Background: Fractures of patella constitute 1% of all fractures. Various techniques have been described for internal fixation of patella fractures. Superiority of one technique over the other has long been debated. Objective: We reviewed a series of seventy patients with transverse or comminuted fractures of patella treated with cerclage and tension band wiring technique to assess if it had any advantages over k. wires and tension band wiring technique. Type of the study: Retrospective study. Methods; Seventy patients with displaced patella fracture, with a mean age of 47 years (range 13-75) were divided into two groups :group A 36 patients were treated with cerclage and tension bands technique ,and group B 34 patients were fixed by 2 K. wires and tension bands technique. Clinical outcome was assessed using the system of Bostman score. Range of motion and evidence of radiological union were assessed at regular follow-ups. Results; All patients in group A gained Excellent result and good result, while only one patient gained poor result in group B . One patient (2.8%) developed superficial infection in group A and three patients( 8.8% ) developed superficial infection in group B. All fractures had united at the end of 10 weeks. Twenty two patients (31.4%) underwent a second surgery for wire removal; 5 cases in group A ( 13.9 % ) two of them due to implant related complications and 15 ( 44.1%) patients for group B mainly due to pain and interference with daily activity. Malunion or non-union was not noted in any of the cases. . Conclusion; The advantages of the cerclage and tension bands technique for fixation of displaced patella fracture are early mobilization, elimination of k-wire related complications, and ease of use in comminuted fracture pattern as well and a lower reoperation rates as compared to other method of fixation by 2 K. wires and tension bands technique. We strongly recommend its use in cases of displaced comminuted transverse fractures of patella .
In the present study the performance of drying process of dffirent solid materials by batch fluidized bed drying
under vacuum conditions was investigated. Three, different solid materials, namely; ion exchange resin-8528,
aspirin and paracetamol were used. The behavior of the drying curves as well as the rate of drying of these
materials had been studied. The experiments were caried out in a 0.0381 m column diameter fluidized by hot
air under yacuum conditions. Four variables affecting on the rate of drying were studied' these variables are
vacuum pressure (100 - 500 mm Hg), air temperature (303-323 K), particle size (0.3-0.8 mm) and initial
moisture content (0.35-0.55 g/g solid)-for resin and (0.1-0.2 g/g soltid) for a
In this study three reactive dyes (blue B, red R and yellow Y) in single , binary and ternary solution were adsorbed by activated carbon AC in equilibrium and kinetic experiments. Surface area, Bulk and real density, and porosity were carried out for the activated carbon.
Batch Experiments of pH (2.5-8.5) and initial concentration (5-100) mg/l were carried out for single solution for each dye. Experiments of adsorbent dosage effect (0.1-1)g per 100 ml were studied as a variable to evaluate uptake% and adsorption capacity for single dyes(5, 10) ppm, binary and ternary (10) ppm of mixture solutions solution of dyes. Langmuir, and Freundlich, models were used as Equilibrium isotherm models for single solution. Extended Langmuir and Freun
BACKGROUND: Cochlear implant has become a routine procedure for management of severe sensorineural hearing loss. Cochlear implant extrusion is one of the most devastating complication of this procedure. A double layer closure of pericranial flap and scalp rotational flap has being showed to decrease the rate of late implant extrusion.OBJECTIVE:The purpose of this study is to evaluate the use of the pericranial flap as second layer coverage after cochlear implant extrusion.PATIENTS AND METHODS:Eight patients with cochlear implant extrusion in Al-Shaheed Gazi Al-Hariri hospital were operated on by using two layer closure ; the pericranial flap as salvage layer used to cover the cochlear implant and scalp rotational flap as a routine coverage,
... Show MoreThe toxic lead additives to gasoline are no longer used in many countries around the world. Many other countries are now phasing out the lead in gasoline. Although the lead fuel is still in use in Iraq, several plans are considered to phase out the lead. The use of organic compounds to replace the lead additives in gasoline is considered now as an option in Iraqi refineries. The main objective of this project was preparation of premium gasoline, by blending of gasoline with Alternative additives (alcohol, aromatic) to enhancing octane number of Al-Doura gasoline pool. Improved gasoline was tested by ASTM standard method which includes octane number measuring by CFR engine analyzer. Gasoline pool RON (80) was used and selective components
... Show Moreِabstract:In this research we prepared nanofibers by electrospinning from poly (Vinyl Alcohol) /TiO2. The spectrum of the solution (Emission) was studied and found to be at 772 nm, several process parameters were such as concentration of TiO2 , and the effect of distance from nozzle tip to the grounded collector (gap distance). The result of the lower concentration of, the smaller the diameter of nanofiber is. Increasing the gap distance will affect nanofibers diameter.
Simple, sensitive and economical spectrophotometric methods have been developed for the determination of cefixime in pure form. This method is based on the reaction of cefixime as n-electron donor with chloranil to give highly colored complex in ethanol which is absorb maximally at 550 nm. Beer's law is obeyed in the concentration ranges 5-250 µg ml-1 with high apparent molar absorptivities of 1.52×103 L.mole-1. cm-1.
In this research we prepared nanofibers by electrospinning from
poly (Vinyl Alcohol) /TiO2. The spectrum of the solution (Emission)
was studied and found to be at 772 nm, several process parameters
were such as concentration of TiO2 , and the effect of distance from
nozzle tip to the grounded collector (gap distance). The result of the
lower concentration of, the smaller the diameter of nanofiber is.
Increasing the gap distance will affect nanofibers diameter