Background: It may be an important prospective clinical use of manufacturing of porous implant for clinical situations, such as cases of limitation in bone height, low bone density .The small segment of porous implant an effective osseointegration allows increasing in contact area provided for small segmented porous provided by its surface configuration. This study was done to Fabricate porous titanium implants by powder technology, as well as the observation of removal torque values of porous titanium implants compared to smooth titanium implants. Materials and methods: Twenty porous titanium implants (3.2mm in diameter and 8mm in length) were manufactured by powder technology using commercially pure titanium powder of ≤75um particles size, with polyvinyl alcohol powder of 212-300um particle size, as a space holder, by volume ratio (70:30) % respectively. The mixed powder was compacted using punch and die set -specially designed for this study –under 20 bar then sintering at 900 ºC by the use of argon gas. Twenty smooth titanium implants were prepared of (3.2mm in diameter and 8mm in length) by lathing of commercially pure titanium rod as a control group. The implants were examined by X-ray diffraction (XRD) and scanning electron microscope (SEM), as well as estimation of porosity percentage. For each tibia of the 20 white New Zealand rabbits, one implant of each type (one porous in right, and the smooth in left tibia), were inserted through surgical procedure carried under serial condition. Mechanical test was performed to evaluate the bone-implant interface, after (2 and 6 weeks) healing periods . Results: Porous implants were obtained successfully by powder technology with 52% porosity and pore size 210um 17±. The porous implant showed significantly higher removal torque values when compared to smooth implants at the two different intervals of examination (2,6 weeks) , this proved to be statistically highly significant, also a highly significant difference was noticed for the means of the torque removal values in the same group at different implantation , with no evidence of clinical features of inflammatory reaction with both . Conclusions: Powder technology seemed to be particularly advantageous in fabrication of porous titanium. Porous implant show an increasing bone ingrowth compared with the smooth type represented by higher removal torque for both healing periods (2, 6) weeks . Key words: Porous titanium implant, powder technology, removal torque test.
This study investigates consecutive reaction assisted by pervaporation for the first time. It studies the saponification of diethyladipate DA with sodium hydroxide NaOH solution synchronous with separating ethanol from the reaction mixture through an aqueous – organic membrane. The effect of time on some variables such as: permeated ethanol concentration EtOH wt%, separation factor (α), concentration of NaOH solution CB in the reaction medium and the conversion of DA to monoethyladipate (the intermediate product) was studied. It was shown that EtOH wt% and the conversion increased with increasing time unlike CB but (α) showed the existence of maximum value during the time of experiment. The process of reaction assisted by pervaporation
... Show MoreMassive multiple-input multiple-output (m-MIMO) is considered as an essential technique to meet the high data rate requirements of future sixth generation (6G) wireless communications networks. The vast majority of m-MIMO research has assumed that the channels are uncorrelated. However, this assumption seems highly idealistic. Therefore, this study investigates the m-MIMO performance when the channels are correlated and the base station employs different antenna array topologies, namely the uniform linear array (ULA) and uniform rectangular array (URA). In addition, this study develops analyses of the mean square error (MSE) and the regularized zero-forcing (RZF) precoder under imperfect channel state information (CSI) and a realist
... Show MoreThe experiment aimed to Manufacture a device for checking the nozzles and testing its efficiency and to study the effect of research factors on the studied traits. The device was manufactured locally through using materials available in the Iraqi market. The system is Both Hydraulic and electronic (ISO 5682-1)1 relay on sensors technology and the test platform was built and designed on a movable trolly at the department of Agricultural Machines and Equipment / College of Agricultural Science / University of Baghdad. The design includes the use of mechanical water pump and electrical AC water pump. The design includes a nozzle holder that can accommodate three nozzles per test. The design also consists of spreading wings and stationa
... Show MoreThe products of composites material are very sesetive to many variables, such as manufacturing process, additive materials, …. etc. Filler or additive plays a major role to determine the formation of the properties and behavior of the composites. In this study, polyethylene terephthalate-based compounds were produced and characterized. The work is concerned to prepare samples of Polyethylene terephthalate (PET) - zinc-ferrite (ZnFe2O4) with different addition ratio as zinc-ferrite (1, 2, 5, 10, 15 and 20) wt% obtained from mixing the solution with a hot pressing method applied under optimum conditions. The densities of the composites for all samples were calculated. Through the work the diffusion of zinc-ferrite i
... Show MoreKE Sharquie, AA Noaimi, SY Mohsin, 2011 - Cited by 4
We have investigated the photoemission and electronic properties at the PTCDI molecules interface on TiO2 and ZnO semiconductor by means of charge transition. A simple donor acceptor scenario used to calculate the rate for electron transfer of delocalized electronics in a non-degenerately TiO2 and ZnO electrodes to redox localized acceptors in an electrolytic. The dependent of electronic transition rate on the potential at contact of PTCDI with TiO2 and ZnO semiconductors, it has been discussion using TiO2 and ZnO electrodes in aqueous solutions. The charge transfer rate is determining by the overlapping electronic coupling to the TiO2 and ZnO electrodes, the transition energy, potential and polarity media within the theoretical scenario of
... Show MoreThe aim of this study is to propose mathematical expressions for estimation of the flexural strength of plain concrete members from ultrasonic pulse velocity (UPV) measurements. More than two hundred
pieces of precast concrete kerb units were subjected to a scheduled test program. The tests were divided into two categories; non-destructive ultrasonic and bending or rupture tests. For each precast unit, direct and indirect (surface) ultrasonic pulses were subjected to the concrete media to measure their travel velocities. The results of the tests were mointered in two graphs so that two mathematical relationships can be drawn. Direct pulse velocity versus the flexural strength was given in the first relationship while the second equati