In this research, we prepared a hybrid composite material of polymeric matrix hand cast method, composite material has been attended from epoxy resin EP as matrix materials reinforced woven roving fiber jute is constant volume fraction (13%), PVC fibers and woven glass fiber with different fraction on the properties of prepared composite materials to PVC fiber and glass fiber, some of mechanical tests were done at room temperature (impact test and banding test). Result shows that the values of (modulus bending elastic and fracture toughness) increase fraction of fiber with the increase of PVC, E-glass, there include (thermal conductivity and dielectric constant). Also experimental result indicated that the (thermal conductivity and dielectric constant) increase with the increase of fiber volume fraction.
Objective This study evaluated the effects of adding titanium oxide (TiO2) nanofillers on the tear strength, tensile strength, elongation percentage, and hardness of room-temperature-vulcanized (RTV) VST50F and high-temperature-vulcanized (HTV) Cosmesil M511 maxillofacial silicone elastomers. Methods Two types of maxillofacial elastomers, VST50F RTV and Cosmesil M511 HTV, were used. Nano-TiO2 powder was applied as a nanofiller. A total of 120 specimens were fabricated, 60 each of VST50F and Cosmesil M511. The specimens of each type of elastomer were divided into three equal groups on which tests were conducted for tear strength, tensile strength, and hardness i.e., 20 specimens were used for each test. Each group of 20 specimens was further
... Show MoreIn this study the thermal conductivity of the epoxy composites were characterized as function of volume fraction, particle size of fillers and the time of immersion(30,60,90)days in water .Composites plates were prepared by incorporating (bi-directional) (0º-90º) glass fiber and silicon carbide (SiC) particles of (0.1,0.5,1)mm as particle size at (10%,20%,30%,40%) percent volume in epoxy matrix.
The composites shows slightly increase of the thermal conductivity with increasing volume fraction, particle size and increase with increasing the days of immersion in water. The maximum thermal conductivity (0.51W/m.K) was obtained before the immersion in water at 90 days for epoxy reinforcement by bi-directional glass fiber and SiC particl
In this investigation, the mechanical properties and microstructure of Metal Matrix Composites (MMCs) of Al.6061 alloy reinforced by ceramic materials SiC and Al2O3 with different additive percentages 2.5, 5, 7.5, and 10 wt.% for the particle size of 53 µm are studied. Metal matrix composites were prepared by stir casting using vortex technique and then treated thermally by solution heat treatment at 530 0C for 1 hr. and followed by aging at 175 0C with different periods. Mechanical tests were done for the samples before and after heat treatment, such as impact test, hardness test, and tensile test. Also, the microstructure of the metal matrix composites was examine
... Show Moreإن النجاح في أداء المتطلبات الفنية والخططية في أي من الألعاب ألرياضيه يستوجب امتلاك العناصر الاساسيه المتعلقة بطبيعة الاداء ونوع الفعالية الرياضية الممارسة , لذا فان اغلب الألعاب الرياضية تعتمد على مكونات ألقدره التوافقيه والادراكيه الحسيه بوصفها احد العناصر الاساسيه في المستويات العليا لما توفره من قاعدة اقتران للصفات البدنيه والحر كيه وقدرات أجهزة الجسم الوظيفية , وفقا للأسس المعتمدة في بناء مهاراته, وع
... Show MoreAcrylic polymer/cement nanocomposites in dark and light colors have been developed for coating floors and swimming pools. This work aims to emphasize the effect of cement filling on the mechanical parameters, thermal stability, and wettability of acrylic polymer. The preparation was carried out using the casting method from acrylic polymer coating solution, which was added to cement nanoparticles (65 nm) with weight concentrations of (0, 1, 2, 4, and 8 wt%) to achieve high-quality specifications and good adhesion. Maximum impact strength and Hardness shore A were observed at cement ratios of 2 wt% and 4 wt%, respectively. Changing the filling ratio has a significant effect on the strain of the nanocomposites. The contact angle was i
... Show MoreWhich children infected with physical growth retardation at childhood it will be the largest problems effecting the child and his parents together. So , at the period of early childhood, there must be a state of satisfactions of need because if they didn’t satisfied it will be very hard to be satisfied or replaced at another period because it will be busy with satisfaction of another need of new period, and even it will be satisfactions it still weak and didn’t be am efficient as the matter of if it be satisfied at the exact time Looking at physical growth and its indicators as length and weight and making a comparison with world indicators at peer age phases helps in spe
... Show MoreThe increasing use of plastics in various aspects of modern life resulted in the availability of enormous amount of wastes, including a negative effect on the environment and humans. So it is necessary to find solutions to deal with these wastes and ensure to use them as solutions to use in concrete mix . In this research the production of concrete containing high and low density polyethylene has been used by (5, 10, 15)% as a replacement of part of the volume of sand, so as to obtain concrete good compressive strength as well as other benefits such as improved possibility of pumping concrete and reduce the loss of concrete for workability polymer is a material that is non-absorbable of water . It is also intended to dispose of these was
... Show MoreThe study aimed to determine of some Optimum conditions for bioremediation and removing of seven mineral elements included hexavalent chromium, nickel, cobalt, cadmium, lead, iron and copper as either alone or in group by living and heat treated cells of baker’s yeast Saccharomyces cerevisiae. The dried baker's yeast from Aldnaamaya China Company was used in this study. Biochemical tests was used to ensure yeast belonging to S. cerevisiae and then used to remove the mentioned mineral elementes under different conditions which included incubation period, pH, and temperature. It was found that the best of these conditions was 60 minutes for duration of incubation, 6 for pH, 25 ᵒC for temperature. During the study the behavior of living
... Show MoreIn this investigation insulator ceramic body was prepared by using iraqi local materials, these are kaolin, silica sand glass, feldspar with weight percentage (45%,25%, 30%)respectively. After the end of treating drying and milling of raw material mixing with different concentrations of sodium silicate(1%,0.7%,0.5%,0.2%,0.1%) while zinc oxide was added at fixed weight percentage. A disc samples was prepared after compaction and then fired by sintering temperatures (1250, 1350)oC respectively.A surface morphology was studied by using optical microscope and measurements of apparent density and porosity was under taken to the sintered samples by using Archimedes method.The study showed that the microscopic images for samples sur