This work deals with the effect of adding aluminum nanoparticles on the mechanical properties, micro-hardness and porosity of memory-shape alloys (Cu-Al-Ni). These alloys have wide applications in various industrial fields such as (high damping compounds and self-lubricating applications). The samples are manufactured using the powder metallurgy method, which involved pressing in only one direction and sintered in a furnace surrounded by an inert gas. Four percentages (0%, 5%, 10%, and 15%) of aluminum nanoparticles were fabricated, which depended on the weight of aluminum powder (13%) in the sample under study. To find out which phase is responsible for the reliability of the formation of this type of alloy and its porosity, X-ray diffraction (XRD) and scanning electron microscopy (SEM) tests are used. The Vickers micro-hardness and porosity properties of these alloys were studied using a Vickers micro-hardness and porosity tester according to ASTM b328-1996. The results showed that increasing the concentration of aluminum nanoparticles in the alloy led to an increase in hardness with a decrease in the porosity, and the sample (15%) gave the best hardness (190.8 HV). The sample (0%) gave the highest porosity (19.573) %.
The research involves using phenol – formaldehyde (Novolak) resin as matrix for making composite material, while glass fiber type (E) was used as reinforcing materials. The specimen of the composite material is reinforced with (60%) ratio of glass fiber.
The impregnation method is used in test sample preparation, using molding by pressure presses.
All samples were exposure to (Co60) gamma rays of an average energy (2.5)Mev. The total doses were (208, 312 and 728) KGy.
The mechanical tests (bending, bending strength, shear force, impact strength and surface indentation) were performed on un irradiated and irrad
... Show MoreTetradentate complexes type [M (HL) 2] were prepared from the reaction of 2-hydroxy -1, 2-diphynel-ethanone oxime [H2L] and KOH with ( Mn II, Fe II, Co II, Ni II , Cu II and Hg II ), in methanol with (2:1) metal: ligand ratio. The general formula for Cu II and Mn II complexes are [M (HL) 2 Cl.H2O] K, for Co II [Co (HL) 2. H2O] and [M (HL) 2] for the rest of complexes. All compounds were characterised by spectroscopic methods, I.R, U.V-Vis, H.P.L.C, atomic absorption and conductivity measurements chloride content. From the data of these measurements, the proposed molecular structures for Fe II and Hg II complexes are tetrahedrals, while Mn II and Cu II complexes are octahedrals, Ni II complex adopting square planar structure and the complex
... Show MoreThe research includes the synthesis and identification of the mixed ligands complexes of M+2ions in general composition[M(Asn)2(SMX)] Where L- Aspargine (C4H8N2O3)symbolized (AsnH) as a primary ligand and Sulfamethoxazole(C10H11N3O3S) symbolized (SMX) as a secondary ligand. The ligands and the metal chlorides were brought in to reaction at room temperature in(v/v) ethanol /water as solvent containing NaOH. The reaction required the following [(metal: 2(Na+Asn-): (SMX)] molar ratios with M(II) ions, Where: M(II)=Mn(II), Co(II), Ni(II), Cu(II), Zn(II), Cd(II) and Hg(II). The UV–Vis and magnetic moment data revealed an octahedral geometry around M(II), The conductivity data show a non-electrolytic nature of the complexes. The antimicrobial a
... Show MoreBackground: Fixed orthodontic appliances impede the maintenance of oral hygiene and result in plaque accumulation leads to enamel demineralization caused by acids produced by bacteria. Studies on plaque control strategies in orthodontic populations are limited. This might be caused by difficulties in the quantitative evaluation of dental plaque because the teeth have various levels of bracket coverage, and different tooth sizes and malocclusions, making the traditional categorical indices complex. The present study aims to evaluate the effect of different hygiene protocols on plaque quantity on bands with different attachments. Materials and method: Twenty patients had four bands within the orthodontic appliance. Then randomly divided into
... Show MoreHeat treatment by solid solution method in the ?+? phase region was used at 970°C for Ti-5Al-2.5Fe alloy. The specimens cooled under different cooling media [water quenched (WQ), air cooled (AC) and furnace cooled (FC)], and subsequently aged at 550°C for 4 hours. Five specimens from each treatment were immersed in simulated body fluid SBF for a period of time (3 months). The dependence of corrosion rate on compositional variation in the phases resulted from various type of cooling rates are discussed based on immersion tests. The EDXA results show the precipitation of phosphate and calcium compounds on the alloy after 3 months of immersion in blood plasma solution forming a bone-like apatite, which enhanced the alloy biocompatibility ma
... Show MoreWith the great development in the field of the Internet, the talk about the new media and its implications began, And its interactive services have made the future of media material sometimes participating in it and manufacturing it at other times,
the public is seeking information and choosing the appropriate ones, as well as exchanging messages with the sender after what the role of the receiver is just receiving information only.
This study aims to demonstrate the effects of using digital media in various forms and types to construct the value system of Iraqi society through the identification of the following aims:
Identify the most popular digital media for the Iraqi public in their daily lives on the Internet.
Identify
Liquid – liquid interface reaction is the method for
preparation nanoparticles (NP'S) which depend on the super
saturation of ions that provide by using the system that consist from
toluene and water, the first one is above the second to obtain
nanoparticles (NP's) CdS at the interface separated between these
two immiscible liquid. The structure properties were characterized by
XRD-diffraction and transmission electron microscopy.
The crystalline size estimate from X-ray diffraction pattern
using Scherer equation to be about 7nm,and by TEM analysis give us
that ananosize is about 5 nm which give a strong comparable with
Bohr radius. Photoluminescence analysis give two emission peak,
the first one around
Background: Lack of durability of the bond of the dental adhesive systems to tooth structure is one of the most important problems in tooth colored restorative work. This in vitro study was performed to evaluate the effect of 2% chlorhexidine gluconate(CHX) on dentin bond strength by using total etch adhesive system at twenty-four hours and three months of water storage. Material and methods:A flat dentin surface was prepared for forty sound human maxillary premolar teeth which were acid etched with 36% phosphoric acid gel after being divided randomly into four groups of ten teeth each according to storage time and CHX application, theCHX was applied for 60 seconds before adhesive application for groups I and III which were tested after twe
... Show More