early age conc

... Show More
View Publication
Crossref (15)
Crossref
Publication Date
Thu Dec 01 2011
Journal Name
Journal Of Engineering
MECHANISTIC EVALUATION OF LIME-MODIFIED ASPHALT CONCRETE MIXTURES
...Show More Authors

Frequently, Load associated mode of failure (rutting and fatigue) as well as, occasionally, moisture damage in some sections poorly drained are the main failure types found in some of the newly constructed road within Baghdad as well as other cities in Iraq. The use of hydrated lime in pavement construction could be one of the possible steps taken in the direction of improving pavement performance and meeting the required standards. In this study, the mechanistic properties of asphalt concrete mixes modified with hydrated lime as a partial replacement of limestone dust mineral filler were evaluated. Seven replacement rates were used; 0,0.5, 1, 1.5, 2, 2.5 and 3 percent by weight of aggregate. Asphalt concrete mixes were prepared at their

... Show More
View Publication Preview PDF
Crossref
Publication Date
Thu Jun 08 2023
Journal Name
Open Engineering
A review of rutting in asphalt concrete pavement
...Show More Authors

Undoubtedly, rutting in asphalt concrete pavement is considered a major dilemma in terms of pavement performance and safety faced by road users as well as the road authorities. Rutting is a bowl-shaped depression in the wheel paths that develop gradually with the increasing number of load applications. Heavy axle loadings besides the high pavement summer temperature enhance the problem of rutting. According to the AASHTO design equation for flexible pavements, a 1.1 in rut depth will reduce the present serviceability index of relatively new pavement, having no other distress, from 4.2 to 2.5. With this amount of drop in serviceability, the entire life of the pavement in effect has been lost. Therefore, it is crucial to look at the mechani

... Show More
View Publication
Scopus (24)
Crossref (20)
Scopus Clarivate Crossref
Publication Date
Sat Oct 01 2022
Journal Name
Journal Of Applied Geophysics
Predicting dynamic shear wave slowness from well logs using machine learning methods in the Mishrif Reservoir, Iraq
...Show More Authors

Crossref (8)
Crossref
Publication Date
Sat Oct 01 2022
Journal Name
Journal Of Applied Geophysics
Predicting dynamic shear wave slowness from well logs using machine learning methods in the Mishrif Reservoir, Iraq
...Show More Authors

View Publication
Scopus (12)
Crossref (8)
Scopus Clarivate Crossref
Publication Date
Mon Jul 01 2019
Journal Name
Journal Of Physics: Conference Series
Effect of Nickel Substitution On Structural and Electrical Properties of Hg<sub>0.5</sub>Pb<sub>0.5</sub>Ba<sub>2</sub>Ca<sub>2</sub>Cu<sub>3-y</sub>Ni<sub>y</sub>O<sub>8+δ</sub> Superconductor Composite
...Show More Authors
Abstract<p>six specimens of the Hg<sub>0.5</sub>Pb<sub>0.5</sub>Ba<sub>2</sub>Ca<sub>2</sub>Cu<sub>3-y</sub> <italic>Ni<sub>y</sub> </italic>O<sub>8+δ</sub> (y=0.2,0.4,0.6,0.8,1.0) superconducting compound were prepared by solid state reaction method, with sintering temperature equal to 1123K for 24 hours. The electrical resistivity was examined by the four probe technique, It was found that all the specimens have metallic behavior and increasing the critical temperature with increasing nickel concentration. The optimum critical temperature T<sub>c</sub> was found equal </p> ... Show More
View Publication
Scopus (4)
Crossref (3)
Scopus Clarivate Crossref
Publication Date
Wed May 31 2017
Journal Name
Al-khwarizmi Engineering Journal
Corrosion control of Buried Low Carbon Steel Structure by Using Alteration Medias method
...Show More Authors


Abstract

The aim of the present work is to control of metal buried corrosion by alteration the media method. This method depended on the characteristics of each media. The corrosion rates in different media (soil, sand, porcelanite stone and gravel) for specimens of low carbon steel were measured by two methods weight loss method and polarization method, weight loss measured by buried specimens in these medias separately for 90 days. The polarization method includes preparing of specimen and salt solutions have electrical resistivity equivalent electrical resistivity of these media. The corrosion rate of two method results in (soil > sand> porcelainte stone> gravel). The lower corrosion rate happene

... Show More
View Publication Preview PDF
Publication Date
Mon Dec 30 2013
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
Corrosion Inhibition of Galvanic Couple Copper Alloy/Mild Steel in Cooling Water System
...Show More Authors

The driving idea for the present work was to combine the effect of polyvinyl alcohol (PVA) as corrosion inhibitor with the distance between the anodic and cathodic elements of the galvanic cell, beside their area ratio, in scope of synergistic suppression of galvanic corrosion on Cu/Fe model couple, using weight loss method. The performance affecting galvanic corrosion process has been tested for three major factors affect the process:
1. Four PVA inhibitor concentrations were selected to be (0, 1000, 4000 and 7000 ppm) in simulated cooling water.
2. Two cathode: anode area ratios as 1:1 and 2.4:1.
3. Two distances apart cathode – anode as 3 and 7 cm.
Maximum corrosion inhibition achieved was 86% which indicates that increa

... Show More
View Publication Preview PDF