The research Reviews the sides of highlight importance of the Nano-Accounting which doing the accounting performance functions fully computerized without the intervention of an accountant, to solve the problem of not keeping up the rationalization of recording and accounting systems, with the rationalization of production which fully computerized.(be invisible and hidden accounting), resulting by linking or interaction of the accounting, additive production system represented three-dimensional printers, open source and recycling. That which result the rationalizing the facilities of production, organization and self-control which derived nanotechnology idea, which aims to minimize materials and change it properties, then view the advantages , and the mechanism of Nano-accounting and the basic pillars upon which, the rationalized sides of accounting performance which traditionally played by the accountant as traditional accounting cycle as recording journal entries, posting ,balancing ,etc. which required changing the concept of accounting records to accounting notation, working on the development of the accounting from existing the accounting records to a good decisions maker, rationalize the principles and concepts of most the accounting and managerial systems as a result of changing the accounting structure, and removing jamming informatics.by direct contact for all internal and external parties, can illustrate the applications of Nano-Accounting by rationalized accounting performance in the manufacturing as a society of the research, and at the General Company for Electrical Industries / air cooler motor plant as a sample of the search.
The paper include study the effect thickness of the polymeric sample which is manufactured by thermo press way. The sample was used as an active tunable R6G laser media. The remarks show that, when the thickness of the samples is increased, with the same concentration, the spectrum will shift towards the short wavelength, & the quantum fluorescence yield will increased. The best result we obtained for the quantum fluorescence yield is (0.68) at the sample, with thickness (0.304mm) in Ethanol solvent, while when we used the Pure Water as a solvent, we found that the best quantum fluorescence yield is (0.63) at (0.18mm) thickness of the sample.
The main challenge of military tactical communication systems is the accessibility of relevant information on the particular operating environment required for the determination of the waveform's ideal use. The existing propagation model focuses mainly on broadcasting and commercial wireless communication with a highs transceiver antenna that is not suitable for numerous military tactical communication systems. This paper presents a study of the path loss model related to radio propagation profile within the suburban in Kuala Lumpur. The experimental path loss modeling for VHF propagation was collected from various suburban settings for the 30-88 MHz frequency range. This experiment was highly affected by ecological factors and existing
... Show MoreIn the present study waste aluminium cans were recycled and converted to produce alumina catalyst. These cans contain more than 98% aluminum oxide in their structure and were successfully synthesized to produce nano sized gamma alumina under mild conditions. A comprehensive study was carried out in order to examine the effect of several important parameters on maximum yield of alumina that can be produced. These parameters were reactants mole ratios (1.5, 1.5, 2, 3, 4 and 5), sodium hydroxide concentrations (10, 20, 30, 40, 50 and 55%) and weights of aluminum cans (2, 4, 6, 8 and 10 g). The compositions of alumina solution were determined by Atomic absorption spectroscopy (AAS); and maximum yield of alumina solution was 96.3% obtain
... Show MoreThe objective of the study is developing a procedure for production and characterization of rice husk ash (RHA). The effects of rice husk (RH) amount, burning/cooling conditions combined with stirring on producing of RHA with amorphous silica, highest SiO2, lowest loss on ignition (LOI), uniform particle shape distribution and nano structured size have been studied. It is concluded that the best amount is 20 g RH in 125 ml evaporating dish Porcelain with burning for 2 h at temperature 700 °C combined with cooling three times during burning to produce RHA with amorphous silica, SiO2 90.78% and LOI 1.73%. On the other hand, cooling and stirring times affect the variation of nano structured size and particle shape dis
... Show MoreThe Dielectric properties of EP/TiO2 and MgO nanocomposite at
a frequency range of (102-106 Hz) were studied. The composite were
prepared with the state volume ratio (0, 0.05, 0.1) for EP/TiO2 and
MgO respectively. The impedance, dielectric constant and dielectric
loss were found decrease with frequency increase.
Abstract
Nano-crystalline ZSM-5 zeolite was synthesized by hydrothermal method using chelating agent and two gel compositions:Compositionɪ:Al2O3:86SiO2:5.5TPA:12.7Na2O:3.4Trien:3320H2O.Compositionɪɪ:Al2O3:68SiO2:5.4TPA:10Na2O:2.6Trien:2626H2O.Study of hydrothermal reaction factors on characteristics of nano- sized zsm-5 has been carried on ,among them are crystallization temperature, crystallization time and concentration of template ( TPAOH ) solution. Synthesis was accomplished in PTFE lined autoclave ( reactor ) . The product were characterized by X-ray diffraction ( XRD ),Atomic force microsc
... Show Moreِabstract:In this research we prepared nanofibers by electrospinning from poly (Vinyl Alcohol) /TiO2. The spectrum of the solution (Emission) was studied and found to be at 772 nm, several process parameters were such as concentration of TiO2 , and the effect of distance from nozzle tip to the grounded collector (gap distance). The result of the lower concentration of, the smaller the diameter of nanofiber is. Increasing the gap distance will affect nanofibers diameter.
In this research we prepared nanofibers by electrospinning from
poly (Vinyl Alcohol) /TiO2. The spectrum of the solution (Emission)
was studied and found to be at 772 nm, several process parameters
were such as concentration of TiO2 , and the effect of distance from
nozzle tip to the grounded collector (gap distance). The result of the
lower concentration of, the smaller the diameter of nanofiber is.
Increasing the gap distance will affect nanofibers diameter