Background: It may be an important prospective clinical use of manufacturing of porous implant for clinical situations, such as cases of limitation in bone height, low bone density .The small segment of porous implant an effective osseointegration allows increasing in contact area provided for small segmented porous provided by its surface configuration. This study was done to Fabricate porous titanium implants by powder technology, as well as the observation of removal torque values of porous titanium implants compared to smooth titanium implants. Materials and methods: Twenty porous titanium implants (3.2mm in diameter and 8mm in length) were manufactured by powder technology using commercially pure titanium powder of ≤75um particles size, with polyvinyl alcohol powder of 212-300um particle size, as a space holder, by volume ratio (70:30) % respectively. The mixed powder was compacted using punch and die set -specially designed for this study –under 20 bar then sintering at 900 ºC by the use of argon gas. Twenty smooth titanium implants were prepared of (3.2mm in diameter and 8mm in length) by lathing of commercially pure titanium rod as a control group. The implants were examined by X-ray diffraction (XRD) and scanning electron microscope (SEM), as well as estimation of porosity percentage. For each tibia of the 20 white New Zealand rabbits, one implant of each type (one porous in right, and the smooth in left tibia), were inserted through surgical procedure carried under serial condition. Mechanical test was performed to evaluate the bone-implant interface, after (2 and 6 weeks) healing periods . Results: Porous implants were obtained successfully by powder technology with 52% porosity and pore size 210um 17±. The porous implant showed significantly higher removal torque values when compared to smooth implants at the two different intervals of examination (2,6 weeks) , this proved to be statistically highly significant, also a highly significant difference was noticed for the means of the torque removal values in the same group at different implantation , with no evidence of clinical features of inflammatory reaction with both . Conclusions: Powder technology seemed to be particularly advantageous in fabrication of porous titanium. Porous implant show an increasing bone ingrowth compared with the smooth type represented by higher removal torque for both healing periods (2, 6) weeks . Key words: Porous titanium implant, powder technology, removal torque test.
Enhancing asphalt binder performance against anticipated distresses is a critical focus in pavement engineering. This study investigates the synergistic influence of nano titanium dioxide (NT) and nano zinc oxide (NZ) on asphalt binder performance. Nine NT:NZ combinations (1:1 to 3:3) were prepared with 1–3% by binder weight, in addition to a reference binder (RB). The performance test program included; conventional tests (penetration, softening point, viscosity, and ductility), Dynamic Shear Rheometer (DSR) for performance grading, Multiple Stress Creep Recovery (MSCR) for rutting evaluation, and Linear Amplitude Sweep (LAS) for fatigue resistance. Furthermore, Statistical analysis (ANOVA) was performed to determine the significa
... Show MoreThis study was done to compare the morphometric parameters of placentas in well controlled patients with preeclampsia, diabetes, and preeclampsia-diabetes with that of normal uncomplicated placentas. Patients & Methods: A total of Twenty four placentas were freshly collected. Six placentas for control group and eighteen placentas for complicated group (preeclamptic-diabetic and preeclamptic--diabetic subgroups). The placentas were grossly examined (shape, number of cotyledons, weight, and thickness). After suitable fixation, tissue processing and sectioning, the sections were stained by hematoxylin and eosin to study the general morphology and morphometry of the following parameters: number of terminal villi, number of syncytial knots, numb
... Show MoreA novel technique for nanoparticles with a chemical method and impact for resistance bacteria methicillin-resistant Staphylococcus aureus (MRSA), UV-visible analysis confirmed the by Fourier transform infrared spectroscopy (FT-IR) and Energy dispersive X-Ray (EDX), Scanning electron microscope (SEM) and X-ray diffraction pattern estimation antimicrobial excellent antibacterial activity against MRSA (with zone of inhibition of 11 ± 02 mm , 9 ± 01 mm,8 ± 03 mm and 7.5 ± 02 mm and 6.5 ± 02 mm) at different concentrations (0.5 ,0.25, 0.125, 0.0625, 0.03125) mg/ml while good activity was 16 ± 03 mm at 17 ± 02 mm zone at 0.25, 0.125 mg/mL, respectively. The increase in microorganism resistance to antibiotics a couple of have caused
... Show MoreThis paper studied the behaviour of reinforced reactive powder concrete (RPC) two-way slabs under static load. The experimental program included testing three simply supported slabs of 1000 mm length, 1000 mm width, and 70 mm thickness. Tested specimens were of identical properties except their steel fibers volume ratio (0.5 %, 1 %, and 1.5 %). Static test results revealed that, increasing steel fibers volume ratio from 0.5% to 1% and from 1% to 1.5%, led to an increase in: first crack load by (32.2 % and 52.3 %), ultimate load by (36.1 % and 17.0 %), ultimate deflection by (33.6 % and 3.4 %), absorbed energy by (128 % and 20.2 %), and the ultimate strain by (1.1 % and 6.73 %). The stiffness and ductility of the specimens also increased. A
... Show MoreIn this research, the structural behavior of reinforced concrete columns made of normal and hybrid reactive powder concrete (hybrid by steel and polypropylene fibers) subjected to chloride salts with concentration was 8341.6 mg/l. The study consists of two parts, the first one is experimental study and the second one is theoretical analysis. Three main variables were adopted in the experimental program; concrete type, curing type and loading arrangement. Twenty (120x120x1200) mm columns were cast and tested depending on these variables. The samples were reinforced using two different bars; Ø8 for ties and Ø12 with minimum longitudinal reinforcement (0.01Ag). The specimens were divided into two main groups based o
... Show MoreThis systematic review aimed to analyse available evidence to answer two focused questions about the efficacy of erythritol powder air‐polishing (EPAP) (i) as an adjunctive during active periodontal therapy (APT) and (ii) as an alternative to hand/ultrasonic instrumentation during supportive periodontal therapy (SPT). Additionally, microbiological outcomes and patient's comfort/perceptions were assessed as secondary outcomes.
PubMed, Cochrane and Medline were searched for relevant articles published before February 2021 following PRISMA guidelines. The search was conducted by three indep
Objective: This study aimed to evaluate the effect of coating titanium (Ti) dental implant with polyether ketone ketone (PEKK) polymer using magnetron sputtering on osseointegration, trying to overcome some of the problems associated with Ti alloys. Material and Methods: Implants were prepared from grade (II) commercially pure titanium (CP Ti), then laser was used to induce roughness on the surface of Ti. PEKK was deposited on the surface of Ti implants by radiofrequency (RF) magnetron sputtering technique. The implants were divided in to three groups: without coating (Ls), with PEKK coating using argon (Ar) as sputtering gas (Ls-PEKK-Ar), and with PEKK coating using nitrogen (N) as sputtering gas (Ls-PEKK-N). All the implants were implante
... Show MoreThe present study included the microscopic and molecular identification of Entamoeba histolytica by using specific primers to detect four virulence factors possessed by Entamoeba histolytica. Virulence factors included Active Cysteine proteinase, Galactose/N-acetyl-D-galactose-lectin, Amoeba pore C and Phospholipase. Titanium dioxide nanoparticles (TiO2NPs) were synthesized from Pseudomonas aeruginosa which producing Pyocyanin pigment as a reducing agent to form it. After that we studied the ability ofTiO2NPs to inhibit virulence factors production and curing the genes responsible for encoding them by using four different dose 2 ,3, 4, 6 mg/Kg and administered by intraperitoneal injection
... Show MoreThe aim of this work is to evaluate some mechanical and physical
properties (i.e. the impact strength, hardness, flexural strength,
thermal conductivity and diffusion coefficient) of
(epoxy/polyurethane) blend reinforced with nano silica powder (2%
wt.). Hand lay-up technique was used to manufacture the composite
and a magnetic stirrer for blending the components. Results showed
that water had affected the bending flexural strength and hardness,
while impact strength increased and thermal conductivity decreased.
In addition to the above mentioned tests, the diffusion coefficient
was calculated using Fick’s 2nd law.