One-third of the total waste generated in the world is construction and demolition waste. Reducing the life cycle of building materials includes increasing their recycling and reuse by using recycled aggregates. By preventing, the need to open new aggregate quarries and reducing the amount of construction waste dumped into landfills, the use of recycled concrete aggregate in drum compacted concrete protects the environment. Four samples of PRCC were prepared for testing (compressive strength, tensile strength, flexural strength, density, water absorption, porosity) as the reference mix and (10, 15, and 20%) of fine recycled concrete aggregate as a partial replacement for fine natural aggregate by volume. The mix is designed according to (ACI 327-15) with the specified cylinder compressive strength (28 MPa). The results showed a decrease in mechanical properties with an increase in partial replacement compared to the reference mixture and an increase in water absorption and porosity at 28 days. This is because old cement mortar on the surfaces of fine recycled concrete aggregates leads to higher porosity and water absorption than fine natural aggregates. At 90 days, results improved slightly. This is due to the non-aqueous cement in the recycled fine concrete aggregate.
In this work, substantial evidence was obtained for ligand reduction in cerium tetrakis acac complexes. Also, this ligand reduction of a negatively charged ligand proved to depend far less on the nature central metal than neutral ligands does. It is supposed that in Mz(acac)z complexes the charge is distributed evenly over the whole molecule. In this work these complexes were prepared and characterized by IR and CHN analysis to indicate the purities of these complexes. The electrochemistry techniques were shown as obtained for ligand reduction. This research was carried out at School of Chemistry and Molecular Science, Sussex University, U.K.
In this study, a Hydroxyapatite (HA) coating was prepared on a titanium implant by an electrochemical deposition process. The titanium pre-treatment by anodizing in 1.65 mol/L sulfuric acid with (10V) at room temperature. The deposition was all conducted at a constant voltage of 6.0 V, for 1 h at room temperature. The coatings thus prepared were characterized with Fourier transform infrared spectroscopy (FTIR) and thickness of the coated layer.The electrochemical deposition of HA occurred on the titanium as a cathode. Coated titanium by HA after anodizing revealed a good corrosion protection efficiency even at a temperature ranged (293-323) K in artificial saliva. Activation energy and pre-exponential factor (kinetic parameters) were calcul
... Show MoreIn this work, the effect of the addition of bright nickel plating and silver carried out by the electroplating method has been studied, on the coating of copper nanoparticles on the copper base metal via the process of thermal evaporation. The improvement of the solar absorber using CuNP in combination with the bright nickel and silver was obtained to be better than copper nanoparticles individually. A bright nickel enhanced the absorbed thermal stability. Also, other optical properties, absorptions, and emissivity slightly decreased from (93% to 87%), while the existence of silver had a slight impact on absorption of about (86.50%). On the other hand, thermal conductivity was evaluated using hot disk analyzer. The results showed a good
... Show MoreIn this work, diamond-like carbon (DLC) thin films were prepared from Cyclohexane. Thin films were deposited on quartz substrate by atmospheric pressure Argon plasma jet system. The plasma jet system was applying high voltage sinusoidal waves of frequency 28 kHz and potential difference of 7.5kV peak to peak across the electrodes. The effect of annealing at 400, 500 and 600 °C under vacuum for two hours on optical properties and structural properties of the DLC thin films were investigated. This effect was clarified by X-ray diffraction (XRD), FTIR, UV-Visible absorption, Scanning Electron Microscopy (SEM) and Raman Spectroscopy. The X-ray diffraction patterns for the annealing DLC thin films show two broad peaks at 2θ, 26.62° and 51.58
... Show MoreHydatid disease is a zoonotic infection caused by Echinococcus species. The cystic form of this infection mostly involves liver and lung. Hydatid disease of the parotid gland even in endemic regions is a very rare entity that may be easily overlooked in daily practice. Herein, I present a case report of a 60-year-old Iraqi female patient who presented with a progressively painless mass in her right parotid. It was diagnosed radiologically as a hydatid cyst and was excised successfully. Histopathologic examination of the resected specimen confirmed the hydatid cyst. This case emphasizes the importance of considering hydatidosis in the differential diagnosis of any parotid mass, especially in endemic countries.
 
... Show MoreModeling the microclimate of a greenhouse located in Baghdad under its weather conditions to calculate the heating and cooling loads by computer simulation. Solar collectors with a V-corrugated absorber plate and an auxiliary heat source were used as a heating system. A rotary silica gel desiccant dehumidifier, a sensible heat exchanger, and an evaporative cooler were added to the collectors to form an open-cycle solar assisted desiccant cooling system. A dynamic model was adopted to predict the inside air and the soil surface temperatures of the greenhouse. These temperatures are used to predict the greenhouse heating and cooling loads through an energy balance method which takes into account the soil heat gain. This is not included in
... Show MoreIn this research, deposition of titanium oxide (TiO2) and vanadium oxide (V2O5) thin film in different mixing percentage (0, 25 ,50, 75 and100)% on the substrate of glass .The coating thickness was ( 50 nm ).
In this research contact angle was measured and the effect of weather conditions. Results showed that the value of the contact angle of the prepared films reached its highest value at 50% (TiO2+V2O5) was 160º.
The results showed that the optical transmittance of TiO2 and V2O5 thin film decrease with increasing the deposition angle and decrease with increasing V2O5 pro
... Show MoreThis studies deals with investigated the potential of a Iraqi bentonite clay for the adsorption of bromo phenol red dye from contaminated water. Impulse adsorption experiments were performed. The contact time influence of initial dye concentration, temperature, pH, ionic strength, partical size adsorbent and adsorbent dosage on bromo phenol red adsorption are investigated in a series of batch adsorption experiments. Adsorption equilibrium data were analyzed and described by the Freundlich, Langmuir and temkin isotherms equations. Thermodynamic parameters inclusive the Gibbs free energy (∆G• ), enthalpy (∆H• ), and entropy (∆S• ), were also calculated. These parameters specified that adsorption of bromo phenol red onto bentonite
... Show MoreBaTiO3 thin films have been deposited on Si (111) and glass substrates by using pulsed laser deposition technique. The films were characterized by using X-ray diffraction, atomic force microscope and optical transmission spectra. The films growth on Si after annealing at 873K showed a polycrystalline nature, and exhibited tetragonal structure, while on glass substrate no growth was noticed at that temperature. UV-VIS transmittance measurements showed that the films are highly transparent in the visible wavelength region and near-infrared region for sample annealing on glass substrate. The optical gap of the film were calculated from the curve of absorption coefficient (αhν) 2 vs. hν and was found tobe 3.6 eV at substrate temperature 5
... Show More