Background: Diabetes mellitus a major factor that has adverse effects on the vascular system and the heart. It causes an increase in cardiac muscle thickness, resulting in decreased compliance and increased peripheral arterial stiffness. This study aims to assess the left ventricular mass (LVM) and left ventricular hemodynamic changes in diabetic patients measured by Doppler echocardiography. Patients and Methods: The study included 50 diabetic patients ranging in age between 25 and 80 years, (mean age: 54.1 ± 15.10, 19 males, 31 females) and 50 healthy subjects, aged 25 to 80 years (mean age: 48.52 ± 14.45, 11 males, 39 females). Doppler echocardiography was used to assess left ventricular function. The measurements included posterior wall thickness at diastole (PWTd), interventricular septum thickness at diastole (IVSTd), left ventricular diameter at the end of diastole (LVIDd), left ventricular diameter at the end of systole (LVIDs), peak velocity at atrial contraction (A), early peak velocity (E), left ventricular ejection fraction (LVEF%), left ventricular mass (LVM), and relative wall thickness (RWT). Results: The data showed that changes in E/A differences between diabetic patients and controls for age ranges 25 to 50 and 60 to 80 years were -24.60% and -31.93% (p < 0.05). There were non-significant differences in the LVIDd/LVIDs ratio between diabetic patients and controls for both age groups: 1.31% and 6.25%, respectively. For 25- to 50-year olds, the changes in RWT and LVM were 50% and 74.43%, respectively (p < 0.05), while the differences in RWT and LVM for 60- to 80-year olds were 48.71% and 70.06%, respectively (p < 0.05). Conclusion: The results indicate that diastolic dysfunction may be higher in diabetic patients compared to healthy subjects, which may be due to adverse influence of diabetes on cardiac muscle. These changes in left ventricular structure may include LV hypertrophy, increase in stiffness, and reduction in compliance, with increase in left ventricular mass, relative wall thickness, posterior wall thickness at diastole, and interventricular septum thickness at diastole.
Background: The world is in front of two emerging problems being scarceness of virgin re-sources for bioactive materials and the gathering of waste production. Employment of the surplus waste in the mainstream production can resolve these problems. The current study aimed to prepare and characterize a natural composite CaO-SiO2 based bioactive material derived from naturally sustained raw materials. Then deposit this innovative novel bioactive coating composite materials overlying Yttria-stabilized tetragonal zirconia substrate. Mate-rials and method; Hen eggshell-derived calcium carbonate and rice husk-derived silica were extracted from natural resources to prepare the composite coating material. The manufac-tured powder was characterized
... Show MoreIn the present investigation, new polymers of Poly [ N - acryl - N - sulfonic acid - N\ yL - 2 - substitute - 4 - oxo - thiazolidine ] Maleic and Succinic diimide were synthesized by seven steps; first step includes esterification of different cyclic anhydride, using one mole of absolute methanol in the presence few drops of conc. H2SO4, yielded mono group ester [I] , which was reaction with thionyl chloride to give ester acid chloride [II] .Then reacted with sulfanilic acid to product compound [III] , which was condensation with hydrazine hydrate to give acid hydrazide [IV] . The new different Schiff bases [V-VIII] were synthesized by reaction of acid hydraizide with different (aliphatic and aromatic) aldehyedes and ketones in the prese
... Show MoreIn the midst of rapid changes and difficultiesand the tough competition faced by the Iraqi banks, it has become necessary to focus on a significant aspect of administrative work; that is strategic planning and the key role of implementation within this process in improving the banking service quality. It has emerged as a critical and main competitive weapon for distinguishing the services provided by banks from each other in an effort to participate in increasing market share of the bank in question in question; in its growth, continuation and profit increase.
The research has addressed the relation between the independent variable (implementation within strategic planning), and the dependent variable (banking service quality and
... Show MoreThe Manganese doped zinc sulfide nanoparticles of the cubic zinc blende structure with the average crystallite size of about 3.56 nm were synthesized using a coprecipitation method using Thioglycolic Acid as an external capping agent for surface modification. The ZnS:Mn2+ nanoparticles of diameter 3.56 nm were manufactured through using inexpensive precursors in an efficient and eco-friendly way. X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM) and Fourier Transform Infrared (FTIR) spectroscopy are used to examine the structure, morphology and chemical composition of the nanoparticles. The antimicrobial activity of (ZnS:Mn2+) nanocrystals was investigated by measuring the diameter of inhibition zone using well diffusion mechanism
... Show MoreNovel derivatives of 1-(´1, ´3, ´4, ´6-tetra benzoyl-β-D-fructofuranosyl)-1H- benzotriazole and 1-(´1, ´3, ´4, ´6-tetra benzoyl-β-D-fructofuranosyl)-1H- benzotriazole carrying Schiff bases moiety were synthesised and fully characterised. The protection of D- fructose using benzoyl chloride was synthesized, followed by nucleophilic addition/elimination between benzotria- zole and chloroacetyl chloride to give 1-(1- chloroacetyl)- 1H-benzotriazole. The next step was condensation reaction of protected fructose and 1-(1-chloroacetyl)-1H- benzotriazole producing a new nucleoside analogue. The novel nucleoside analogues underwent a second conden- sation reaction with different aromatic and aliphatic amines to provide new Schiff b
... Show MorePure and Fe-doped zinc oxide nanocrystalline films were prepared
via a sol–gel method using -
C for 2 h.
The thin films were prepared and characterized by X-ray diffraction
(XRD), atomic force microscopy (AFM), field emission scanning
electron microscopy (FE-SEM) and UV- visible spectroscopy. The
XRD results showed that ZnO has hexagonal wurtzite structure and
the Fe ions were well incorporated into the ZnO structure. As the Fe
level increased from 2 wt% to 8 wt%, the crystallite size reduced in
comparison with the pure ZnO. The transmittance spectra were then
recorded at wavelengths ranging from 300 nm to 1000 nm. The
optical band gap energy of spin-coated films also decreased as Fe
doping concentra