The electrical properties of pure NiO and NiO:Ag films which are deposited on glass substrate with various dopant concentrations (1wt%, 2wt%, 3wt% and 4wt%) at room temperature and 450 °C annealing temperature will be presented. Further, the structural properties were investigated by X-ray diffraction and the surface morphology of the deposited samples was examined by SEM. The results of the Hall effect showed that all the films were p-type. Hall mobility decreases while both carrier concentration and conductivity increase with the increasing of annealing temperatures and doping percentage, Thus, the behavior of semiconductor, and also the DC conductivity from which the activation energy decreases with the doping concentration increase and transport mechanism of the charge carriers can be estimated.
In this work, the effect of annealing temperature on the electrical properties are studied of p-Se/ n-Si solar cell, which p-Se are deposit by DC planar magnetron sputtering technique on crystal silicon. The chamber was pumped down to 2×10−5 mbar before admitting the gas in. The gas was Ar. The sputtering pressure varied within the range of 4x10-1 - 8x10-2mbar by adjusting the pumping speed through the opening control of throttle valve. The electrical properties are included the C-V and I-V measurements. From C-V measurements, the Vbi are calculated while from I-V measurements, the efficiency of solar cell is calculated.
In this research, the effect of each of the concentrations ( Nd+3) was studied (N) the thickness of the thin disk (d) the number of times that the pumping beam passes through the effective medium of this laser (Mp) the reflectivity of the laser output mirror (R 2) The losses of the effective medium (L) and the pumping power used in achieving the reverse qualification (PP) on each of the pumping threshold capacities (Pp.th) and the output power of the laser (Pout) and the efficiency (ŋ) in Nd3+ thin-disk lasers (TDLs) pumping quasi-three-level With continuous operation (cw), at room temperature, and in the Gaussian mode (TEM00),
We found under these opera
... Show MoreIndium Antimonide (InSb) thin films were grown onto well cleaned glass substrates at substrate temperatures (473 K) by flash evaporation. X-ray diffraction studies confirm the polycrystalline of the films and the films show preferential orientation along the (111) plane .The particle size increases with the increase of annealing time .The transmission spectra of prepared samples were found to be in the range (400-5000 cm-1 ) from FTIR study . This indicates that the crystallinity is improved in the films deposited at higher annealing time.
This work aim to prepare Ag/R6G/PMMA nanocomposite thin
films by In-situ plasma polymerization and study the changes in the
optical properties of fluorophore due to the presence of Ag
nanoparticles structures in the vicinity of the R6G laser dye. The
concentrations of R6G dye/MMA used are: 10-4M solutions were
prepared by dissolving the required quantity of the R6G dye in
MMAMonomer. Then Silver nanoparticles with 50 average particles
size were mixed with MMAmonomer with concentration of 0.3, 0.5,
0.7wt% to get R6G silver/MMA in liquid phase. The films were
deposited on glass substrates by dielectric barrier discharge plasma
jet. The Ag/R6G/PMMA nanocomposite thin films were
characterization by UV-Visible
In this work, the spectra for plasma glow produced by pulse
Nd:YAG laser (λ=532 and 1064nm) on Ag:Al alloy with same molar
ratio samples in distilled water were analyzed by studying the atomic
lines compared with aluminum and silver strong standard lines. The
effect of laser energies of the range 300 to 800 mJ on spectral lines,
produced by laser ablation, were investigated using optical
spectroscopy. The electron temperature was found to be increased
from 1.698 to 1.899 eV, while the electron density decreased from
2.247×1015 to 5.08×1014 cm-3 with increasing laser energy from 300
to 800 mJ with wavelength of 1064 nm. The values of electron
temperature using second harmonic frequency are greater than of<
This contribution investigates the impact of adding transition metal of Ti to CeOy samples at various concentrations referring to 0, 15.84, 24.46, 34.46, 36.23, 38.46, 45.38% and pure TiOy, correspondingly. The samples were fabricated by the magnetron sputtering technique. X-ray diffraction (XRD) configurations demonstrate the presence of α-Ce2O3 and Ce2O3 phases with increased Ti contents in the systems. X-ray photoelectron spectroscopy (XPS) experimentation confirms the purity of the S1-sample (CeO2) and the purity of the S8-sample (TiO2). Further XPS analysis reveals that Ti incorporation in the doped systems functions as a reducing agent because of the existence of α-Ce2O3 and Ce2O3 phases. Moreover, based on UV–vis spectroscopy res
... Show MoreThis contribution investigates the impact of adding transition metal of Ti to CeOy samples at various concentrations referring to 0, 15.84, 24.46, 34.46, 36.23, 38.46, 45.38% and pure TiOy, correspondingly. The samples were fabricated by the magnetron sputtering technique. X-ray diffraction (XRD) configurations demonstrate the presence of α-Ce2O3 and Ce2O3 phases with increased Ti contents in the systems. X-ray photoelectron spectroscopy (XPS) experimentation confirms the purity of the S1-sample (CeO2) and the purity of the S8-sample (TiO2). Further XPS analysis reveals that Ti incorporation in the doped systems functions as a reducing agent because of the existence of α-Ce2O3 and Ce2O3 phases. Moreover, based on UV–vis spectroscopy res
... Show MoreThe Sr doped La1Ba1-xSrx Ca2Cu4O8.5+δ samples with 0 ≤ x ≤ 0.3 had been prepared using the solid state reaction. The samples were claimed at 800°C for 3hr, palletized and sintered at 860°C for 20hr in air . Dielectric constant and loss by means of capacitance have been investigated with frequencies in the range of 1kHZ to 1MHZ for our samples at room temperature. Also, Shore hardness has been measured. The dielectric constant and loss decrease slightly with the increase of frequency for all compounds. Additionally, the partial substitution of Sr+2 into Ba+2 sites never have effect on the dielectric properties. X-ray diffraction (XRD) analysis showed a tetragonal structure and the
... Show MoreCadmium sulphide CdS films with 200 nm have been prepared by thermal evaporation technique on glass substrate at substrate room temperature under vacuum of 10-5mbar.In this paper, the effect of Dielectric Barrier Discharge plasma on the optical properties of the CdS film. The prepared films were exposed to different time intervals (0, 3, 5, 8) min. For every sample, the Absorption A, absorption coefficient α , energy gap Eg ,extinction coefficient K and dielectric constant ε were studied. It is found that the energy gap were decreased with exposure time, and absorption , Absorption coefficient, refractive index, extinction coefficient, dielectric constant increased with time of exposure to the plasma. Our study conside
... Show MoreLiquid – liquid interface reaction is the method for
preparation nanoparticles (NP'S) which depend on the super
saturation of ions that provide by using the system that consist from
toluene and water, the first one is above the second to obtain
nanoparticles (NP's) CdS at the interface separated between these
two immiscible liquid. The structure properties were characterized by
XRD-diffraction and transmission electron microscopy.
The crystalline size estimate from X-ray diffraction pattern
using Scherer equation to be about 7nm,and by TEM analysis give us
that ananosize is about 5 nm which give a strong comparable with
Bohr radius. Photoluminescence analysis give two emission peak,
the first one around