This study included preparation for the unsaturated polyester samples before and after reinforced by the Alumina oxide powder of different volume fraction amounting (2%,4%,6%). And this research included the study of some of mechanical properties such as (Hardness,compressive,wear). The results showed that the increase of the hardness and compressive strength after the reinforced and the increase with the volume fraction increase. As the wear test shows that the wear rate increases with applied load increase(5,10,15) from (10.6-18.6) gm/cm befor reninforced and from(5.4-15.2)gm/cm,(4.7-12.9)gm/cm,(48.1)gm/cm,after reinforced from the different volume fraction, and the wear rate decrease with the volume fraction increase
An Investigation of estimated Mechanical Properties of AL-Alloys 2024-T3, which is the most commonly used in industrial applications, been established experimentally. A new novel Plasma Peening techniques had applied for the whole surfaces of the material by CNC-Plasma machine for 48 specimen, and then a new investigation were toke over to figure the amount of change in mechanical properties and estimated fatigue life. It found that improvement was showing a nonlinear behavior according to peening duration time, speed, peening distance, peening number, and amount of effected power on the depth of the material thickness. The major improvement was at medium speed long duration time normal peening distance. Which shows up t
... Show MoreThe study included examination of three types of different origin and orange juice at the rate of recurring per sample, the results showed that the highest rates of acid (pH) in the A and juice were (4). And salts of calcium is 120 ppm in juice C and 86 ppm of magnesium in the juice B, for heavy metals the highest rate of lead .18 recorded ppm in juice B, 1.32 ppm of copper in juice A, 5 ppm of iron in the juice B, 1.3 ppm of zinc in the juice B, 0.05 ppm of aluminum in each of the sappy B and A, 0.02 ppm of cobalt in the juice B, 0.3 ppm of nickel in the juice B, 170.6 ppm sodium in C juice, but for the acids, organic that the highest rates were 3.2 part Millions of acid in the juice owner a, 260 ppm of the acid in the juice the ascorbi
... Show MoreNatural fibers and particles reinforced composites are being broadly used due to their bio and specific properties such as low density and easy to machine and production with low cost. In this work, water absorption and mechanical properties such as tensile strength, flexural strength and impact strength of recycled jute fibers reinforced epoxy resin were enhanced by treating these fibers with alkaline solution. The recycled jute fibers were treated with different concentration of (NaOH) solution at (25 0C) for a period of (24) hours. From the obtained results, it was found that all these properties are improved when fibers treated with (7.5wt% NaOH) related to untreated fibers. Conversely, the mentioned properties of composit
... Show MoreThe CdSe pure films and doping with Cu (0.5, 1.5, 2.5, 4.0wt%) of thickness 0.9μm have been prepared by thermal evaporation technique on glass substrate. Annealing for all the prepared films have been achieved at 523K in vacuum to get good properties of the films. The effect of Cu concentration on some of the electrical properties such as D.C conductivity and Hall effect has been studied.
It has been found that the increase in Cu concentration caused increase in d.c conductivity for pure CdSe 3.75×10-4(Ω.cm)-1 at room temperatures to maximum value of 0.769(Ω.cm)-1 for 4wt%Cu.All films have shown two activation energies, where these value decreases with increasing doping ratio. The maximum value of activation energy was (0.319)eV f
Different percents(1.0,2.5,5.0 and 10)wt%of MgO powders were added to ZnO powder to study their effects on the physical properties of ZnO.Density, porpsity and water absorption of ZnO were decreased as MgO weigth percentage content increased. The values of vickers hardneess have double values especially at 1.0 wt % of MgO.
Bobbin friction stir welding (BFSW) is a variant of the conventional friction stir welding (CFSW); it can weld the upper and lower surface of the work-piece in the same pass. This technique involves the bonding of materials without melting. In this work, the influence of tool design on the mechanical properties of welding joints of 6061-T6 aluminum alloy with 6.25 mm thickness produced by FSW bobbin tools was investigated and the best bobbin tool design was determined. Five different probe shapes (threaded straight cylindrical, straight cylindrical with 3 flat surfaces, straight cylindrical with 4 flat surfaces, threaded straight cylindrical with 3 flat surface and threaded straight cylindrical with 4 flat surfaces) with various dimensio
... Show MoreIn this paper, three tool paths strategies; iso-planar, helical and adaptive have been implemented to investigates their effect on the mechanical properties of Brass 65-35 formed by single point incremental sheet metal forming process. To response this task, a fully digital integrated system from CAD modeling to finished part (CAD/CAM) for SPIF process has been developed in this paper.
The photo-micrographs shows an identical grain formation due to the plastic deformation of the incremental forming process, change in the grain shape and size was observed. It's found that the adaptive tool path play a significant role to increase the hardness of the formed specimen from (48 to 90 HV) and the grain texture of the formed specimen found a
InSb alloy was prepared then InSb:Bi films have been prepared successfully by thermal evaporation technique on glass substrate at Ts=423K. The variation of activation energies(Ea1,Ea2)of d.c conductivity with annealing temperature (303, 373, 423, 473, 523 and 573)K were measured, it is found that its values increases with increasing annealing temperature. To show the type of the films, the Hall and thermoelectric power were measured. The activation energy of the thermoelectric power is much smaller than for d.c conductivity and increases with increasing annealing temperature .The mobility and carrier concentration has been measured also.
In this study the melting point and hardness of the paraffin wax was improved by mixing it with 1:1 ratio of micro crystalline wax then adding weight percentage wt% of locally produced nano particles (CuO,ZnO,AI2O3 and bentonite ) for each addition to the wax mixture. The results showed an increase in the melting point and hardness values of the prepared samples by increasing the weight percentage of each nano particles additives. . It was found that the addition of nano bentonite to the wax mixture gave high melting point values (122.5°C)and hardness (81.2)followed by melting point value (97°C)and hardness(68.2)resulting from the addition of CuO nano particles to the wax mixture compared to other used nano particles.