Background: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the denture base at 45 degree) are consist of (80) artificial teeth from the same model of central incisor, they were prepared , treated and bonded to the conventional heat cured and high impact acrylic denture base material then processed. Control group (Group A 40 samples) in which acrylic resins PMMA cured by conventional water- bath processing technique (74°C for 1.5 hours then boil for 30 minutes),the group was subdivided to 20 samples heat cure acrylic and 20 samples high impact acrylic. Experimentalgroups (Group B 40 samples) in which acrylic resins was cured by autoclave at 121°C, 210KPa. For 30min.the group subdivided to 20 samples heat cure acrylic and 20 samples high impact acrylic. For each subgroup, the 20 samples were subdivided according to surface treatment into: 1-Five acrylic teeth without any surface treatment (control). 2- Five acrylic teeth with diatoric preparation (retention grooves). 3- Five acrylic teeth conditioned with thinner. 4- Five acrylic teeth with retention grooves and thinner. Results: Statistical analysis revealed that chemical and mechanical treatment of acrylic teeth improved the shear bond with heat cure and high impact acrylicalsoautoclave processing improvedthe shear bond with acrylic teeth in high impact acrylic. Conclusion: Autoclave polymerization is suggested as alternative method for processing denture base resins. Autoclave polymerization can be easily performed in laboratory conditions. In High Impact Acrylic, there were highly significant differences of autoclave processing technique compared with water bath regarding the shear bond strength with acrylic teeth.
A dynamic analysis method has been developed to investigate and characterize embedded delamination on the dynamic response of composite laminated structures. A nonlinear finite element model for geometrically large amplitude free vibration intact plate and delamination plate analysis is presented using higher order shear deformation theory where the nonlinearity was introduced in the Green-Lagrange sense. The governing equation of the vibrated plate were derived using the Variational approach. The effect of different orthotropicity ratio, boundary condition and delamination size on the non-dimenational fundamental frequency and frequency ratios of plate for different stacking sequences are studied. Finally th
... Show MoreEnhancement of heat transfer in the tube heat exchanger is studied experimentally by using discrete twisted tapes. Three different positions were selected for inserting turbulators along tube section (horizontal position by α= 00, inclined position by α= 45 0 and vertical position by α= 900). The space between turbulators was fixed by distributing 5 pieces of these turbulators with pitch ratio PR = (0.44). Also, the factor of constant heat flux was applied as a boundary condition around the tube test section for all experiments of this investigation, while the flow rates were selected as a variable factor (Reynolds number values vary from 5000 to 15000). The results s
... Show MoreThe effect of linear thermal stratification in stable stationary ambient fluid on free convective flow of a viscous incompressible fluid along a plane wall is numerically investigated in the present work. The governing equations of continuity, momentum and energy are solved numerically using finite difference method with Alternating Direct implicit Scheme. The velocity, temperature distributions
and the Nusselt number are discussed numerically for various values of physical parameters and presented through graphs. ANSYS program also used to solve the problem. The results show that the effect of stratification parameter is marginalized with the increase in Prandtl number, and the increase in Grashof number does not practically vary the
The printed circuit heat exchanger is a plate type heat exchanger with a high performance and compact size. Heat exchangers such as this need a unique form of bonding and other techniques to be used in their construction. In this study, the process of joining plates, diffusion bonding, was performed and studied. A special furnace was manufactured for bonding purposes. The bonding process of copper metal was carried out under specific conditions of a high temperature up to 700 oC, high pressure of 3.45 MPa, and in an inert environment (Argon gas) to make tensile samples. The tensile samples are cylindrical shapes containing groves representing the flow channels in the printed circuit heat exchanger and checking their tensile st
... Show MoreThis research aims to investigate the thermal performance of different thermal composite insulators, wrapped around a closed-loop copper pipe (CLP). To achieve this aim a system was designed and manufactured. It is consisted of closed water tank insulated by Rock Wool, and supplied with two electric heaters, two thermostat, a flow meter, a water pump, digital temperature scales, and four series of (CLP).
Six insulators were prepared namely; composites of Impregnated Fiberglass with Elastoclad and foaming Rubber (FER), Impregnated Fiberglass with Elastoclad resin and Polymeric Membrane (FEM), Impregnated Fiberglass with Polyurethane thermoset resin and Foaming Rubber (FUR), Impregnated Fiberglass with Polyurethane thermoset resin and P
The current study was conducted on 504(Ros-308) broiler chicks during the period 28/9/2017-9/11/2018to determine the effect of heat shock in early age and additives such as ginseng in three levels on birds weight and feedconsumption. Results showed that the exposure to high temperature (38-400C) lead to significant decrease (p≤≤≤≤≤0.05 (inaverage body weight at7 day of age and significant decrease in body weight in birds expousured to high temperature inthe periods 2, 4 and 6 hours compared with control (Table 1). Significant decrease in live body weight when exposure to2hr compared with 6hr namely (138.54) and (144.21), respectively while no significant difference between 2 and 4h.Results showed no significant effect in body we
... Show MoreEmploying phase-change materials (PCM) is considered a very efficient and cost-effective option for addressing the mismatch between the energy supply and the demand. The high storage density, little temperature degradation, and ease of material processing register the PCM as a key candidate for the thermal energy storage system. However, the sluggish response rates during their melting and solidification processes limit their applications and consequently require the inclusion of heat transfer enhancers. This research aims to investigate the potential enhancement of circular fins on intensifying the PCM thermal response in a vertical triple-tube casing. Fin arrays of non-uniform dimensions and distinct distribution patterns were des
... Show More Heat exchanger is an important device in the industry for cooling or heating process. To increase the efficiency of heat exchanger, nanofluids are used to enhance the convective heat . transfer relative to the base fluid. - Al2O3/water nanofluid is used as cold stream in the shell and double concentric tube heat exchanger counter current to the hot stream basis oil. These nanoparticles were of particle size of 40 nm and it was mixed with a base fluid (water) at volume
concentrations of 0.002% and 0.004%. The results showed that each of Nusselt number and overall heat transfer coefficient increased as nanofluid concentrations increased. The pressure drop of nanofluid increased slightly than the base fluid because
Introduction: We aimed to assess the impact of adhesive and wires types on the tensile bond strength of fixed lingual retainers. Methods: A total of 160 intact bovine teeth were collected, cleaned, stored in 25% sodium hypochlorite, and randomly assigned to two groups based on the adhesive type: a two-step adhesive and a one-step adhesive. Each group was further divided into four subgroups based on the type of lingual retainer wire, which included (A) 8-strand braided stainless steel wire, (B) three-strand titanium retainer wire, (C) stainless steel chain, and (D) fiber-reinforced retainer. A tensile bond strength test was conducted using a universal testing machine at a controlled speed of 10 mm/min. Result: The 8-strand braided stainles
... Show More