Background: The Initial (primary) stability is one of the factors that play an important role in the success of the dental implants. The purpose of this study was to evaluate the initial stability of dental implant with horizontal plate by using five analytical tests: insertion torque, removal torque, resonance frequency analysis, push-in test and pull-out test. Materials and methods: Two different lengths of dental implants (5mm and 10mm) were tested in this study; each dental implant was 4mm in diameter with a square threads shape of 1mm pitch and 0.5mm depth. The crestal area was 4.2mm diameter contained a right angle margin circumferential ring while the apical area was tapered with two self-tapping grooves. In this study, the initial stability of dental implants’ design was compared with initial stability of dental implants of the same dimensions and design that engage horizontal plates of 1.5mm thickness at the apical part. All dental implants were implanted into a solid rigid polyurethane foam blocks (artificial bone) of 0.48g/cm3 density and tested by the five initial stability tests. Each test was done with forty samples (twenty samples of 5mm length and twenty samples of 10mm length). Results: The statistical analysis was performed and the result showed that there was very highly significant difference between dental implants with the horizontal plates and dental implants without the horizontal plates of both 5mm and 10 mm lengths in four initial stability tests which were insertion torque, removal torque, push-in test and pull-out test. The statistical analysis of the resonance frequency analysis showed that there was non-significant difference between dental implants with the horizontal plates and dental implants without the horizontal plates of both lengths. Conclusion: These results implied that the dental implants with the horizontal plates had better primary stability compared with the dental implants without the horizontal plates confirming that the horizontal plates enhanced the primary stability of the dental implants.
Flurbiprofen (FLB) is chemically 2-(3- fluoro-4-phenyl phenyl) propanoic acid. It is a nonsteroidal anti-inflammatory drug (NSAID) used in the treatment of rheumatoid arthritis and osteoarthritis. Oral administration of this drug is associated with severe gastrointestinal side effects like ulceration and gastrointestinal bleeding. The solution to this problem lies in the fact that topically applied NSAIDs are safer than orally. This study aims to prepare different topical semisolid formulation of FLB as cream base (o/w), (w/o) and gel base using different gel-forming agents in different concentrations. Comparing characterization properties in addition to release and diffusion study for all the prepared formulas to select the best on
... Show MoreThis experimental research was conducted to quantify the combined effect of the external bonded Carbon Fiber Reinforced Polymer (CFRP) plate width and prestressing on the flexural performance of reinforced concrete (RC) beams in terms of strength improvement. Seven beams (one control and six strengthened) were subjected to two-point loading tests. The experimental methodology consisted of the testing of three different widths of the CFRP plates (25, 40, and 60 mm) in non-prestressed and prestressed conditions. Prestressing was accomplished by tensioning the plates to 23% of the CFRP tensile strength using a novel, locally developed mechanical anchorage system, which is one of the key experimental contributions that distinguishes thi
... Show MoreAbstract: Polarization beam splitter (PBS) integrated waveguides are the key components in the receiver of quantum key distribution (QKD) systems. Their function is to analyze the polarization of polarized light and separate the transverse-electric (TE) and transverse-magnetic (TM) polarizations into different waveguides. In this paper, a performance study of polarization beam splitters based on horizontal slot waveguide has been investigated for a wavelength of . PBS based on horizontal slot waveguide structure shows a polarization extinction ratio for quasi-TE and quasi-TM modes larger than with insertion loss below and a bandwidth of . Also, the fabrication tolerance of the structure is analyzed.<
... Show MoreBackground: The aim of this study was to evaluate the shear bond strength (SBS) and adhesive remnant index (ARI) of different orthodontic adhesive systems after exposure to aging media (water storage and acid challenge). Materials and methods: Eighty human upper premolar teeth were extracted for orthodontic purposes and randomly divided into two groups (40 teeth each): the first group in which the bonded teeth were stored in distilled water for 30 days at 37°C, and the second group in which the bonded teeth were subjected to acid challenge. Each group was further subdivided into four subgroups (10 teeth each) according to the type of adhesive system that would be bonded to metal brackets: either non-fluoride releasing adhesive (NFRA),
... Show MoreBACKGROUND: The humeral shaft fractures have a good rate of union, despite this fact, still there is a significant rate of nonunion after nonoperative treatment and more often after operative treatment. AIM: The aim of the study is to evaluate the autogenous onlay graft with compression plate for treatment of persistent humeral shaft non-union with failed previous surgery both radiological and functional outcome. MATERIALS AND METHODS: A prospective study on twenty patients having persistent aseptic non-union age between 20 and 60 years old, after failed surgical treatment of fractures humeral shaft in Al-Zahra teaching and Al-Kindy teaching hospitals, while infected nonunion, diabetes mellitus, secondary metastasis, smoking, a
... Show MorePurpose: This study aimed to compare the stability and marginal bone loss of implants inserted with flapped and flapless approaches 8 weeks after surgery and 3 months after loading. Material and Methods: Thirty SLActive implants were inserted in 11 patients and early loaded with final restoration 8 weeks after healing period. The stability values determined by Osstell and the marginal bone loss measured by CBCT at the initial time (1st) and 8 weeks of the healing period (2nd) and 3 months after loading (3rd). Results: The overall survival rate was 100%. A significant increase in the 3rd implant stability value in the age of ˂ 40. A significant decrease in the 2nd implant stability value in both gender and traumatic zone with a flapless app
... Show MoreCountries have faced the challenges of high levels of public debt and seek to define the optimum limits to reduce risks to which the financial system can be exposed and its impact on the economy as a whole. Hence the importance of research in studying the impact of internal and external public debt components on indicators of stability of the financial system for the period 2005-2017 for the purpose of knowing the extent of the financial stability indicators response to the high level of the public debt from its optimum ratio, as the aim of the research is to estimate and analyze the dynamic relationship of short and long term between the components of public debt and indicators of financial stability using the (ARDL) model that
... Show More