Background: This study aimed to evaluate the effect of zirconia different surface treatments (primer, sandblast with 50μmAl2O3, Er,Cr:YSGG laser) on shear bond strength between zirconia surface and resin cement. Material and methods: Sixty presintered Y-TZP zirconia cylinder specimens (IPS e.max ZirCAD, Ivoclar vivadent) will be fabricated and sintered in high temperature furnace of (1500 C for 8 hours) according to manufacturer’s instructions to the selected size and shape of (5mm. in diameter and 6mm in height). All specimens were ground flat using 600.800.1000.1200, aluminum oxide abrasive paper to obtain a standardized surface roughness. Surface roughness values were then recorded in µm using surface roughness tester (profilometer) to obtain a standardized data base line for all samples. The specimens were then randomly divided into three main groups (n=20); group A: no surface treatment (control group), group B: specimens in this group treated with 50μm Al2O3 and group C: specimens in this group treated with Er,Cr:YSGG laser. Sixty sound human premolars were used in this study, after construction of acrylic blocks, the occlusal surface of the teeth were ground flat, with diamond cutting disk to obtain a flat dentine surface . Prior to cementation of zirconia cylinders to tooth specimens subgroups (A1,B1,C1) will receive a coat of metal/zirconia primer and left to react for three minutes, while the subgroups (A2,B2,C2) were left undisturbed. Bonding surface of zirconia cylinder was then luted with SpeedCEM self adhesive resin cement under a static load of 2Kg. placed on the vertical arm of the surveyor and allowed to auto cure for 4minutes.The final cemented specimens were then stored in distilled water at room temperature for 24hours. All specimens were subjected to shear loading force in a universal testing machine at crosshead speed of 1mm/min. The shear bond strength values were analyzed statistically with one-way ANOVA; the fractured surfaces of zirconia cylinders were examined with a stereo-microscope to observe the failure mode. Results: The air borne-particle of 50μm followed by primer application showed significantly the higher bond strength than other groups. Conclusion : Within the limitation of this study, the results showed that sandblasting the bonding surface of zirconium cylinders with 50μmAl2O3 produced the highest values of shear bond strength , also the use of primer enhanced shear bond strength as well. Keyword: zirconia surface treatments, shear bond strength.
The research aims to know the effect of investment risks measured by the beta coefficient on the efficiency of stock pricing measured by the pricing error. The research was applied in the banks listed in the Iraq market for the period (2017-2020). That affects the value of the shares of the companies listed in it and the risks associated with it, as the risks are a dynamic process that changes over time depending on the variables that affect the general development of the economy, so these fluctuations should be taken into account to achieve maximizing returns and reducing risks and what is reflected in stock prices in the Iraqi markets Securities, through which the following question was asked: How does investment risk affect the efficienc
... Show MoreIntroduction: Since the hallmark of gestational trophoblastic disease is trophoblastic proliferation, Ki67 is regarded as the best marker in studying hydatidiform mole.This study was conducted to evaluate the role of this proliferative marker in distinguishing among hydropic abortion, partial and complete hydatidiform mole. Materials and methods: This is a cross sectional study involving the application of Ki67 on a total of 90 histological samples of curetting materials from molar (partial and complete mole) and non molar hydropic abortion belong to Iraqi females, so three study groups were created. Immunohistochemical expression in villous cytotrophoblasts, syncytiotrophoblasts and stromal cells were recorded separately by three i
... Show MoreThe anatomic characteristics of the leaves of 22 taxa of Stachys L. representing seven of the currently recognized sections distributed in northern Iraq, were examined. The study did not found any variations in the characteristics of the stomata system of the leaves.Therewere variations with a good taxonomic value in other anatomic characteristics.Thevariations in characters of the mesophyll tissue in S.kurdica var.brevidens Bom ex Bhattacharjeewas bifacial but in S.kurdica var.kurdica Boiss. & Hohen.was unifacial .The study also found that the taxa S.benthamiana Bioss., S.lanigera (Bornm.) Rech.f. andS.kotscyi Bioss. with 3 vascular bundles in the middle vein while the taxa S.ballotiformis Vatke., S.megalodonta Hausskn. &Bo
... Show MoreBackground: Ultrasound is a valuable tool for evaluating fetal problems throughout pregnancy. Amniotic fluid anomalies have been associated with unfavorable maternal, fetal, and obstetrical outcomes. Objective: To determine the effect of echogenic amniotic fluid during term pregnancy on the presence of meconium stain liquor and pregnancy outcome. Methods: A cross-sectional study was conducted on 1080 term pregnant women who visited Al-Elwiya Maternity Teaching Hospital from May 1st, 2021, to May 1st, 2023. Ultrasound was used to analyze echogenic amniotic fluid and turbid liquor. The liquor state was tested either after an artificial membrane rupture in the vaginal delivery trial or during a cesarean section. Results: Echogenic amni
... Show MoreCurrent studies interested on the biosynthesis of zinc oxide nanoparticles (ZnO-NPs) using hot plants extracts of Allium sativum and characterization of them using: Atomic Force Microscopy (AFM), X-ray diffractions (XRD), Fourier Transform Infrared Spectroscopy (FT- IR), UV–visible spectral and Hot stage. The results found that all NPs are had nano-size. ZnO NPs was produced by four procedures using hot extract of Allium sativum. The average diameters were: 101.59 nm, 110.33 nm, 75.69 nm, 88.67 nm for first, second, third and fourth procedures respectively compared with 47.57 nm for standard NPs. The Roughness averages (Ra) were: 10.8 nm, 6.83 nm, 13.8 nm, 0.541 nm for first, second, third and fourth respectively. The Root mean square (Sq
... Show More