Background: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the denture base at 45 degree) are consist of (80) artificial teeth from the same model of central incisor, they were prepared , treated and bonded to the conventional heat cured and high impact acrylic denture base material then processed. Control group (Group A 40 samples) in which acrylic resins PMMA cured by conventional water- bath processing technique (74°C for 1.5 hours then boil for 30 minutes),the group was subdivided to 20 samples heat cure acrylic and 20 samples high impact acrylic. Experimentalgroups (Group B 40 samples) in which acrylic resins was cured by autoclave at 121°C, 210KPa. For 30min.the group subdivided to 20 samples heat cure acrylic and 20 samples high impact acrylic. For each subgroup, the 20 samples were subdivided according to surface treatment into: 1-Five acrylic teeth without any surface treatment (control). 2- Five acrylic teeth with diatoric preparation (retention grooves). 3- Five acrylic teeth conditioned with thinner. 4- Five acrylic teeth with retention grooves and thinner. Results: Statistical analysis revealed that chemical and mechanical treatment of acrylic teeth improved the shear bond with heat cure and high impact acrylicalsoautoclave processing improvedthe shear bond with acrylic teeth in high impact acrylic. Conclusion: Autoclave polymerization is suggested as alternative method for processing denture base resins. Autoclave polymerization can be easily performed in laboratory conditions. In High Impact Acrylic, there were highly significant differences of autoclave processing technique compared with water bath regarding the shear bond strength with acrylic teeth.
Background: The combination of thermoplastic nylon resin materials and auto polymerizing resin is necessary in some situation for repair and adjustment. This study evaluated shear bond strength between thermoplastic nylon material (flexible) and auto polymerizing acrylic resin subjected to holes and silica coated layer. Materials and Method: Forty five (45) specimens were prepared from flexible acrylic bonded to auto-polymerizing acrylic resin and divided into three groups according to the surface treatments as follows: Group A: 15 specimens of flexible acrylic bonded with cold-cure acrylic by holes. Group B: 15 specimens of flexible acrylic bonded with cold-cure acrylic by silica coated layer. Group C: 15 specimens of flexible acrylic bon
... Show MoreSoaking dentures with disinfection solutions is an effective way of keeping dentures in a healthy status; however, immersions in these solutions have a negative effect on the bond strength of denture base and denture teeth. The aim of this study was to evaluate the bond strength between denture acrylic teeth and heat-cured Poly (methyl methacrylate) denture base material (with and without nano silica) after disinfection with different chemical disinfectants for a simulated period of six months. One hundred specimens of maxillary central incisors attached to PMMA were divided into two groups; 50 specimens of PMMA without nano silica and 50 specimens of PMMA reinforced with 5 wt% of nano silica. Specimens of each group were immersed in five i
... Show MoreABSRTACT Background: Soft liner material is become important in dental prosthetic treatment. They are applied to the surface of the dentures to achieve more equal force distribution , reduce localized pressure and improve denture retention by engaging undercut . So the aim of the study is to evaluate the effect of different surface treatment by air-abrasion AL2O3 and laser treatment with CO2 laser on improving the shear bond strength of the denture liner to acrylic denture base material . Materials and methods: the 30 specimens of heat cured acrylic denture base material (high Impact acrylic )and heat cured soft liner (Vertex ,Nether Lands )were prepared for this study .They were designed and divided according to type of the s
... Show MoreBackground: Recently, Poly propylene fibers with and without plasma treatment have been used to reinforce heat cure denture base acrylic but, so far some of properties like tensile strength , wettability and wear resistance not evaluated yet, the aim of the study is to clarify the influence of incorporation of treated and untreated fibers on these properties. Materials and methods: Twenty one specimens were fabricated for every tested property(tensile strength, wear resistance and wettability) that classified into three groups(control, untreated poly propylene fibers reinforced specimens and Oxygen plasma treated group)and for each test sevens amples were used(n=7). Tensile strength was tested using Instron universal testing machine, wear
... Show MoreBackground: The most widely used material for fabrication of denture base is poly methyl methacrylate, despite its popularity, the main problems associated with it as a denture base material are poor strength particularly under fatigue failure inside the patient mouth, impact failure outside the patient mouth, which are the main causes for fracture of denture, several studies was done to increase mechanical properties of denture base. The present study was conducted to evaluate and compare the effect of addition single walled carbon nanotubes in different concentrations to polymethyl methacrylate on some mechanical properties (surface hardness, surface roughness, impact strength and transverse strength). Materials and methods: Forty eight
... Show MoreBackground: The aim of this study was to evaluate the effect of thermo cycling and different pH of artificial saliva (neutral, acidic, basic) on impact and transverse strength of heat cure acrylic resin reinforced of with 5% silanated ZrO2 nano fillers. Materials and methods: 120 samples were prepared, 60 samples for impact strength test and another 60 samples for transverse strength test, for each test, samples were divided into two major groups (before and after thermo cycling), then each of these major groups were further subdivided into 3 subgroups according to the pH of prepared artificial saliva (neutral, acidic, basic). Charpy impact device was used for impact strength test and Flexural device was used for transverse strength test. R
... Show MoreBackground: The denture base inaccuracies during processing negatively influence the retention and stability of finished complete denture. The aims of this study were to evaluate teeth movement and palatal adaptation of autoclave cured denture bases and their relationship with palatal depths and investments. Materials and methods: A nightly maxillary complete dentures prepared, processed and organized to be tested as follows: 1. Processing methods: water bath and autoclave with both fast and slow cycles. 2. Palatal depth: shallow, medium and deep. 3. Investing medium: stone and silicone. For every finished denture, two measurements were done: first: teeth movement by attaching metallic reference screws on the right and left centrals, first
... Show MoreBackground: The main drawback of soft lining materials was that they debonded from the denture base after a certain period of usage. Therefore, the purpose of this research was to determine the impact of oxygen and argon plasma treatment on the shear bonding strength of soft liners to two different kinds of denture base materials: conventional acrylic resin and high impact acrylic resin. Materials and Methods: Heat cure conventional and high impact acrylic blocks (40 for each group) were prepared. A soft liner connected the final test specimen of two blocks of each acrylic material. Shear bond strength (SBS) was assessed using universal testing machine. Additional blocks were also prepared for analyzing Vickers microhardness, contact ang
... Show MoreBackground: The base of the denture is largely responsible for providing the prosthesis with retention, stability, and support by being closely adapted to the oral mucosa. However; the process of bone resorption is irreversible and may lead to an inadequate fit of the prosthesis; this can be overcome by relining. Materials and methods: Acrylic based soft denture liner is prepared by preparing polymer from purified methylmethacrylate monomer with (10-2) initiator and (30%) dibutylphthalate plasticizer concentrations. Biological properties were evaluated in comparison with the control material through subcutaneous specimens' implantation in the New Zealand rabbits. Excisional biopsies were taken after (1, 3, days 1, 2, 3, 4 weeks) period. Mic
... Show MoreBackground: acrylic resin denture base consider a common denture base material for its acceptable cost, aesthetic and easy processing but still has disadvantages including easy of fracture and low impact strength. Material and method: The experimental group was prepared by addition of 15% phosphoric acid 2-hydroxyethyl methacrylate ester (PA2HEME) with polymethyl methacrylate monomer; the experimental groups was compared with the control one. The specimens were prepared according to ADA specification No. 12 with dimension 65 mm x 10 mm x2.5 mm (length x width x thickness respectively). The prepared specimens were tested by three-point flexural strength utilizing Instron Universal Testing Machine (WDW, Layree Technology Co.), Shore D hard
... Show More