Background: Poly (methylmethacrylate) is the most widely used material in denture fabrication. The characteristics of acrylic resin which support microorganism development can threaten the oral health of denture users. This study was assigned to prepareand incorporate Ag-Zn zeolite powder into heat cured denture base material as antimicrobial material and to investigate its effect on some properties of heat cured acrylic denture base materials. Materials and methods: Sliver –zinc zeolite was prepared by ion exchange method and characterized then incorporated into poly (methylmethacrylate) powder in0.5% by weight. Specimens were constructed and divided into 6 groups according to the using tests; each group was subdivided into 2 groups. The tests conducted in this study were: impact strength test, transverse strength test, surface hardness test, surface roughness test, water sorption test, water solubility test and color change measurement after addition. The results were statistically analyzed by t-test at p value≤ 0.05. Results: Characterization methods results showed the incorporation of sliver and zinc ion without change of zeolite structure framework. A non-significant effect resulted from the addition of 0.5% sliver –zinc zeolite on the impact strength, transverse strength, surface hardness, surface roughness and cause no change in color of heat cure denture base. Also a highly significant decrease in water sorption and a significant increase of water solubility were observed. Conclusion: Preparation of sliver-zinc zeolite could be performed successfully and the addition of 0.5% of antimicrobial sliver-zinc zeolite into heat cure acrylic had a non significant effect on the impact strength, transverse strength, surface hardness, surface roughness and did not change the color, also there was a significant decrease in water sorption and increase in water solubility of acrylic resin. Key words: Denture stomatitis, Antimicrobial agent, Ag- Zn Zeolite.
The study of biomechanical indicators in the arc of the run and the upgrading stage is one of the important variables that affect the nature of the upgrading and thus affect the result of the race due to the importance of these stages and the consequent variables during the last steps. That’s why, the jump-trainings based on assistant means or body weight positively affect the step-time for each of the three steps in the acceleration arc. As well as, it focuses on the momentary strength of each step at this stage. It also significantly affects the speed of motor performance to suit the activity in which the runner needs to perform perfect steps with high flow in order to convert the horizontal speed to a vertical one. This is achieved thr
... Show MoreCitrus fruit contain variety of flavonoids such as Hesperidin (the principal flavonoid in oranges and grapefruit). Hesperidin is found in high concentration in fruit peel of oranges and in substantially lower concentration in juice of these fruits. Hesperidin was extracted from oranges peel by treating the peels with calcium hydroxide. HPLC technique was used to determine hesperidin. Hesperidin was saperated and purified in a purity of about 90.1-95.7% and yield about 1.5 %w/w from oranges peel dry powder. Both hesperidin and oranges peel extract showed significan antibacterial activity. Sensitivity to hesperidin and oranges peel extracts were not similar for the chosen bacteriaCrude orange peel extract gave a various antimicro
... Show MoreHypothyroidism has been associated with disorders of glucose and insulin metabolism..The present study was designed to evaluate the possible change in some hormones (free testosterone, estradiol, prolactin, insulin), glucose and homeostasis model assessment of insulin resistance (HOMA-IR) in women with primary hypothyroidism under thyroid hormone replacement therapy .This cross-sectional study was carried on 62 hypothyroid patients׳ women and 22 healthy women as control group at the specialized center for endocrinology and diabetes, AL-Rasafa Directorate of Health Baghdad, with age range(15-60 years), diagnosed as having primary hypothyroidism on thyroxine replacement therapy with duration not less than four months.
... Show MoreThe Neutron Fermi Age, t, and the neutron slowing down density, q (r, t) , have been measured for some materials such as Graphite and Iron by using gamma spectrometry system UCS-30 with NaI (Tl) detector. This technique was applied for Graphite and Iron materials by using Indium foils covered by Cadmium and the measurements done at the Indium resonance of 1.46 eV. These materials are exposed to a plane 241Am/Be neutron source with recent activity 38 mCi. The measurements of the Fermi Age were found to be t = 297 ± 21 cm2 for Graphite, t = 400 ± 28 cm2 for Iron. Neutron slowing down density was also calculated depending on the recent experimental t value and distance.
This study focused on the improvement of the quality of gasoline and enhancing its octane number by the reduction of n-paraffins using zeolite 5A. This study was made using batch and continuous mode. The parameters which affected the n-paraffin removal efficiency for each mode were studied. Temperature (30 and 40 ˚C) and mixing time up to 120 min for different amounts of zeolite ranging (10-60 g) were investigated in a batch mode. A maximum removal efficiency of 64% was obtained using 60 g of zeolite at 30 ˚C after a mixing time 120 min. The effect of feed flow rate (0.3-0.8 l/hr) and bed height (10-20 cm) were also studied in a continuous mode. The equilibrium isotherm study was made using different amounts of zeolite (2-20 g) and the
... Show MoreThe present research was conducted to synthesis Y-Zeolite by sol-gel technique using MWCNT (multiwalled carbon nanotubes) as crystallization medium to get a narrow range of particle size distribution with small average size compared with ordinary methods. The phase pattern, chemical structure, particle size, and surface area were detected by XRD, FTIR, BET and AFM, respectively. Results shown that the average size of Zeolite with and without using MWCNT were (92.39) nm and (55.17) nm respectively .Particle size range reduced from (150-55) nm to (130-30) nm. The surface area enhanced to be (558) m2/g with slightly large pore volume (0.231) km3/g was obtained. Meanwhile, degree of crystallization decrease
... Show More