Background: It may be an important prospective clinical use of manufacturing of porous implant for clinical situations, such as cases of limitation in bone height, low bone density .The small segment of porous implant an effective osseointegration allows increasing in contact area provided for small segmented porous provided by its surface configuration. This study was done to Fabricate porous titanium implants by powder technology, as well as the observation of removal torque values of porous titanium implants compared to smooth titanium implants. Materials and methods: Twenty porous titanium implants (3.2mm in diameter and 8mm in length) were manufactured by powder technology using commercially pure titanium powder of ≤75um particles size, with polyvinyl alcohol powder of 212-300um particle size, as a space holder, by volume ratio (70:30) % respectively. The mixed powder was compacted using punch and die set -specially designed for this study –under 20 bar then sintering at 900 ºC by the use of argon gas. Twenty smooth titanium implants were prepared of (3.2mm in diameter and 8mm in length) by lathing of commercially pure titanium rod as a control group. The implants were examined by X-ray diffraction (XRD) and scanning electron microscope (SEM), as well as estimation of porosity percentage. For each tibia of the 20 white New Zealand rabbits, one implant of each type (one porous in right, and the smooth in left tibia), were inserted through surgical procedure carried under serial condition. Mechanical test was performed to evaluate the bone-implant interface, after (2 and 6 weeks) healing periods . Results: Porous implants were obtained successfully by powder technology with 52% porosity and pore size 210um 17±. The porous implant showed significantly higher removal torque values when compared to smooth implants at the two different intervals of examination (2,6 weeks) , this proved to be statistically highly significant, also a highly significant difference was noticed for the means of the torque removal values in the same group at different implantation , with no evidence of clinical features of inflammatory reaction with both . Conclusions: Powder technology seemed to be particularly advantageous in fabrication of porous titanium. Porous implant show an increasing bone ingrowth compared with the smooth type represented by higher removal torque for both healing periods (2, 6) weeks . Key words: Porous titanium implant, powder technology, removal torque test.
Background: Dental implants act as infrastructure for fixed restoration to look like as a natural tooth. Osseointegration is a biological events and considered as a base for success of dental implant. The aim of this study is to evaluate the bond strength between bone and Ti implant coated with mixture of nano hydroxyapatite-chitosan-collagen compared with Ti implants coated with nano hydroxyapatite implanted in rabbit tibia, after different period of implantation time (two and six weeks) by torque removal test. Material and methods: 36 screws of commercially pure titanium; 8mm in length and 3mm diameter , 18 screws coated with mixture of nano hydroxyapatite-chitosan-collagen and18 screws coated with nano hydroxyapatite by dip coating. St
... Show MoreThe main objectives of this study are to study the enhancement of the load-carrying capacity of Asymmetrical castellated beams with encasement the beams by Reactive Powder Concrete (RPC) and lacing reinforcement, the effect of the gap between top and bottom parts of Asymmetrical castellated steel beam at web post, and serviceability of the confined Asymmetrical castellated steel. This study presents two concentrated loads test results for four specimens Asymmetrical castellated beams section encasement by Reactive powder concrete (RPC) with laced reinforcement. The encasement of the Asymmetrical castellated steel beam consists of, flanges unstiffened element height was filled with RPC for each side and laced reinforced which are use
... Show MoreThe shoulder and hip joints though essentially both are ball and socket joints, show structural variability to serve functional needs.
This study aims at revealing some of the structural and functional properties of each of the two joints regarding the factors that contribute to the stability of any joint in the body, namely: bone, ligament, and muscle.
In this research, the performance of a two kind of membrane was examined to recovering the nutrients (protein and lactose) from the whey produced by the soft cheese industry in the General Company for Food Products inAbo-ghraab.Wheyare treated in two stages, the first including press whey into micron filter made of poly vinylidene difluoride (PVDF) standard plate type 800 kilo dalton, The membrane separates the whey to permeate which represent is the main nutrients and to remove the fat and microorganisms.The second stage is to isolate the protein by using ultra filter made of polyethylsulphone(PES)type plate with a measurement of 10,60 kilo dalton and the recovery of lactose in the form of permeate.
The results showed that the percen
Abstract Background: One of the most important methods to replace lost teeth is dental implants. In order to increase the strength of connection of the implant with the jaw bone to provide early loading after placement, implant is coated by different coating materials that achieved that purpose. The aim of this study was to evaluate the influence of coating CP Ti implant with calcium carbonate on the strength of bone-implant interface after two and six weeks of implantation in rabbit femur bone by torque removal test, histological and histomorphometric analysis. Materials and methods: Coating the surface of commercially pure titanium screws with extra pure synthetic calcium carbonate via electrophoretic deposition method (EPD) was done. The
... Show MoreTitanium alloy (Ti-6Al-4V or Gr.23) was widely used as a dental alloy. In the current study, polymerization of eugenol (PE) on Gr.23 titanium alloys was conducted by an electrochemical process before and after being treated by Micro Arc Oxidation (MAO). The formed films were characterized by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), and X-ray diffraction (XRD). The corrosion behavior of Gr.23 alloy in an artificial saliva environment at a temperature range of 293–323 K has been studied and assessed by means of electrochemical polarization and impedance spectroscopy techniques. Three cases are taken into consideration; bare Gr.23, Gr.23 coated by PE, and Gr.23 coated by PE after MAO treatment. The maxi
... Show MoreBackground: Dental implants are a suitable option for the replacement of some or all missing teeth. The successful insertion of a biocompatible material into living tissue with little to no evidence of rejection has revolutionized medicine and dentistry. An increase in bone response was observed with local administration of growth hormone around dental implants. Growth hormone may act as a bone stimulant in the placement of endosseous dental implants and enhances osseointegration. The aim of the study was to evaluate immunohistochemically the effect of the topical application of growth hormone on the osseointegration of cpTi implant. Materials and Methods: Eighty titanium screw implants were inserted in the tibia of the forty adult rabbits.
... Show MoreBackground: The purpose of this study was to evaluate the effect of in vitro long-term simulation of oral conditions on the bond strength of PEEK CAD/CAM lingual retainers.
Material and methods: The sample consisted of 12 PEEK CAD/CAM retainers each composed of 2 centrally perforated 3x4mm pads joined by a connector. They were treated by 98% sulfuric acid for 1 minute and then conditioned with Single Bond Universal and bonded to the lingual surface of premolar teeth by 3M Transbond TM System. Half of the retainers were artificially aged using a 30-day water storage and 5000 thermocycling protocol before bond strength testing to compare with the non-aged specimens.
Results: The artificially aged retainers showed a marginally
... Show MoreSteady conjugate natural convection heat transfers in a two-dimensional enclosure filled with fluid saturated porous medium is studied numerically. The two vertical boundaries of the enclosure are kept isothermally at same temperature, the horizontal upper wall is adiabatic, and the horizontal lower wall is partially heated. The Darcy extended Brinkman Forcheimer model is used as the momentum equation and Ansys Fluent software is utilized to solve the governing equations. Rayleigh number (1.38 ≤ Ra ≤ 2.32), Darcy number (3.9 * 10-8), the ratio of conjugate wall thickness to its height (0.025 ≤ W ≤ 0.1), heater length to the bottom wall ratio (1/4 ≤ ≤ 3/4) and inclination angle (0°, 30° and 60°) are the main consid