The master sintering concept is introduced as a unifying sintering model for the initial, intermediate and final stage of sintering. The master sintering curve is independent on the time-temperature trajectory due to account for its integral. The master sintering curve is constructed on a material parameter, which is the activation energy for sintering and other curve shaping parameters, which depends on the initial state of the powder. Literature data of sintering of TiO2 compacts with two initial packing densities of 55% and 69% of theoretical is utilized for the construction of the master sintering curves. The higher initial packing density compact shows higher densification rate, which is reflected by different set of shaping parameters compared with those of lower initial packing density. The master grain growth curve of TiO2 compacts is also constructed which shows slower grain growth for the higher initial packing density compact
In this work, magnesium aluminate spinel (MA) (MgO 28 wt%, Al2O3 72 wt%) stoichiometric compound , were synthesized via solid state reaction (SSR) Single firing stage, and the impact of sintering on the physical properties and thermal properties as well as the fine structure and morphology of the ceramic product were examined. The Spinel samples were pressed at of (14 MPa) and sintering soaking time (2h). The effect of adding oxide titania (TiO2) was studied. The obtained powders were calcined at a temperature range of 1200 and 1400 °C. The calcined samples spinel were characterized by XRD, it showed the presence of developed spinel phase end also showed that the best catalyst is titania. The SEM image showed the high sintering temperat
... Show MoreThe sintering behavior of Alumina was investigated by adding TiO2. The addition of TiO2 lowered the sintering temperature of the Alumina compared with those of pure Alumina. The result suggests that TiO2 acts as an activator for sintering of Alumina. Water absorption, apparent porosity and density were examined for both pure and TiO2 added to Alumina samples. The variations of sintering behavior were discussed in terms of shrinkage, porosity, water absorption and density. Thermal shock resistance was also examined. In term of this work, the way of improving the thermal shock resistance in oxide- based materials by adding reactive Titania powder to the Alumina samples. The laboratory results showed an improvement in thermal shock resistance
... Show MoreThis research studies the effect of particle packing density on sintering TiO2 microstructure. Sintering experiment was conducted on compacts involving of monodisperse spherical TiO2 particles. The experimental results are modeled using L2-Regression technique in studing the effect of two theoretical values of 55% and 69% of initial packing densities. The mathematical simulation shows that the lower values of density compacts sintered fast to theoretical density and this reflects that particle packing density improved densification rate because of the competing influence of grain growth at higher values of densities.
The Elliptic Curve Cryptography (ECC) algorithm meets the requirements for multimedia encryption since the encipher operation of the ECC algorithm is applied at points only and that offer significant computational advantages. The encoding/decoding operations for converting the text message into points on the curve and vice versa are not always considered a simple process. In this paper, a new mapping method has been investigated for converting the text message into a point on the curve or point to a text message in an efficient and secure manner; it depends on the repeated values in coordinate to establish a lookup table for encoding/ decoding operations. The proposed method for mapping process is&
... Show MoreRecent research has examined the improvement of physical and dielectric properties of BaTiO3 ceramic material by small addition of excess TiO2 or BaCO3. The prepared samples sintered at different temperatures and varying soaking time. The results show that increasing the sintering temperature within 1350°C and soaking time of 10 hrs give better electrical and physical properties, which indicate the reaction is complete at higher temperature and period.
The emphasis of Master Production Scheduling (MPS) or tactic planning is on time and spatial disintegration of the cumulative planning targets and forecasts, along with the provision and forecast of the required resources. This procedure eventually becomes considerably difficult and slow as the number of resources, products and periods considered increases. A number of studies have been carried out to understand these impediments and formulate algorithms to optimise the production planning problem, or more specifically the master production scheduling (MPS) problem. These algorithms include an Evolutionary Algorithm called Genetic Algorithm, a Swarm Intelligence methodology called Gravitational Search Algorithm (GSA), Bat Algorithm (BAT), T
... Show MoreHigh temperature superconductor with nominal composition Bi1.6Pb0.4Sr1.8Ba0.2Ca2 Cu3O10+? was prepared by solid state reaction method. Two sets of samples have been prepared .The first one was quenched in air; the second set was quenched in liquid nitrogen. X-ray diffraction analyses showed an orthorhombic structure with two phases, high –Tc phase (2223) and low-Tc phase (2212) in addition to that impure phase was found. It has been observed that quenched in air samples display a sharp superconducting transition and a higher-Tc phase than that of the quenched in liquid nitrogen samples.
This research studies the effect of grain size for the final stage in sintering Al2O3 .The experimental results for α- Al2O3 powder are modeled using ( L2-Regression ) technique in order to study the effect grain size distribution on densification rate using four kinds for the initial particle size which were ( 1.44 , 2.54 , 0.7-2.54 ,1.15-3.53 ) µm , and for sintering time (0-241) min. The mathematical simulation for grain size changing shows that the densification rates boots up as the grain size goes lower, this was due to the increase of contact area between the grains.